01 / Nylon cable entry
Nylon Cable Glands
Nylon cable glands hold and seal unarmoured cables at enclosure entries. Straight bodies suit direct cable runs, angled and flexible forms help route the cable, and multi-hole seals take several cables through one opening.
- Cable outside diameter
- Entry thread and wall
- Body form and bend clearance
Cable gland families
Compare cable glands by material, cable construction and duty.
Choose nylon, brass or stainless steel by body material, or compare EMC, armoured, hazardous-area, marine and conduit-entry designs by the job they must perform.
Nylon Cable Glands range
Choose your nylon cable glands
Lightweight cable glands in straight, angled, flexible, long-thread and multi-hole forms.
Models & dimensions
Nylon Cable Glands: specifications and dimensions
Select a product to see its specifications, drawings and sizes.
Nylon Cable Glands
Which fitting do you need?
Choose a product above, or show all products to compare sizes and construction.- 01Cable and seal range
- 02Entry thread and dimensions
- 03Material and installation duty
One-Piece Nylon Cable Gland
01 / Nylon cable entry
One-Piece Nylon Cable Gland
A nylon cable gland with the body, clamping claw and seal retained in one assembly for straight cable entry into an enclosure.
Product reference
- Construction
- Standard Nylon Cable Glands
- Application
- A straight, unarmoured cable entry where keeping the sealing and clamping parts together simplifies assembly.
Key specifications
- Structure
- One-piece / united structure
- Body material
- Nylon PA/PA6
- Seal and O-ring
- EPDM or silicone rubber
- protection
- IP68
Product specifications
Construction and details

Assembly arrangement and dimensions
Compare the arrangement of the illustrated parts. Confirm the assembly instructions for the selected model.
Read the marked dimensions with the current model drawing; do not infer sizes by measuring the illustration.
Model specification tablesFurther specifications
- Static temperature
- -40°C to 100°C; short term to 120°C
- Dynamic temperature
- -20°C to 80°C; short term to 100°C
- Thread types
- Metric, PG, G (PF/BSP) and NPT
- Colours
- Black or grey; other colours available to order.
- Body material flammability
- UL 94 V-2
Key features
- Retained assemblyThe body, clamping claw and seal stay together, reducing the number of loose parts during installation.
- Nylon bodyThe nylon body uses EPDM or silicone sealing parts.
- Four thread systemsMetric, PG, G and NPT versions connect to different enclosure entries.
Divided Nylon Cable Gland
02 / Nylon cable entry
Divided Nylon Cable Gland
A divided nylon cable gland with separate body, clamping and sealing parts for straight cable entries.
Product reference
- Construction
- Standard Nylon Cable Glands
- Application
- An unarmoured cable entry where separate sealing and clamping parts are useful during assembly.
Key specifications
- Structure
- Multi-part / divided structure
- Body material
- Nylon PA66
- Seal and O-ring
- EPDM rubber; other seal options by model
- protection
- IP68, 10 bar
Product specifications
Construction and details
Further specifications
- Static temperature
- -40°C to 100°C; short term to 120°C
- Dynamic temperature
- -20°C to 80°C; short term to 100°C
- Thread types
- Metric, PG, G (PF/BSP) and NPT
- Colours
- Black (RAL 9005), grey (RAL 7035); other colours by request
Key features
- Separate componentsThe multi-part construction opens up the seal and clamping components during assembly.
- Nylon and elastomer constructionThe body is PA66 with an EPDM seal and O-ring; alternative seals are available for some models.
- Black and grey optionsThe range includes black RAL 9005 and grey RAL 7035 bodies.
Nylon Cable Gland with Flexible Bend-Protection Tail
03 / Nylon cable entry
Nylon Cable Gland with Flexible Bend-Protection Tail
A PA66 cable gland with an extended flexible tail that supports the cable as it leaves the enclosure.
Product reference
- Construction
- Flexible Bend-Protection Glands
- Application
- A cable exit that needs local bend support close to the gland.
Key specifications
- Product type
- Flexible / anti-bending nylon cable gland
- Body material
- Nylon PA66
- Seal material
- EPDM or silicone rubber
- protection
- IP68
Product specifications
Construction and details

Assembly arrangement and dimensions
Compare the arrangement of the illustrated parts. Confirm the assembly instructions for the selected model.
Read the marked dimensions with the current model drawing; do not infer sizes by measuring the illustration.
Model specification tablesFurther specifications
- Static temperature
- Operating range: −40°C to +100°C; short term to +120°C
- Thread types
- Metric and PG
- Colours
- Black or grey; other colours available to order.
Key features
- Flexible tailThe spiral tail provides a gradual transition from the gland body to the free cable.
- Cable clamping and sealingThe claw and elastomer seal hold the cable at the entry while the tail supports the adjacent length.
- Metric and PG versionsThe range includes Metric and PG entry threads.
90-Degree Nylon Cable Gland
04 / Nylon cable entry
90-Degree Nylon Cable Gland
A 90-degree nylon cable gland that turns the cable alongside the enclosure instead of straight out from it.
Product reference
- Construction
- Right-Angle Nylon Cable Glands
- Application
- An enclosure with limited straight-out clearance or a cable path that must turn close to the entry.
Key specifications
- Product type
- 90-degree / right-angle nylon cable gland
- Body material
- Nylon PA66
- Seal and washer
- NBR or EPDM, depending on model
- protection
- IP68
Product specifications
Construction and details
Further specifications
- Static temperature
- -40°C to 100°C; short term to 120°C
- Dynamic temperature
- -20°C to 80°C; short term to 100°C
- Thread types
- Metric, PG, G (PF/BSP) and NPT
- Colours
- Black (RAL 9005), light grey (RAL 7035); other colours by request
Key features
- Right-angle exitThe elbow body changes the cable direction by 90 degrees.
- PA66 bodyThe body combines nylon construction with an NBR or EPDM sealing arrangement, depending on the model.
- Entry-thread optionsMetric, PG, G and NPT versions suit different threaded entries.
Extended-Thread Nylon Cable Gland
05 / Nylon cable entry
Extended-Thread Nylon Cable Gland
A nylon cable gland with an extended entry thread for thicker enclosure walls and recessed mounting positions.
Product reference
- Construction
- Extended-Thread Nylon Glands
- Application
- A panel or threaded opening that needs more thread engagement than the standard gland provides.
Key specifications
- Product type
- Extended-thread nylon cable gland
- Body material
- Nylon PA/PA6
- Seal material
- EPDM or silicone rubber
- protection
- IP68
Product specifications
Construction and details
Further specifications
- Static temperature
- -40°C to 100°C; short term to 120°C
- Dynamic temperature
- -20°C to 80°C; short term to 100°C
- Thread types
- Metric, PG, G (PF/BSP) and NPT
- Colours
- Black or grey; other colours available to order.
- Body material flammability
- UL 94 V-2
Key features
- Extended male threadThe longer entry thread reaches through thicker panels or further into a threaded opening.
- Straight cable sealThe cable-side claw and seal retain the straight-entry arrangement.
- Nylon constructionThe nylon body uses EPDM or silicone sealing parts.
Multi-Hole Nylon Cable Gland
06 / Nylon cable entry
Multi-Hole Nylon Cable Gland
A nylon cable gland with a multi-hole sealing insert for several small cables through one enclosure opening.
Product reference
- Construction
- Multi-Hole Nylon Cable Glands
- Application
- Several separate cables need to share one threaded entry.
Key specifications
- Product type
- Multi-hole nylon cable gland
- Body material
- Nylon PA6
- Seal material
- NBR or EPDM, depending on model
- protection
- IP68
Product specifications
Construction and details

Assembly arrangement and dimensions
Compare the arrangement of the illustrated parts. Confirm the assembly instructions for the selected model.
Read the marked dimensions with the current model drawing; do not infer sizes by measuring the illustration.
Model specification tablesFurther specifications
- Static temperature
- -40°C to 100°C; short term to 120°C
- Dynamic temperature
- -20°C to 80°C; short term to 100°C
- Thread types
- Metric and PG
- Colours
- Black (RAL 9005), light grey (RAL 7035); other colours by request
Key features
- Multi-hole insertSeparate bores position the cables within one sealing insert.
- Shared gland bodyOne gland body compresses the complete insert around the individual cables.
- PA6 bodyThis multi-hole construction uses PA6 with NBR or EPDM sealing options.
Nylon Corrugated Conduit Connector
07 / Nylon cable entry
Nylon Corrugated Conduit Connector
A nylon fitting that secures corrugated conduit to a threaded enclosure entry using a sealing nut.
Product reference
- Construction
- Nylon Conduit Connectors
- Application
- A corrugated conduit run needs a threaded connection to a box, machine or enclosure.
Key specifications
- Product type
- Nylon corrugated-conduit connector
- Body components
- Nylon PA6/PA66 body, locknut and sealing nut
- Seal and washer
- EPDM or silicone rubber
- protection
- IP68
Product specifications
Construction and details

Assembly arrangement and dimensions
Compare the arrangement of the illustrated parts. Confirm the assembly instructions for the selected model.
Read the marked dimensions with the current model drawing; do not infer sizes by measuring the illustration.
Model specification tablesFurther specifications
- Static temperature
- -40°C to 100°C; short term to 120°C
- Dynamic temperature
- -20°C to 80°C; short term to 100°C
- Thread types
- Metric, PG, G (PF/BSP) and NPT
- Application
- Corrugated conduit to enclosure or machine entry
- Colours
- Black or grey; other colours available to order.
- Body material flammability
- UL 94 V-2
Key features
- Conduit clamping nutThe sealing nut retains the corrugated conduit at the fitting body.
- Seal and washerEPDM or silicone sealing parts fit between the conduit, body and enclosure.
- Separate assembly partsThe construction comprises the locknut, washer, body, seal and sealing nut.
Quick-Connect Nylon Fitting for Corrugated Conduit
08 / Nylon cable entry
Quick-Connect Nylon Fitting for Corrugated Conduit
A PA66 push-fit connector for attaching corrugated conduit to equipment or an enclosure.
Product reference
- Construction
- Nylon Conduit Connectors
- Application
- A corrugated conduit connection calls for a push-fit construction without a separate compression nut.
Key specifications
- Product type
- Quick-connect nylon fitting for corrugated conduit
- Body material
- Nylon PA66
- temperature
- -40°C to 105°C
- Application
- Push-fit connection of corrugated conduit to equipment or enclosures
Product specifications
Construction and details
Key features
- Push-fit connectionThe corrugated conduit inserts into the fitting body without a separate compression nut.
- Nylon bodyThe PA66 body connects the conduit to the equipment entry.
Nylon Waterproof Breathable Cable Gland
09 / Nylon cable entry
Nylon Waterproof Breathable Cable Gland
A nylon cable entry with a breathable insert for sealed equipment housings.
Product reference
- Construction
- Breathable Nylon Cable Glands
- Application
- Cable sealing and ventilation in a lightweight nylon body.
Key specifications
- Body material
- Nylon
- Clamping insert
- Nylon PA
- Seal material
- NBR or EPDM
- Protection rating
- IP68
Product specifications
Construction and details

Product views and dimensions
Read the marked dimensions with the current model drawing; do not infer sizes by measuring the illustration.
Drawing markers: AG · GL · H
Model specification tablesFurther specifications
- Operating temperature
- −40°C to +100°C; short term to +120°C
- Colours
- Black or white
Key features
- Breathable cable entryThe body combines a cable seal with an enclosure vent.
- Four cable-entry sizesChoose M12, M16 or M20 threads and a 4–8 or 5–10 mm cable range.
Model specification tables
Model sizes
One-Piece Nylon Cable Gland
Nylon cable entry
One-Piece Nylon Cable Gland
Model specificationsMetric thread
| Code | Thread | Cable diameter range (mm) | Thread outside diameter C1 (mm) | Thread length C2 (mm) | Spanner size A&F (mm) |
|---|---|---|---|---|---|
| NLM8-UN | M8X1.25 | 2-4.8 | 8 | 7.5 | 13/12 |
| NLM10-UN | M10X1.5 | 3-6 | 10 | 8 | 15/13 |
| NLM12A-UN | M12X1.5 | 3-6.5 | 12 | 9 | 18/16 |
| NLM12B-UN | M12X1.5 | 3-6.5 | 12 | 15 | 18/15 |
| NLM12C-UN | M12X1.5 | 3-5.5 | 12 | 8.5 | 18/19 |
| NLM12D-UN | M12X1.5 | 4-8 | 12 | 9 | 18/16 |
| NLM12E-UN | M12X1.5 | 3-5.5 | 12 | 15 | 18/19 |
| NLM12F-UN | M12X1.5 | 4-8 | 12 | 15 | 18/19 |
| NLM16A-UN | M16X1.5 | 4-8 | 16 | 9 | 22/19 |
| NLM16B-UN | M16X1.5 | 4-8 | 16 | 15 | 22/19 |
| NLM16C-UN | M16X1.5 | 5-10 | 16 | 9 | 22/19 |
| NLM16D-UN | M16X1.5 | 5-10 | 16 | 15 | 22/22 |
| NLM18A-UN | M18X1.5 | 5-10 | 18 | 9 | 24/22 |
| NLM18B-UN | M18X1.5 | 5-10 | 18 | 15 | 24/22 |
| NLM20A-UN | M20X1.5 | 6-12.5 | 20 | 10 | 27/24 |
| NLM20B-UN | M20X1.5 | 8.5-14 | 20 | 11 | 27/27 |
| NLM20C-UN | M20X1.5 | 8.5-14 | 20 | 15 | 27/27 |
| NLM22-UN | M22X1.5 | 8.5-14 | 22 | 11 | 27/27 |
| NLM24-UN | M24X1.5 | 8.5-14 | 24 | 11 | 27/27 |
| NLM25A-UN | M25X1.5 | 8.5-14 | 25 | 11.6 | 33/27 |
| NLM25B-UN | M25X1.5 | 12.5-18 | 25 | 11.6 | 33/33 |
| NLM25C-UN | M25X1.5 | 12.5-18 | 25 | 15 | 33/33 |
| NLM32A-UN | M32X1.5 | 14-22 | 32 | 15 | 41/42 |
| NLM32B-UN | M32X1.5 | 17-25 | 32 | 15 | 41/42 |
| NLM36A-UN | M36X1.5 | 14-22 | 36 | 12 | 45/42 |
| NLM36B-UN | M36X1.5 | 17-25 | 36 | 12 | 45/42 |
| NLM40-UN | M40X1.5 | 23-32 | 40 | 15 | 50/52 |
| NLM50-UN | M50X1.5 | 30-41 | 50 | 15 | 62/62 |
| NLM63-UN | M63X1.5 | 35-46 | 63 | 18 | 75/65 |
Model specificationsNPT thread
| Code | Thread | Cable diameter range (mm) | Thread outside diameter Cl (mm) | Thread length C2 (mm) | Spanner size A&F (mm) |
|---|---|---|---|---|---|
| NLNPT1/4-UN | NPT1/4” | 4-8 | 13.157 | 8.5 | 19 |
| NLNPT3/8-UN | NPT3/8″ | 5-10 | 16.662 | 10 | 22 |
| NLNPT1/2-UN | NPT1/2” | 6-12.5 | 20.955 | 10 | 24 |
| NLNPT3/4-UN | NPT3/4″ | 12.5-18 | 26.441 | 15 | 33 |
| NLNPT1-UN | NPT1H | 17-25 | 33.249 | 15 | 41 |
| NLNPT11/4A-UN | NPT 11/4” | 17-25.5 | 41.91 | 15 | 52 |
| NLNPT11/4B-UN | NPT 11/4” | 24-32 | 41.91 | 15 | 52 |
Model specificationsPG thread
| Code | Thread | Cable diameter range (mm) | Thread outside diameter Cl (mm) | Thread length C2 (mm) | Spanner size A&F (mm) |
|---|---|---|---|---|---|
| NLPG7A-UN | PG7 | 3-6.5 | 12.5 | 9 | 18/16 |
| NLPG7B-UN | PG7 | 4-8 | 12.5 | 8 | 17/19 |
| NLPG7C-UN | PG7 | 4-8 | 12.5 | 15 | 17/19 |
| NLPG9A-UN | PG9 | 4-8 | 15.2 | 9 | 22/19 |
| NLPG9B-UN | PG9 | 4-8 | 15.2 | 15 | 22/19 |
| NLPG11A-UN | PG11 | 5-10 | 18.6 | 9 | 24/22 |
| NLPG11B-UN | PG11 | 5-10 | 18.6 | 15 | 24/22 |
| NLPG13.5A-UN | PG13.5 | 6-12.5 | 20.4 | 10 | 27/24 |
| NLPG13.5B-UN | PG13.5 | 6-12.5 | 20.4 | 15 | 27/24 |
| NLPG16A-UN | PG16 | 8.5-14 | 22.5 | 10.8 | 30/27 |
| NLPG16B-UN | PG16 | 8.5-14 | 22.5 | 15 | 30/27 |
| NLPG19A-UN NLPG19B-UN | PG19 | 8.5-14 8.5-14 | 24 24 | 11 15 | 30/27 30/27 |
| NLPG21A-UN | PG21 | 12.5-18 | 28.3 | 12 | 36/33 |
| NLPG21B-UN | PG21 | 12.5-18 | 28.3 | 15 | 36/33 |
| NLPG25A-UN | PG25 | 14-20 | 30 | 13 | 36/37 |
| NLPG25B-UN | PG25 | 14-20 | 30 | 15 | 36/37 |
| NLPG29A-UN | PG29 | 17-25 | 37 | 12 | 46/41 |
| NLPG29B-UN | PG29 | 17-25 | 37 | 15 | 46/41 |
| NLPG36-UN | PG36 | 24-32 | 47 | 14 | 57/52 |
| NLPG42-UN | PG42 | 30-41 | 54 | 15 | 64/62 |
| NLPG48-UN | PG48 | 35-45.5 | 59.3 | 18 | 70/65 |
Model specificationsG thread
| Code | Thread | Cable diameter range (mm) | Thread outside diameter Cl (mm) | Thread length C2 (mm) | Spanner size A&F (mm) |
|---|---|---|---|---|---|
| NLG1/4-UN | G(PF)1/4″ | 4-8 | 13.157 | 8.5 | 19/19 |
| NLG3/8-UN | G(PF)3/8″ | 5-10 | 16.662 | 10 | 22/22 |
| NLG1/2-UN | G(PF)1/2″ | 6-12.5 | 20.955 | 10 | 27/24 |
| NLG3/4-UN | G(PF)3/4″ | 12.5-18 | 26.441 | 12 | 36/33 |
| NLG1-UN | G(PF)1″ | 17-25 | 33.249 | 15 | 46/41 |
| NLG11/4-UN | G(PF)1 1/4″ | 30-41 | 41.91 | 15 | 57/52 |
| NLG11/2-UN | G(PF)1 1/2″ | 25-32 | 48 | 15 | 60/62 |
| NLG2-UN | G(PF)2″ | 29-38 | 60 | 18 | 60/62 |
Model specificationsG/NPT threads
| Product Code | Thread AG | Cable range(mm) | Thread outside diameter C1 (mm) | Thread length GL (mm) | Spanner Size (mm) |
|---|---|---|---|---|---|
| NLG1/4A-UN | G1/4″ | 3-5.3 | 13.157 | 8.5 | 19/19 |
| NLG1/4B-UN | G1/4″ | 4-8 | 13.157 | 8.5 | 19/19 |
| NLG3/8A-UN | G3/8″ | 3-7 | 16.662 | 10 | 22/22 |
| NLG3/8B-UN | G3/8″ | 5-10 | 16.662 | 10 | 22/22 |
| NLG1/2A-UN | G1/2″ | 5-9 | 20.955 | 10 | 27/24 |
| NLG1/2B-UN | G1/2″ | 6-12.5 | 20.955 | 10 | 27/24 |
| NLG3/4A-UN | G3/4″ | 7-13 | 26.441 | 12 | 36/33 |
| NLG3/4B-UN | G3/4″ | 12.5-18 | 26.441 | 12 | 36/33 |
| NLG1A-UN | G1″ | 15-22 | 33.249 | 15 | 46/41 |
| NLG1B-UN | G1″ | 17-25 | 33.249 | 15 | 46/41 |
| NLG1 1/4A-UN | G11/4″ | 17-25.5 | 41.91 | 15 | 57/52 |
| NLG1 1/4B-UN | G11/4″ | 30-41 | 41.91 | 15 | 57/52 |
| NLG1 1/2A-UN | G11/2″ | 25-32 | 48 | 15 | 60/62 |
| NLG1 1/2B-UN | G11/2″ | 24-32 | 48 | 15 | 60/62 |
| NLG2A-UN | G2″ | 29-38 | 60 | 18 | 60/62 |
| NLG2B-UN | G2″ | 39-45.5 | 60 | 18 | 60/62 |
| NLNPT1/4A-UN | NPT1/4″ | 3-5.3 | 13.157 | 8.5 | 19/19 |
| NLNPT1/4B-UN | NPT1/4″ | 4-8 | 13.157 | 8.5 | 19/19 |
| NLNPT3/8A-UN | NPT3/8″ | 3-7 | 16.662 | 10 | 22/22 |
| NLNPT3/8B-UN | NPT3/8″ | 5-10 | 16.662 | 10 | 22/22 |
| NLNPT1/2A-UN | NPT1/2″ | 5-9 | 20.955 | 10 | 24/24 |
| NLNPT1/2B-UN | NPT1/2″ | 6-12.5 | 20.955 | 10 | 24/24 |
| NLNPT3/4A-UN | NPT3/4″ | 7-13 | 26.441 | 15 | 33/33 |
| NLNPT3/4B-UN | NPT3/4″ | 12.5-18 | 26.441 | 15 | 33/33 |
| NLNPT1A-UN | NPT1″ | 15-22 | 33.249 | 15 | 41/41 |
| NLNPT1B-UN | NPT1″ | 17-25 | 33.249 | 15 | 41/41 |
| NLNPT1 1/4A-UN | NPT11/4″ | 17-25.5 | 41.91 | 15 | 52/52 |
| NLNPT1 1/4B-UN | NPT11/4″ | 24-32 | 41.91 | 15 | 52/52 |
Divided Nylon Cable Gland
Nylon cable entry
Divided Nylon Cable Gland
Model specificationsMetric thread
| Code | Thread | Cable diameter range (mm) | Thread outside diameter Cl (mm) | Thread length C2 (mm) | Spanner size A&F (mm) |
|---|---|---|---|---|---|
| NLM12A-DS | M12X1.5 | 3-5.5 | 12 | 8.5 | 18/19 |
| NLM12B-DS | M12X1.5 | 4.5-7.8 | 12 | 8.5 | 18/19 |
| NLM16A-DS | M16X1.5 | 4-8 | 16 | 10 | 22/19 |
| NLM16B-DS | M16X1.5 | 4-8 | 16 | 15 | 22/19 |
| NLM16C-DS | M16X1.5 | 6-10 | 16 | 10 | 22/22 |
| NLM16D-DS | M16X1.5 | 6-10 | 16 | 15 | 22/22 |
| NLM20A-DS | M20X1.5 | 6-12.5 | 20 | 10 | 24/24 |
| NLM20B-DS | M20X1.5 | 9-14 | 20 | 10 | 27/27 |
| NLM20C-DS | M20X1.5 | 9-14 | 20 | 15 | 27/27 |
| NLM22-DS | M22X1.5 | 9-14 | 20 | 10 | 27/27 |
| NLM25A-DS | M25X1.5 | 10-16 | 25 | 10 | 33/33 |
| NLM25B-DS | M25X1.5 | 13-18 | 25 | 10 | 33/33 |
| NLM25C-DS | M25X1.5 | 10-16 | 25 | 15 | 33/33 |
| NLM25D-DS | M25X1.5 | 13-18 | 25 | 15 | 33/33 |
| NLM32A-DS | M32X1.5 | 15-22 | 32 | 15 | 41/42 |
| NLM32B-DS | M32X1.5 | 18-25 | 32 | 15 | 41/42 |
| NLM40-DS | M40X1.5 | 24-31 | 40 | 20 | 50/52 |
| NLM50-DS | M50X1.5 | 31-41 | 50 | 22 | 62/62 |
| NLM63-DS | M63X1.5 | 44-51 | 63 | 25 | 75/75 |
| NLM75-DS | M75X2.0 | 56-66 | 75 | 25 | 92/92 |
| NLM90-DS | M90X2.0 | 66-77 | 90 | 25 | 110/110 |
Model specificationsPG thread
| Code | Thread | Cable diameter range (mm) | Thread outside diameter Cl (mm) | Thread length C2 (mm) | Spanner size A&F (mm) |
|---|---|---|---|---|---|
| NLPG7-DS | PG7 | 4.5-7.8 | 12.5 | 8 | 17/19 |
| NLPG9-DS | PG9 | 4.5-7.8 | 15.2 | 8.2 | 22/19 |
| NLPG11-DS | PG11 | 6-10 | 18.6 | 10 | 24/22 |
| NLPG13.5-DS | PG13.5 | 7-12.5 | 20.4 | 10 | 27/24 |
| NLPG16-DS | PG16 | 9-14 | 22.5 | 10.8 | 30/27 |
| NLPG21-DS | PG21 | 13-18 | 28.3 | 12 | 36/33 |
| NLPG29-DS | PG29 | 18-25 | 37 | 12 | 46/41 |
| NLPG36-DS | PG36 | 24-31 | 47 | 14 | 57/52 |
| NLPG42-DS | PG42 | 31-41 | 54 | 15 | 64/62 |
Model specificationsG thread
| Code | Thread | Cable diameter range (mm) | Thread outside diameter Cl (mm) | Thread length C2 (mm) | Spanner size A&F (mm) |
|---|---|---|---|---|---|
| NLG1/4-DS | G(PF)1/4″ | 5-7.8 | 13.157 | 8.5 | 19/19 |
| NLG3/8-DS | G(PF)3/8″ | 6-10 | 16.662 | 10 | 22/22 |
| NLG1/2-DS | G(PF)1/2″ | 7-12.5 | 20.955 | 10 | 27/24 |
| NLG3/4-DS | G(PF)3/4″ | 12.5-18 | 26.441 | 12 | 36/33 |
| NLG1-DS | G(PF)1″ | 17-25 | 33.249 | 15 | 46/41 |
| NLG11/4-DS | G(PF)1-1/4″ | 24-32 | 41.91 | 15 | 57/52 |
| NLG11/2-DS | G(PF)1-1/2″ | 31-41 | 48 | 22 | 60/62 |
| NLG2-DS | G(PF)2″ | 44-51 | 60 | 26 | 72/65 |
Nylon Cable Gland with Flexible Bend-Protection Tail
Nylon cable entry
Nylon Cable Gland with Flexible Bend-Protection Tail
Model specificationsPG and Metric threads
| Code | Model | Cable diameter range (mm) | Thread outside diameter L2 (mm) | Thread length L1 (mm) | Mounting hole (mm) | Joint length H (mm) | Spanner size (mm) |
|---|---|---|---|---|---|---|---|
| PG7-NFL | PG7 | 3~6.5 | 12.5 | 8 | 12.5 | 58 | 16 |
| PG9-NFL | PG9 | 4~8 | 15.2 | 8 | 15.2 | 73 | 19 |
| PG11-NFL | PG11 | 5~10 | 18.6 | 8 | 18.6 | 73 | 22 |
| PG13.5-NFL | PG13.5 | 6~12 | 20.4 | 9 | 20.4 | 80 | 24 |
| PG-16NFL | PG16 | 10~14 | 22.5 | 10 | 22.5 | 90 | 27 |
| PG21-NFL | PG21 | 13~18 | 28.3 | 10 | 28.3 | 105 | 33 |
| M12-NFL | M12 | 3~6.5 | 12 | 8 | 12 | 58 | 16 |
| M16-NFL | M16 | 4~8 | 16 | 8 | 16 | 73 | 19 |
| M18-NFL | M18 | 5~10 | 18 | 8 | 18 | 73 | 22 |
| M20-NFL | M20 | 6~12 | 20 | 9 | 20 | 80 | 24 |
| M22-NFL | M22 | 10~14 | 22 | 10 | 22 | 90 | 27 |
| M25-NFL | M25 | 13~18 | 25 | 10 | 25 | 105 | 33 |
| M27-NFL | M27 | 13~18 | 27 | 10 | 27 | 105 | 33 |
90-Degree Nylon Cable Gland
Nylon cable entry
90-Degree Nylon Cable Gland
Model specificationsPG thread
| Model | Cable diameter range (mm) | Thread length GL (mm) | Height H (mm) | Spanner Size (mm) | Thread outside diameter AG (mm) | Mounting hole diameter (mm) |
|---|---|---|---|---|---|---|
| NLWPG9 | 4-8 | 8 | 37 | 19 | 15.2 | 15.2-15.5 |
| NLWPG11 | 5-10 | 8 | 39 | 22 | 18.6 | 18.6-18.9 |
| NLWPG13.5 | 6-12 | 9 | 43 | 24 | 20.4 | 20.4-20.7 |
| NLWPG16 | 10-14 | 10 | 48 | 27 | 22.5 | 22.5-22.8 |
| NLWPG21 | 13-18 | 11 | 56 | 33 | 28.3 | 28.3-28.6 |
| NLWPG29 | 18-25 | 11 | 68 | 41/42 | 37 | 37-37.3 |
Model specificationsMetric thread
| Model | Cable diameter range (mm) | Thread length GL (mm) | Height H (mm) | Spanner Size (mm) | Thread outside diameter AG (mm) | Mounting hole diameter (mm) |
|---|---|---|---|---|---|---|
| NLWM16X1.5 | 4-8 | 8 | 37 | 19 | 16 | 16-16.3 |
| NLWM20X1.5 | 6-12 | 9 | 43 | 24 | 20 | 20-20.3 |
| NLWM22X1.5 | 10-14 | 10 | 48 | 27 | 22 | 22-22.3 |
| NLWM25X1.5 | 1348 | 11 | 56 | 33 | 25 | 25-25.3 |
| NLWM32X1.5 | 18-25 | 11 | 68 | 41/42 | 32 | 32-32.3 |
Extended-Thread Nylon Cable Gland
Nylon cable entry
Extended-Thread Nylon Cable Gland
Model specificationsPG thread
| Model | Thread O.D. (mm) | Mounting hole diameter (mm) | Thread Length (mm) | Body thickness (mm) | Cable diameter range (mm) | Spanner size A&F (mm) |
|---|---|---|---|---|---|---|
| PG7-L | 12.5 | Φ12.6-13 | 15 | 10 | 3-6.5 | 18/16 |
| PG7-L | 12.5 | Φ12.6-13 | 15 | 10 | 2~5 | 18/16 |
| PG9-L | 15.2 | Φ15.3-15.5 | 15 | 10 | 4~8 | 22/19 |
| PG9-L | 15.2 | Φ15.3-15.5 | 15 | 10 | 2-6 | 22/19 |
| PG11-L | 18.6 | Φ18.7-19 | 15 | 7-10 | 5-10 | 24/22 |
| PG11-L | 18.6 | Φ18.7-19 | 15 | 7-10 | 3~7 | 24/22 |
| PG13.5-L | 20.4 | Φ20.5-21 | 15 | 8-11 | 6-11 | 27/24 |
| PG13.5-L | 20.4 | Φ20.5-21 | 15 | 8-11 | 5-9 | 27/24 |
| PG1-L6 | 22.5 | Φ22.6-23 | 15 | 11 | 10-14 | 30/27 |
| PG16-L | 22.5 | Φ22.6-23 | 15 | 11 | 7-12 | 30/27 |
| PG21-L | 28.3 | Φ28.5-29 | 15 | 11 | 13-18 | 36/33 |
| PG21-L | 28.3 | Φ28.5-29 | 15 | 11 | 9-16 | 36/33 |
Model specificationsMetric thread
| Model | Entry thread | Mounting hole diameter (mm) | Thread Length (mm) | Body thickness (mm) | Cable diameter range (mm) | Spanner size A&F (mm) |
|---|---|---|---|---|---|---|
| M12-L | M12X1.5 | Φ12.2-12.5 | 15 | 10 | 3-3.5 | 18/16 |
| M12-L | M12X1.5 | Φ12.2-12.5 | 15 | 10 | 2-5 | 18/16 |
| M16-L | M16X1.5 | Φ16.2-16.5 | 15 | 10 | 4-8 | 22/19 |
| M16-L | M16X1.5 | Φ16.2-16.5 | 15 | 10 | 2-6 | 22/19 |
| M18-L | M18X1.5 | Φ18.2-18.5 | 15 | 10 | 5-10 | 24/22 |
| M18-L | M18X1.5 | Φ18.2-18.5 | 15 | 10 | 3-7 | 24/22 |
| M20-L | M20X1.5 | Φ20.2-20.5 | 15 | 11 | 6-12 | 27/24 |
| M20-L | M20X1.5 | Φ20.2-20.5 | 15 | 11 | 5-9 | 27/24 |
| M22-L | M22X1.5 | Φ22.2-22.5 | 15 | 11 | 10-14 | 30/27 |
| M22-L | M22X1.5 | Φ22.2-22.5 | 15 | 11 | 7-12 | 30/27 |
| M25-L | M25X1.5 | Φ25.2-25.5 | 15 | 11 | 13-18 | 33/33 |
| M25-L | M25X1.5 | Φ25.2-25.5 | 15 | 11 | 9-16 | 33/33 |
| M32-L | M32X1.5 | Φ32.2-32.5 | 15 | 11 | 18-25 | 39/36 |
| M32-L | M32X1.5 | Φ32.2-32.5 | 15 | 11 | 13-20 | 39/36 |
Multi-Hole Nylon Cable Gland
Nylon cable entry
Multi-Hole Nylon Cable Gland
Model specificationsMulti-hole seal sizes
| Seal layout | Code | Cable diameter range (mm) | Thread outside diameter C1 (mm) | Thread length C2 (mm) | Spanner size A&F (mm) |
|---|---|---|---|---|---|
![]() | NMA 12-H2-03 | 1.2−3 | 12 | 8.5 | 18/19 |
![]() | NMA 16-H2-04 | 1.5−4 | 16 | 15 | 22/22 |
![]() | NMA20-H2-06 | 3−6 | 20 | 15 | 27/27 |
![]() | NMA22-H2-06 | 3−6 | 22 | 10 | 27/27 |
![]() | NMA25-H2-6.5 | 3−6.5 | 25 | 15 | 33/33 |
![]() | NMA25-H2-08 | 4−8 | 25 | 15 | 33/33 |
![]() | NMA32-H2-10 | 5−10 | 32 | 15 | 41/42 |
![]() | NMA40-H2-13 | 7−13 | 40 | 20 | 50/52 |
![]() | NPGA7-H2-03 | 1.2−3 | 12.5 | 8.5 | 17/19 |
![]() | NPGA9-H2-03 | 1.2−3 | 15.2 | 8.5 | 22/19 |
![]() | NPGA11-H2-04 | 1.5−4 | 18.6 | 10 | 24/22 |
![]() | NPGA13.5-H2-05 | 2−5 | 20.4 | 10 | 27/24 |
![]() | NPGA16-H2-06 | 3−6 | 22.5 | 10.8 | 30/27 |
![]() | NPGA21-H2-6.5 | 3−6.5 | 28.3 | 12 | 36/33 |
![]() | NPGA21-H2-08 | 4−8 | 28.3 | 12 | 36/33 |
![]() | NPGA29-H2-10 | 6−10 | 37 | 12 | 46/41 |
![]() | NPGA36-H2-13 | 7−13 | 47 | 14 | 57/52 |
![]() | NGA1/4-H2-03 | 1.2−3 | 13.157 | 8 | 19/19 |
![]() | NGA3/8-H2-04 | 1.5−4 | 16.662 | 15 | 22/22 |
![]() | NGA 1 /2-H2-06 | 3−6 | 20.995 | 15 | 27/27 |
![]() | NGA 1/2-H2-6.5 | 3−6.5 | 20.995 | 15 | 27/33 |
![]() | NGA 1 /2-H2-08 | 4−8 | 20.995 | 15 | 27/33 |
![]() | NGA3/4-H2-6.5 | 3−6.5 | 26.441 | 15 | 36/33 |
![]() | NGA3/4-H2-08 | 4−8 | 26.441 | 15 | 36/33 |
![]() | NGA1 1/4-H2-13 | 7−13 | 41.91 | 16 | 57/52 |
![]() | NMA12-H3-2.6 | 1-2.6 | 12 | 8.5 | 18/19 |
![]() | NMA16-H3-04 | 1.5-4 | 16 | 15 | 22/22 |
![]() | NMA20S-H3-05 | 2-5 | 20 | 10 | 24/24 |
![]() | NMA20-H3-05 | 2-5 | 20 | 15 | 27/27 |
![]() | NMA22-H3-05 | 2-5 | 22 | 10 | 27/27 |
![]() | NMA25-H3-05 | 2-5 | 25 | 15 | 33/33 |
![]() | NMA25-H3-08 | 4-8 | 25 | 15 | 33/33 |
![]() | NMA32-H3-10 | 6-10 | 32 | 15 | 41/42 |
![]() | NMA40-H3-11 | 7-11 | 40 | 20 | 50/52 |
![]() | NMA50-H3-12 | 7-12 | 50 | 22 | 62/62 |
![]() | NMA63-H3-13 | 8-13 | 63 | 25 | 75/75 |
![]() | NPGA7-H3-2.6 | 1−2.6 | 12.5 | 8.5 | 17/19 |
![]() | NPGA9-H3-2.6 | 1−2.6 | 15.2 | 8.5 | 22/19 |
![]() | NPGA11-H3-04 | 1.5−4 | 18.6 | 10 | 24/22 |
![]() | NPGA13.5-H3-05 | 2−5 | 20.4 | 10 | 27/24 |
![]() | NPGA16-H3-05 | 2−5 | 22.5 | 10.8 | 30/27 |
![]() | NPGA21-H3-05 | 2−5 | 28.3 | 12 | 36/33 |
![]() | NPGA21-H3-08 | 4−8 | 28.3 | 12 | 36/33 |
![]() | NPGA29-H3-10 | 6−10 | 37 | 12 | 46/41 |
![]() | NPGA36-H3-11 | 7−11 | 47 | 14 | 57/52 |
![]() | NPGA42-H3-12 | 7−12 | 54 | 15 | 64/62 |
![]() | NPGA48-H3-13 | 8−13 | 59.3 | 18 | 70/65 |
![]() | NGA1/4-H3-2.6 | 1−2.6 | 13.157 | 8 | 19/19 |
![]() | NGA3/8-H3-04 | 1.5−4 | 16.662 | 15 | 22/22 |
![]() | NGA1/2-H3-05 | 2−5 | 20.995 | 15 | 27/27 |
![]() | NGA1/2-H3-05 | 2−5 | 20.995 | 15 | 27/33 |
![]() | NGA1/2-H3-08 | 4−8 | 20.995 | 15 | 27/33 |
![]() | NGA3/4-H3-05 | 2−5 | 26.441 | 15 | 36/33 |
![]() | NGA3/4-H3-08 | 4-8 | 26.441 | 15 | 36/33 |
![]() | NGA1 1/4-H3-11 | 7-11 | 41.91 | 16 | 57/52 |
![]() | NGA1 1/2-H3-12 | 7-12 | 48 | 22 | 60/62 |
![]() | NGA2-H3-13 | 8-13 | 60 | 25 | 75/75 |
![]() | NMA 12H4-2.3 | 1-2.3 | 12 | 8.5 | 18/19 |
![]() | NMA 16-H4-3.2 | 1-3.2 | 16 | 15 | 22/22 |
![]() | NMA20S-H4-04 | 1.5-4 | 20 | 10 | 24/24 |
![]() | NMA20-H4-2.5 | 1-2.5 | 20 | 15 | 27/27 |
![]() | NMA20-H4-3.5 | 1-3.5 | 20 | 15 | 27/27 |
![]() | NMA20-H4-4.5 | 2-4.5 | 20 | 15 | 27/27 |
![]() | NMA22-H4-2.5 | 1-2.5 | 22 | 15 | 27/27 |
![]() | NMA22-H4-3.5 | 1-3.5 | 22 | 15 | 27/27 |
![]() | NMA22-H4-4.5 | 2-4.5 | 22 | 15 | 27/27 |
![]() | NMA25-H4-05 | 2-5 | 25 | 15 | 33/33 |
![]() | NMA25-H4-06 | 3-6 | 25 | 15 | 33/33 |
![]() | NMA25-H4-07 | 3-7 | 25 | 15 | 33/33 |
![]() | NMA25-H4-08 | 4-8 | 25 | 15 | 33/33 |
![]() | NMA25-H4-09 | 5-9 | 25 | 15 | 33/33 |
![]() | NMA2-H4-07 | 3-7 | 32 | 15 | 41/42 |
![]() | NMA32-H4-09 | 5-9 | 32 | 15 | 41/42 |
![]() | NMA40-H4-11 | 7-11 | 40 | 20 | 50/52 |
![]() | NMA40-H4-12 | 7-12 | 40 | 20 | 50/52 |
![]() | NPGA7-H4-2.3 | 1-2.3 | 12.5 | 8.5 | 17/19 |
![]() | NPGA9-H4-2.3 | 1-2.3 | 15.2 | 8.5 | 22/19 |
![]() | NPGA 11-H4-3.2 | 1-3.2 | 18.6 | 10 | 24/22 |
![]() | NPGA 13.5-H4-04 | 1.5-4 | 20.4 | 10 | 27/24 |
![]() | NPGA 16-H4-2.5 | 1-2.5 | 22.5 | 10.8 | 30/27 |
![]() | NPGA 16-H4-3.5 | 1-3.5 | 22.5 | 10.8 | 30/27 |
![]() | NPGA 16-H4-4.5 | 2-4.5 | 22.5 | 10.8 | 30/27 |
![]() | NPGA21-H4-05 | 2-5 | 28.3 | 12 | 36/33 |
![]() | NPGA21-H4-06 | 3-6 | 28.3 | 12 | 36/33 |
![]() | NPGA21-H4-07 | 3-7 | 28.3 | 12 | 36/33 |
![]() | NPGA21-H4-08 | 4-8 | 28.3 | 12 | 36/33 |
![]() | NPGA21-H4-09 | 5-9 | 28.3 | 12 | 36/33 |
![]() | NPGA29-H4-07 | 3-7 | 37 | 12 | 46/41 |
![]() | NPGA29-H4-09 | 5-9 | 37 | 12 | 46/41 |
![]() | NPGA36-H4-11 | 7-11 | 47 | 14 | 57/52 |
![]() | NPGA36-H4-12 | 7-12 | 47 | 14 | 57/52 |
![]() | NGA 1 /4-H4-2.3 | 1-2.3 | 13.157 | 8 | 19/19 |
![]() | NGA3/8-H4-3.2 | 1-3.2 | 16.662 | 15 | 22/22 |
![]() | NGA 1 /2-H4-2.5 | 1-2.5 | 20.995 | 15 | 27/27 |
![]() | NGA 1 /2-H4-3.5 | 1-3.5 | 20.995 | 15 | 27/27 |
![]() | NGA 1 /2-H4-4.5 | 2-4.5 | 20.995 | 15 | 27/27 |
![]() | NGA 1 /2-H4-05 | 2-5 | 20.995 | 15 | 27/33 |
![]() | NGA 1 /2-H4-06 | 3-6 | 20.995 | 15 | 27/33 |
![]() | NGA 1 /2-H4-07 | 3-7 | 20.995 | 15 | 27/33 |
![]() | NGA 1 /2-H4-08 | 4-8 | 20.995 | 15 | 27/33 |
![]() | NGA 1 /2-H4-09 | 5-9 | 20.995 | 15 | 27/33 |
![]() | NGA3/4-H4-05 | 2-5 | 26.441 | 15 | 36/33 |
![]() | NGA/4-H4-06 | 3-6 | 26.441 | 15 | 36/33 |
![]() | NGA3/4-H4-07 | 3-7 | 26.441 | 15 | 36/33 |
![]() | NGA3/4-H4-08 | 4-8 | 26.441 | 15 | 36/33 |
![]() | NGA3/4-H4-09 | 5-9 | 26.441 | 15 | 36/33 |
![]() | NGA1 1/4-H4-11 | 7-11 | 41.91 | 16 | 57/52 |
![]() | NGA1 1/4-H4-12 | 7-12 | 41.91 | 16 | 57/52 |
![]() | NMA20-H5-03 | 1-3 | 20 | 15 | 27/27 |
![]() | NMA22-H5-03 | 1-3 | 22 | 10 | 27/27 |
![]() | NMA25-H5-06 | 3-6 | 25 | 15 | 33/33 |
![]() | NMA32-H5-08 | 4-8 | 32 | 15 | 41/42 |
![]() | NPGA 16-H5-03 | 1-3 | 22.5 | 10.8 | 30/27 |
![]() | NPGA21-H5-06 | 3-6 | 28.3 | 12 | 36/33 |
![]() | NPGA29-H5-08 | 4-8 | 37 | 12 | 46/41 |
![]() | NGA 1 /2-HS-03 | 1-3 | 20.995 | 15 | 27/27 |
![]() | NGA 1 /2-H5-06 | 3-6 | 20.995 | 15 | 27/33 |
![]() | NGA3/4-H5-06 | 3-6 | 26.441 | 15 | 33/33 |
![]() | NMA16A-H6-2.1 | 1-2.1 | 16 | 15 | 22/22 |
![]() | NMA25A-H6-5.3 | 2-5.3 | 25 | 15 | 33/33 |
![]() | NMA32A-H6-5.5 | 2-5.5 | 32 | 15 | 41/42 |
![]() | NMA32A-H6-07 | 3-7 | 32 | 15 | 41/42 |
![]() | NMA63A-H6-12 | 7-12 | 63 | 25 | 75/75 |
![]() | NPGA11-H6-2.1 | 1-2.1 | 18.6 | 10 | 24/22 |
![]() | NPGA21-H6-5.3 | 2-5.3 | 28.3 | 12 | 36/33 |
![]() | NPGA29-H6-5.5 | 2-5.5 | 37 | 12 | 46/41 |
![]() | NPGA29-H6-07 | 3-7 | 37 | 12 | 46/41 |
![]() | NPGA48-H6-12 | 7-12 | 59.3 | 18 | 70/65 |
![]() | NGA3/8-H6-2.1 | 1-2.1 | 16.662 | 15 | 22/22 |
![]() | NGA 1 /2-H6-5.3 | 2-5.3 | 20.995 | 15 | 27/33 |
![]() | NGA3/4-H6-5.3 | 2-5.3 | 26.441 | 15 | 33/33 |
![]() | NGA2-H6-12 | 7-12 | 60 | 25 | 75/75 |
![]() | NMA25-H7-4.3 | 2-4.3 | 25 | 15 | 33/33 |
![]() | NPGA21-H7-4.3 | 2-4.3 | 28.3 | 12 | 36/33 |
![]() | NGA 1 /2-H7-4.3 | 2-4.3 | 20.995 | 15 | 27/33 |
![]() | NGA3/4-H7-4.3 | 2-4.3 | 26.441 | 15 | 33/33 |
![]() | NMA25-H8-04 | 1.5-4 | 25 | 15 | 33/33 |
![]() | NPGA21-H8-04 | 1.5-4 | 28.3 | 12 | 36/33 |
![]() | NGA 1 /2-H8-04 | 1.5-4 | 20.995 | 15 | 27/33 |
![]() | NGA3/4-H8-04 | 1.5-4 | 26.441 | 15 | 33/33 |
![]() | NMA 10-0306 | 03*06 | 10 | 8 | 15/13 |
![]() | NMA25-0614 | 06*14 | 25 | 15 | 33/33 |
![]() | NMA32-0519 | 05*19 | 32 | 15 | 41/42 |
Nylon Corrugated Conduit Connector
Nylon cable entry
Nylon Corrugated Conduit Connector
Model specificationsConduit and entry sizes
| Model | Conduit size | Thread | Thread outside diameter Cl (mm) | Thread length C2 (mm) |
|---|---|---|---|---|
| M12-10 | AD 10 | M12*1.5 | 12 | 9 |
| M16-NC13 | AD 13 | M16*1.5 | 16 | 10 |
| M16-NC13L | AD 13 | M16*1.5 | 16 | 15 |
| M16-NC15.8 | AD 15.8 | M16*1.5 | 16 | 15 |
| M20-NC15.8 | AD 15.8 | M20*1.5 | 20 | 10 |
| M20-NC15.8L | AD 15.8 | M20*1.5 | 20 | 15 |
| M22-NC15.8 | AD 15.8 | M22*1.5 | 22 | 15 |
| M25-NC15.8 | AD 15.8 | M25*1.5 | 25 | 15 |
| M16-NC18.5 | AD18.5 | M16*1.5 | 16 | 15 |
| M20-NC18.5 | AD 18.5 | M20*1.5 | 20 | 10 |
| M20-NC18.5 | AD 18.5 | M20*1.5 | 20 | 15 |
| LM22-NC18.5 | AD 18.5 | M22*1.5 | 22 | 15 |
| M16-NC21.2 | AD21.2 | M16*1.5 | 16 | 15 |
| M20-NC21.2 | AD21.2 | M20*1.5 | 20 | 15 |
| M25-NC21.2 | AD21.2 | M25*1.5 | 25 | 10 |
| M25-NC21.2L | AD21.2 | M25*1.5 | 25 | 15 |
| M25-NC25 | AD25 | M25*1.5 | 25 | 15 |
| M25-NC28.5 | AD 28.5 | M25*1.5 | 25 | 15 |
| M32-NC34.5 | AD 34.5 | M32*1.5 | 32 | 15 |
| M40-NC42.5 | AD 42.5 | M40*1.5 | 40 | 15 |
| M5O-NC42.5 | AD 42.5 | M50*1.5 | 50 | 15 |
| M5O-NC48.5 | AD48.5 | M50*1.5 | 50 | 15 |
| M5O-NC54.5 | AD 54.5 | M50*1.5 | 50 | 22 |
| M63-NC54.5 | AD 54.5 | M63*1.5 | 63 | 25 |
| PG7-NC10 | AD 10 | PG7 | 12.5 | 9 |
| PG9-NC10 | AD 10 | PG9 | 15.2 | 9 |
| PG9-NC13 | AD 13 | PG9 | 15.2 | 10 |
| PG11-NC13 | AD 13 | PG11 | 18.6 | 10 |
| PG11-NC15.8 | AD 15.8 | PG11 | 18.6 | 10 |
| PG13.5-NC15.8 | AD 15.8 | PG13.5 | 20.4 | 10 |
| PG16-NC15.8 | AD 15.8 | PG16 | 22.5 | 10.8 |
| PG13.5-NC18.5 | AD 18.5 | PG13.5 | 20.4 | 10 |
| PG16-NC18.5 | AD 18.5 | PG16 | 22.5 | 10.8 |
| PG16-NC21.2 | AD21.2 | PG16 | 22.5 | 13 |
| PG21-NC21.2 | AD21.2 | PG21 | 28.3 | 13 |
| PG21-NC25 | AD25.0 | PG21 | 28.3 | 13 |
| PG21-NC28.5 | AD28.5 | PG21 | 28.3 | 13 |
| PG29-NC34.5 | AD34.5 | PG29 | 37 | 13 |
| PG36-NC42.5 | AD42.5 | PG36 | 47 | 15 |
| PG42-NC42.5 | AD42.5 | PG42 | 54 | 16 |
| PG42-NC48.0 | AD48.0 | PG42 | 54 | 16 |
| PG48-NC54.5 | AD54.5 | PG48 | 59.3 | 16 |
| PF1/4-NC10 | AD 10 | G(PF)1/4″ | 13.1 | 9 |
| PF3/8-NC13 | AD 13 | G(PF)3/8″ | 16.6 | 15 |
| PF1/2-NC15.8 | AD15.8 | G(PF)1/2″ | 20.9 | 15 |
| PF1/2-NC18.5 | AD 18.5 | G(PF)1/2″ | 20.9 | 15 |
| PF1/2-NC21.2 | AD21.2 | G(PF)1/2″ | 20.9 | 15 |
| PF3/4-NC21.2 | AD21.2 | G(PF)3/4″ | 26.4 | 15 |
| PF3/4-NC28.5 | AD28.5 | G(PF)3/4″ | 26.4 | 15 |
| PF1-NC34.5 | AD34.5 | G(PF)1″ | 33.2 | 15 |
| PF11/4-NC42.5 | AD42.5 | G(PF)1-1/4″ | 41.9 | 15 |
| PF11/2-NC54.5 | AD54.5 | G(PF)1-1/2″ | 48 | 15 |
| PF2-NC54.5 | AD54.5 | G(PF)2″ | 60 | 15 |
Quick-Connect Nylon Fitting for Corrugated Conduit
Nylon cable entry
Quick-Connect Nylon Fitting for Corrugated Conduit
Model specificationsMetric thread
| Conduit size (AD) | Entry thread | Pack quantity (pcs) |
|---|---|---|
| AD10 | M10*1.5 | 100 |
| AD10 | M12*1.5 | 100 |
| AD10 | M16*1.5 | 100 |
| AD13 | M12*1.5 | 100 |
| AD13 | M18*1.5 | 100 |
| AD15.8 | M16*1.5 | 100 |
| AD15.8 | M20*1.5 | 100 |
| AD18.5 | M20*1.5 | 50 |
| AD21.2 | M20*1.5 | 50 |
| AD21.2 | M25*1.5 | 50 |
| AD25 | M25*1.5 | 50 |
| AD28.5 | M27*1.5 | 50 |
| AD34.5 | M32*1.5 | 20 |
| AD34.5 | M36*1.5 | 20 |
| AD42.5 | M40*1.5 | 10 |
| AD54.5 | M50*1.5 | 10 |
Model specificationsPG thread
| Conduit size (AD) | Entry thread | Pack quantity (pcs) |
|---|---|---|
| AD10 | PG7 | 100 |
| AD13 | PG9 | 100 |
| AD15.8 | PG11 | 100 |
| AD18.5 | PG13.5 | 50 |
| AD21.2 | PG16 | 50 |
| AD28.5 | PG21 | 50 |
| AD34.5 | PG29 | 20 |
| AD42.5 | PG36 | 10 |
| AD54.5 | PG48 | 10 |
Nylon Waterproof Breathable Cable Gland
Nylon cable entry
Nylon Waterproof Breathable Cable Gland
Model specificationsNylon breathable connector dimensions
| Entry thread | Cable diameter (mm) | Airflow at 70 mbar (ml/min) | Thread diameter AG (mm) | Thread length GL (mm) | Spanner size (mm) | Protection rating |
|---|---|---|---|---|---|---|
| M12×1.5 | 4–8 | ≥100 | 12 | 9 | 19 | IP68 |
| M16×1.5 | 4–8 | ≥100 | 16 | 9 | 22 | IP68 |
| M16×1.5 | 5–10 | ≥100 | 16 | 9 | 22 | IP68 |
| M20×1.5 | 5–10 | ≥100 | 20 | 9 | 24 | IP68 |
Product comparison
Compare models
Compare the construction and application of each model.| Product | Construction | Use when | Check first | Review |
|---|---|---|---|---|
| One-Piece Nylon Cable Gland | Standard Nylon Cable Glands | A straight, unarmoured cable entry where keeping the sealing and clamping parts together simplifies assembly. |
| View specifications |
| Divided Nylon Cable Gland | Standard Nylon Cable Glands | An unarmoured cable entry where separate sealing and clamping parts are useful during assembly. |
| View specifications |
| Nylon Cable Gland with Flexible Bend-Protection Tail | Flexible Bend-Protection Glands | A cable exit that needs local bend support close to the gland. |
| View specifications |
| 90-Degree Nylon Cable Gland | Right-Angle Nylon Cable Glands | An enclosure with limited straight-out clearance or a cable path that must turn close to the entry. |
| View specifications |
| Extended-Thread Nylon Cable Gland | Extended-Thread Nylon Glands | A panel or threaded opening that needs more thread engagement than the standard gland provides. |
| View specifications |
| Multi-Hole Nylon Cable Gland | Multi-Hole Nylon Cable Glands | Several separate cables need to share one threaded entry. |
| View specifications |
| Nylon Corrugated Conduit Connector | Nylon Conduit Connectors | A corrugated conduit run needs a threaded connection to a box, machine or enclosure. |
| View specifications |
| Quick-Connect Nylon Fitting for Corrugated Conduit | Nylon Conduit Connectors | A corrugated conduit connection calls for a push-fit construction without a separate compression nut. |
| View specifications |
| Nylon Waterproof Breathable Cable Gland | Breathable Nylon Cable Glands | Cable sealing and ventilation in a lightweight nylon body. |
| View specifications |
Need a size that is not shown? Send us the cable diameter and entry thread.
Selection checks
Choose the right size and construction
Measure the cable diameter and identify the enclosure thread. These details determine which gland will fit.
- Cable outside diameterMeasure the cable jacket where it will sit in the seal.
- Entry thread and wallMatch the thread size and pitch, and allow enough thread length for the wall and locknut.
- Body form and bend clearanceChoose a straight, angled or flexible exit with room for the cable bend and tightening tools.
Product support
Need help choosing a cable gland?
Send a model name, a photo or a short question. We can help with sizes, samples and a quotation. If you have them, the details below help us narrow down the options.
Request product support- CableOutside diameter and cable type, if known.
- Armour or screenA cable cross-section photo can help identify the construction.
- Equipment entryThread marking, hole size or an entry drawing.
- Body and sealTell us if your project specifies a material.
- InstallationDescribe where the gland will be used and any heat, water or chemical exposure.
- Project requirementsInclude any required standard or certificate reference.
- Model or photoStart with a model number, a photo or a short question.
Nylon Cable Glands FAQ
Cable gland questions
Find answers about fit, assembly and product differences.
Nylon Cable Glands
01When should I choose a flexible or angled nylon gland?
A flexible exit supports the cable where it leaves the gland. An angled body changes the exit direction when a straight run would take too much space. Check the cable bend radius and clearance around the entry.
02What size cables fit a multi-hole nylon gland?
Each hole has its own sealing range. Match the outside diameter of every cable to its hole and use the specified blanking plugs for any unused holes.
One-Piece Nylon Cable Gland
One-Piece Nylon Cable Gland
01How does the one-piece gland differ from the divided version?
The one-piece design keeps the body, claw and seal together. The divided version separates these parts for access during assembly.
02Does an M thread size also specify the cable diameter?
No. The entry thread fits the enclosure, while the sealing range fits the cable jacket. Choose a model row that matches both dimensions.
Divided Nylon Cable Gland
Divided Nylon Cable Gland
01Why choose a divided nylon gland?
Its separate components give access to the seal and clamping parts before the gland is assembled. A one-piece gland keeps those components together.
02Can the divided gland be installed around an already terminated cable?
A divided construction does not by itself mean a split cable-entry system. The cable termination must fit through the relevant parts unless the assembly drawing explicitly allows another method.
Nylon Cable Gland with Flexible Bend-Protection Tail
Nylon Cable Gland with Flexible Bend-Protection Tail
01What does the flexible tail do?
It supports the cable near the enclosure entry, where an abrupt bend could concentrate movement. The cable still needs enough free length for its own minimum bend radius.
02Which temperature range applies when the cable moves?
Use the dynamic temperature range for a moving cable. Static and short-term limits describe different duties.
90-Degree Nylon Cable Gland
90-Degree Nylon Cable Gland
01When is a right-angle gland useful?
It is useful when adjacent equipment limits straight-out cable clearance. Allow room for the elbow, tightening tools and the cable bend beyond the outlet.
02Can a straight gland and this elbow use the same mounting position?
They may share a thread size, but the elbow needs additional sideways space. The installation also needs room to turn and tighten the body.
Extended-Thread Nylon Cable Gland
Extended-Thread Nylon Cable Gland
01How much thread length is needed for a thick panel?
Allow for the panel thickness, sealing washer and any locknut. The remaining engagement must suit the threaded opening or locknut used in the installation.
02Does a longer entry thread change the cable range?
Thread length and cable sealing range are separate dimensions. A longer thread does not make the same seal suitable for a larger cable.
Multi-Hole Nylon Cable Gland
Multi-Hole Nylon Cable Gland
01How is a multi-hole insert selected?
Choose the number of bores and each bore diameter from the actual outside diameter of every cable. A single overall bundle diameter is not enough.
02Can unused holes be left open?
An open bore leaves a path through the seal. Use the specified blanking arrangement or an insert with the required number of holes.
Nylon Corrugated Conduit Connector
Nylon Corrugated Conduit Connector
01Is this a cable gland or a conduit connector?
It grips and seals the corrugated conduit. Its fit is selected from the conduit profile and size, not from the diameter of a cable inside the conduit.
02How does it differ from the quick-connect fitting?
This version uses a sealing nut. The quick-connect version accepts the conduit through a push-fit connection without a separate compression nut.
Quick-Connect Nylon Fitting for Corrugated Conduit
Quick-Connect Nylon Fitting for Corrugated Conduit
01Does it use the same assembly method as the sealing-nut connector?
No. This fitting uses a push-fit conduit connection. The sealing-nut version retains the conduit by tightening a separate nut.
02Which dimensions identify the conduit size?
The conduit outside profile and nominal size identify the conduit end. The equipment-entry dimensions identify the other end; both are needed to choose the fitting.
Nylon Waterproof Breathable Cable Gland
Nylon Waterproof Breathable Cable Gland
01Which cable diameters fit?
Choose 4–8 mm or 5–10 mm according to the table; the M12 entry is offered for 4–8 mm cable.
02What is the airflow?
Each listed size has airflow of at least 100 ml/min at 70 mbar.