AI Search

Tell us in one sentence about your application or question to search related products, technical articles and calculators.

Waterproof Connectors / T topology

T-Branch Waterproof Connectors

Three-port T connectors for adding a branch to a cable run.

  • Circuit: Conductors shared between the main run and branch
  • Terminals: Pole count, conductor size and connection method
  • Three ports: Cable outside diameter at each entry
Product formsModel-specific constructions and connection layoutsModel sizesDimensions, connections and cable rangesApplication conditionsCable, mounting and environment vary by model

Waterproof connector groups

Inline joints and branched cable connections.

Inline connectors join two cables. T, Y and multi-way connectors route branches, with screw, push-in or lever terminals across the range.

T-Branch Waterproof Connectors range

Choose your t-branch waterproof connectors

T-shaped connectors join three cable routes in one body. The range offers different terminal arrangements for a main run and a side branch.

Choose one product or compare the full group

Models & specifications

T-Branch Waterproof Connectors: specifications and dimensions

Select a product to see its specifications, drawings and sizes.

Product selection

Match the T connector to the branch circuit.

Identify the conductors that join inside the body, then check the cable size at each of the three ports.
  • 01Circuit: Conductors shared between the main run and branch
  • 02Terminals: Pole count, conductor size and connection method
  • 03Three ports: Cable outside diameter at each entry
TXM20 Press-Terminal T-Connector

01 / Sealed wire connection

TXM20 Press-Terminal T-Connector

This TXM20 has three cable ports in a T-shaped body and press-type terminals. Its 2- and 3-contact configurations accept 0.5–2.5 mm² conductors.

Product reference

Product group
T-Branch Waterproof Connectors
Application
Create a three-cable T junction with press-operated terminals.

Key specifications

Product Type
Waterproof T-Connector / 3-Way Splice
Series / Model
TXM20
Shell Material
Nylon PA66
Conductor Material
Nickel-plated copper (Y2) and stainless steel

Product specifications

Construction and details

TXM20 Press-Terminal T-Connector — Terminal arrangement and dimensions
TXM20 Press-Terminal T-Connector

Terminal arrangement and dimensions

Use the current model instructions to confirm conductor preparation and terminal connections.

Read the marked dimensions with the current model drawing; do not infer sizes by measuring the illustration.

Model specification tables
TXM20 Press-Terminal T-Connector — Seal insert options
TXM20 Press-Terminal T-Connector

Seal insert options

Match the illustrated opening count and cable range to the actual cable and selected insert.

Further specifications
O-Ring Material
Silicone
IP Rating
IP68
Operating Temperature
-40°C to +105°C
Rated Voltage / Current
380V / 16A
Pin Counts Available
2, 3
Applicable Wire Size
0.5–2.5 mm²
Applicable Cable O.D.
5-8mm, 9-12mm
Termination
Press-type Quick Wiring Terminal (Tool-less)
Housing flammability
UL94 V-0
Storage temperature
Room temperature
Dielectric withstand voltage
1,500 V
Installation torque
0.6–0.8 N·m
Key features
  • Press-operated terminalsThe quick-wiring mechanism holds the conductors without terminal screws.
  • Cable-seal optionsSeal ranges cover 5–8 or 9–12 mm cable outside diameter.
  • Nylon body and silicone sealThe PA66 housing uses a silicone sealing ring.
TXM20 Screw-Terminal T-Connector

02 / Sealed wire connection

TXM20 Screw-Terminal T-Connector

This TXM20 uses screw terminals to connect three cables through a T-shaped body. It has 2- and 3-contact options for 0.5–4 mm² conductors.

Product reference

Product group
T-Branch Waterproof Connectors
Application
Create a three-cable T junction where screw terminals are preferred.

Key specifications

Product Type
Waterproof T-Connector / 3-Way Splice
Series / Model
TXM20
Shell Material
Nylon PA66
Conductor Material
Nickel-plated 59-1 brass

Product specifications

Construction and details

TXM20 Screw-Terminal T-Connector — Terminal arrangement and dimensions
TXM20 Screw-Terminal T-Connector

Terminal arrangement and dimensions

Use the current model instructions to confirm conductor preparation and terminal connections.

Read the marked dimensions with the current model drawing; do not infer sizes by measuring the illustration.

Model specification tables
TXM20 Screw-Terminal T-Connector — Contact faces and seal inserts
TXM20 Screw-Terminal T-Connector

Contact faces and seal inserts

Confirm the mating interface, contact arrangement and mounting dimensions for the selected model.

Match the illustrated opening count and cable range to the actual cable and selected insert.

Further specifications
O-Ring Material
Silicone
IP Rating
IP68
Operating Temperature
-40°C to +105°C
Rated Voltage / Current
400 V / 25 A
Pin Counts Available
2, 3
Applicable Wire Size
0.5–4 mm²
Applicable Cable O.D.
5-8mm, 9-12mm
Termination
Screw Terminal
Housing flammability
UL94 V-0
Storage temperature
Room temperature
Dielectric withstand voltage
2,500 V
Installation torque
0.6–0.8 N·m
Key features
  • Screw-terminal junctionScrews clamp the conductors inside the three-port housing.
  • Cable-seal optionsSeal ranges cover 5–8 or 9–12 mm cable outside diameter.
  • Nylon body and silicone sealThe PA66 housing uses a silicone sealing ring.
TXM25 Screw-Terminal T-Connector

03 / Sealed wire connection

TXM25 Screw-Terminal T-Connector

TXM25 connects three cables in a T-shaped body using screw terminals. The conductor range is 0.5–2.5 mm², with seal configurations for cable jackets up to 14 mm.

Product reference

Product group
T-Branch Waterproof Connectors
Application
Build a three-way screw-terminal splice where the TXM25 conductor and seal ranges suit the cables.

Key specifications

Product Type
Waterproof T-Connector / 3-Way Splice
Series / Model
TXM25
Shell Material
Nylon PA66
Conductor Material
Nickel-plated 59-1 brass

Product specifications

Construction and details

TXM25 Screw-Terminal T-Connector — Terminal arrangement and dimensions
TXM25 Screw-Terminal T-Connector

Terminal arrangement and dimensions

Use the current model instructions to confirm conductor preparation and terminal connections.

Read the marked dimensions with the current model drawing; do not infer sizes by measuring the illustration.

Model specification tables
TXM25 Screw-Terminal T-Connector — Contact faces and seal inserts
TXM25 Screw-Terminal T-Connector

Contact faces and seal inserts

Confirm the mating interface, contact arrangement and mounting dimensions for the selected model.

Match the illustrated opening count and cable range to the actual cable and selected insert.

Further specifications
O-Ring Material
Silicone
IP Rating
IP68
Operating Temperature
-40°C to +105°C
Rated Voltage / Current
380 V / 25 A
Pin Counts Available
2, 3, 4, 5
Applicable Wire Size
0.5–2.5 mm²
Applicable Cable O.D.
5-8mm, 9-12mm, 10-14mm
Termination
Screw Terminal
Housing flammability
UL94 V-0
Storage temperature
Room temperature
Dielectric withstand voltage
1,500 V
Installation torque
0.6–0.8 N·m
Key features
  • Three cable portsThe T-shaped housing provides three cable-entry positions.
  • Cable-seal optionsSeal ranges cover 5–8, 9–12 or 10–14 mm cable outside diameter.
  • Nylon body and silicone sealThe PA66 housing uses a silicone sealing ring.

Model specification tables

Model sizes and specifications

Open a table to compare model sizes and connection details.
TXM20 Press-Terminal T-Connector

T-Branch Waterproof Connectors

TXM20 Press-Terminal T-Connector

Model specificationsTXM20 — model specifications
ModelTXM20-06TXM20-07TXM20-08TXM20-09
Quantity/bag10101010
Core2 Core2 Core3 Core3 Core
Cable range(mm)5-89-125-89-12
Per Pcs weight(g)61.860.466.264.8
One carton weight(kg)15.815.51716.5
TXM20 Screw-Terminal T-Connector

T-Branch Waterproof Connectors

TXM20 Screw-Terminal T-Connector

Model specificationsTXM20 — model specifications
ModelTXM20-10TXM20-11TXM20-12TXM20-13
Quantity/bag10101010
Core2 Core2 Core3 Core3 Core
Cable range(mm)5-89-125-89-12
Per Pcs weight(g)6967.877.175.3
One carton weight(kg)17.517.319.519.1
TXM25 Screw-Terminal T-Connector

T-Branch Waterproof Connectors

TXM25 Screw-Terminal T-Connector

Model specificationsTXM25 — model specifications
ModelTXM 25-31TXM 25-32TXM 25-33TXM 25-34TXM 25-31TXM 25-32TXM 25-33TXM 25-34TXM 25-31TXM 25-32TXM 25-33TXM 25-34
Quantity/bag555555555555
Core2 Core2 Core2 Core3 Core3 Core3 Core4 Core4 Core4 Core5 Core5 Core5 Core
Cable range(mm)5-89-1210-145-89-1210-145-89-1210-145-89-1210-14
Per Pcs weight(g)63.862.661.465.864.663.467.866.665.269.868.667.4
One carton weight(kg)24.323.923.52524.624.225.825.324.826.52625.6

Need help matching an existing part? Send us its model name or a photo.

Selection checks

Choose the right model

T-shaped connectors join three cable routes in one body. The range offers different terminal arrangements for a main run and a side branch.

  1. CircuitConductors shared between the main run and branch
  2. TerminalsPole count, conductor size and connection method
  3. Three portsCable outside diameter at each entry

Product support

Need a model recommendation or a quote?

Send a model name, a photo or a short question. We can help with product selection, samples and pricing. Share any of the details below that you already have.

Request product support
  • T-connector model or wiring sketchSend a model or a simple sketch of the main cable run and its side branch.
  • Pole count and conductor sizeInclude the number of conductors and their cross-section if available.
  • Cable diameter at all three portsList the jacket diameter of the two main-run cables and the branch cable, if known.
  • Circuit voltage and currentInclude the circuit voltage and the current the connection will carry, if known.

T-Branch Waterproof Connectors FAQ

Product questions

Find answers about fit, wiring and product differences.

T-Branch Waterproof Connectors

01Does a T shape tell me which conductors connect?

No. The shape shows the cable routes. Check the terminal layout to see how each conductor connects between the three entries.

02Do all three ports accept the same cable size?

Do not assume so. Compare the cable sealing range for each port with the diameter of the cable that will enter it.

TXM20 Press-Terminal T-Connector

TXM20 Press-Terminal T-Connector

01Which TXM20 models use the press-type terminal?

The press-terminal range uses TXM20-06 through TXM20-09. The screw-terminal range has separate model numbers, TXM20-10 through TXM20-13.

02Which cable diameters fit this TXM20?

The seal options cover 5–8 or 9–12 mm. These are cable-jacket diameters, separate from the conductor cross-section.

TXM20 Screw-Terminal T-Connector

TXM20 Screw-Terminal T-Connector

01Which screw-terminal TXM20 fits a 3-contact, 9–12 mm cable connection?

TXM20-13 provides 3 contacts with the 9–12 mm cable seal. TXM20-12 uses the same contact count with a 5–8 mm seal.

02Which cable diameters fit this TXM20?

The seal options cover 5–8 or 9–12 mm. These are cable-jacket diameters, separate from the conductor cross-section.

TXM25 Screw-Terminal T-Connector

TXM25 Screw-Terminal T-Connector

01How does TXM25 differ from the screw-terminal TXM20?

TXM25 has a 0.5–2.5 mm² conductor range and includes a 10–14 mm cable-seal option. The screw-terminal TXM20 accepts 0.5–4 mm² conductors with 5–8 or 9–12 mm cable seals.

02Which cable diameters fit this TXM25?

The seal options cover 5–8, 9–12 or 10–14 mm. These are cable-jacket diameters, separate from the conductor cross-section.

03Can I order TXM25 by the model code alone?

No. Some TXM25 codes occur with more than one contact count or cable seal. Include the contact count and cable outside diameter with the code so the required configuration is unambiguous.