Our Low-Profile Hex Protective Vent provides IP68 protection with a sleek, flush-mount design. Made from nickel-plated brass, it equalizes pressure and prevents condensation in outdoor enclosures.
Key Features

| Product Number (Code) |
Metric thread (M) |
Material | Thread Length
(GL) |
Thread O.D.
(AG) |
Total Height (H) |
Waterproof Grade | Air Permeability | Spanner Size (A&F) |
| HT-T001PLJ | M5×0.8 | Brass nickel plated | 5mm | 5mm | 9.2mm | IP68 | ≥200ml/min/@70mbar | 8 |
| HT-T002PLJ | M6×1 | Brass nickel plated | 5mm | 6mm | 9.2mm | IP68 | ≥200ml/min/@70mbar | 10 |
| HT-T003PLJ | M8×1.25 | Brass nickel plated | 7mm | 8mm | 12mm | IP68 | ≥550ml/min/@70mbar | 12 |
| HT-T003A1PLJ | M8×1 | Brass nickel plated | 8mm | 7mm | 12mm | IP68 | ≥800ml/min/@70mbar | 12 |
| HT-T005PLJ | M10×1.5 | Brass nickel plated | 8mm | 10mm | 13mm | IP68 | ≥600ml/min/@70mbar | 14 |
| HT-T006PLJ | M12×1.5 | Brass nickel plated | 8mm | 12mm | 13mm | IP68 | ≥1200ml/min/@70mbar | 16 |
| HT-T007PLJ | M12×1.5 | Brass nickel plated | 10mm | 12mm | 15mm | IP68 | ≥1200ml/min/@70mbar | 16 |
| HT-T008PLJ | M16×1.5 | Brass nickel plated | 10mm | 16mm | 15mm | IP68 | ≥2300ml/min/@70mbar | 20 |
| HT-T010PLJ | M20×1.5 | Brass nickel plated | 10mm | 20mm | 15mm | IP68 | ≥2300ml/min/@70mbar | 12 |