Enclosure Accessories / Waterproof Vents & Valves
Waterproof Vents & Valves
Waterproof vents, explosion-proof valves, relief valves and membranes. Compare materials, airflow, opening pressure and mounting dimensions.
- Vent and valve function: Venting, pressure relief or both
- Flow requirement: Airflow, pressure difference and flow direction
- Mounting: Thread or opening size and enclosure-wall thickness
Vent categories
Choose a vent by material and function.
Browse plastic and metal vents, explosion-proof valves, relief valves and membranes.
Waterproof Vents & Valves range
Choose a vent or valve.
Choose the material and mounting form, then compare airflow and opening pressure for your enclosure.
01Plastic Waterproof VentsThreaded and snap-in nylon vents for enclosure pressure equalization.
02Stainless Steel Waterproof VentsStainless steel vents with standard, flat-hex and slotted heads.
03Nickel-Plated Brass Waterproof VentsThreaded brass vents with nickel-plated bodies.
04Aluminum Alloy Waterproof VentsLightweight metal vents in threaded and low-profile forms.
05Waterproof Breathable Explosion-Proof ValvesB/H series and battery-pack valves combine normal breathing with pressure release.
06Safety One-Way Pressure-Relief ValvesD and S series relief valves, metal filters and push-button exhaust valves.
- D03 Aluminum One-Way Pressure-Relief Valve
- D01 Stainless Steel One-Way Pressure-Relief Valve
- D02 Stainless Steel One-Way Pressure-Relief Valve
- D10 Aluminum One-Way Pressure-Relief Valve
- D10Y Aluminum One-Way Pressure-Relief Valve
- D10Y1 Aluminum One-Way Pressure-Relief Valve
- S07/S09 Aluminum Pressure-Relief Valve
- S10 Aluminum Pressure-Relief Valve
- S10Y Aluminum Pressure-Relief Valve
- G10/G16 Aluminum Filter Valve
- M02/G01 Push-Button Quick-Exhaust Valve
07Plastic Vent CapsTQM caps with ePTFE membranes and model-specific mounting holes.
08Plastic Waterproof Breathable PlugsD15, D17, W17 and D38 press-in plugs with HDPE bodies.
09Metal Humidity IndicatorsThreaded indicators for checking humidity inside an enclosure.
10Waterproof Breathable MembranesePTFE membranes in rolls and die-cut pieces for enclosure vents.
Models & specifications
Waterproof Vents & Valves: specifications and dimensions
Select a product to see its specifications, drawings and sizes.
Product selection
Choose a vent or valve.
Choose continuous venting, pressure relief at a set opening pressure, or both functions in one valve. Then choose the mounting size.- 01Vent and valve function: Venting, pressure relief or both
- 02Flow requirement: Airflow, pressure difference and flow direction
- 03Mounting: Thread or opening size and enclosure-wall thickness
PA66 Compact Threaded Waterproof Breathable Vent
01 / Enclosure openings
PA66 Compact Threaded Waterproof Breathable Vent
A threaded PA66 vent with a compact hexagonal cap and silicone O-ring. Select the thread, body height and airflow together; two M12×1.5 options have different heights and flow rates.
Product reference
- Product group
- Plastic Waterproof Vents
- Application
- A small threaded enclosure opening needs a breathable vent.
Key specifications
- Product Type
- Compact PA66 vent
- Body material
- PA66
- Temperature resistance
- −40°C to +125°C
- Ingress protection
- IP67
Product specifications
Construction and details

Product views and dimensions
Read the marked dimensions with the current model drawing; do not infer sizes by measuring the illustration.
Model specification tablesFurther specifications
- Color / finish
- Black, gray or white
- Moisture permeability
- >5,000 g/(24 h·m²)
- Static water pressure resistance
- >100 mbar for 30 minutes
- Area-normalized airflow at 70 mbar
- ≥1.2 L/(min·cm²); customizable
- O-ring material
- Silicone rubber
Key features
- Body materialPA66.
- Mounting-face sealSilicone rubber.
PA66 Large Threaded Waterproof Breathable Vent
02 / Enclosure openings
PA66 Large Threaded Waterproof Breathable Vent
A PA66 vent with a broad hexagonal body for M16 to M42 entries. Whole-valve airflow ranges from 4,500 to 8,500 mL/min at 70 mbar across the listed sizes.
Product reference
- Product group
- Plastic Waterproof Vents
- Application
- A larger metric opening needs higher airflow.
Key specifications
- Product Type
- Large-thread PA66 vent
- Body material
- PA66
- Temperature resistance
- −40°C to +125°C
- Ingress protection
- IP67
Product specifications
Construction and details

Product views and dimensions
Read the marked dimensions with the current model drawing; do not infer sizes by measuring the illustration.
Model specification tablesFurther specifications
- Color / finish
- Black, gray or white
- Moisture permeability
- >5,000 g/(24 h·m²)
- Static water pressure resistance
- >100 mbar for 30 minutes
- Area-normalized airflow at 70 mbar
- ≥1.2 L/(min·cm²); customizable
Key features
- Body materialPA66.
K01–K03 PA66 Snap-in Waterproof Breathable Vent
03 / Enclosure openings
K01–K03 PA66 Snap-in Waterproof Breathable Vent
A black PA66 snap-in vent available in K01, K02 and K03 sizes. Compare the snap dimensions and overall height before choosing the panel opening.
Product reference
- Product group
- Plastic Waterproof Vents
- Application
- A nylon vent must snap into an unthreaded panel opening.
Key specifications
- Product Type
- K01 / K02 / K03
- Body material
- PA66 body and cover
- Temperature resistance
- −40°C to +125°C
- Ingress protection
- IP67
Product specifications
Construction and details

Product views and dimensions
Read the marked dimensions with the current model drawing; do not infer sizes by measuring the illustration.
Model specification tablesFurther specifications
- Models
- K01, K02, K03
- Color
- Black
- Membrane
- ePTFE, or non-woven PET with ePTFE
- O-ring material
- Silicone rubber
- Storage temperature
- Room temperature
- Moisture permeability
- >5,000 g/(24 h·m²)
- Static water pressure resistance
- 100 mbar for 30 minutes
Key features
- Body materialPA66 body and cover.
- Mounting-face sealSilicone rubber.
Stainless Steel Threaded Waterproof Breathable Vent
04 / Enclosure openings
Stainless Steel Threaded Waterproof Breathable Vent
A stainless steel vent with side air ports and a hexagonal mounting body. Metric, G and NPT options have separate dimensional rows.
Product reference
- Product group
- Stainless Steel Waterproof Vents
- Application
- Enclosure ventilation with a stainless steel body.
Key specifications
- Product Type
- Stainless threaded vent
- Body material
- 304 or 316 stainless steel
- Temperature resistance
- −40°C to +150°C
- Ingress protection
- IP68
Product specifications
Construction and details

Product views and dimensions
Read the marked dimensions with the current model drawing; do not infer sizes by measuring the illustration.
Model specification tables
Product views and dimensions
Read the marked dimensions with the current model drawing; do not infer sizes by measuring the illustration.
Model specification tablesFurther specifications
- Color / finish
- Natural metal finish
- Moisture permeability
- >5,000 g/(24 h·m²)
- Static water pressure resistance
- >100 mbar for 30 minutes
- Area-normalized airflow at 70 mbar
- ≥1.2 L/(min·cm²); customizable
Key features
- Body material304 or 316 stainless steel.
Low-profile Hex Stainless Steel Waterproof Breathable Vent
05 / Enclosure openings
Low-profile Hex Stainless Steel Waterproof Breathable Vent
A low-profile stainless steel vent with a hexagonal cap, side air ports and silicone O-ring. The M12×1.5 thread is available in two body and thread lengths.
Product reference
- Product group
- Stainless Steel Waterproof Vents
- Application
- A low-profile stainless vent is needed at the enclosure surface.
Key specifications
- Product Type
- Stainless flat-hex vent
- Body material
- 304 or 316 stainless steel
- Temperature resistance
- −40°C to +150°C
- Ingress protection
- IP68
Product specifications
Construction and details

Product views and dimensions
Read the marked dimensions with the current model drawing; do not infer sizes by measuring the illustration.
Model specification tablesFurther specifications
- Color / finish
- Natural metal finish
- Moisture permeability
- >5,000 g/(24 h·m²)
- Static water pressure resistance
- >100 mbar for 30 minutes
- Area-normalized airflow at 70 mbar
- ≥1.2 L/(min·cm²); customizable
- O-ring material
- Silicone rubber
Key features
- Body material304 or 316 stainless steel.
- Mounting-face sealSilicone rubber.
Round Slotted Stainless Steel Waterproof Breathable Vent
06 / Enclosure openings
Round Slotted Stainless Steel Waterproof Breathable Vent
A round stainless steel vent driven by a single screwdriver slot. The table lists head outside diameter rather than a hexagonal spanner size.
Product reference
- Product group
- Stainless Steel Waterproof Vents
- Application
- A round stainless vent head with screwdriver access.
Key specifications
- Product Type
- Stainless round-slotted vent
- Body material
- 304 or 316 stainless steel
- Temperature resistance
- −40°C to +150°C
- Ingress protection
- IP68
Product specifications
Construction and details

Product views and dimensions
Read the marked dimensions with the current model drawing; do not infer sizes by measuring the illustration.
Model specification tablesFurther specifications
- Color / finish
- Natural metal finish
- Moisture permeability
- >5,000 g/(24 h·m²)
- Static water pressure resistance
- >100 mbar for 30 minutes
- Area-normalized airflow at 70 mbar
- ≥1.2 L/(min·cm²); customizable
- Drive
- Single slot
Key features
- Body material304 or 316 stainless steel.
Slotted Stainless Steel Waterproof Breathable Vent with Hex Base
07 / Enclosure openings
Slotted Stainless Steel Waterproof Breathable Vent with Hex Base
A tall slotted stainless steel vent with a hexagonal base. M5×0.8 and M6×1 versions share a 16 mm overall length and a minimum airflow of 300 mL/min at 70 mbar.
Product reference
- Product group
- Stainless Steel Waterproof Vents
- Application
- A slotted stainless vent with a hexagonal mounting base.
Key specifications
- Product Type
- Stainless hex-base slotted vent
- Body material
- 304 or 316 stainless steel
- Temperature resistance
- −40°C to +150°C
- Ingress protection
- IP68
Product specifications
Construction and details

Product views and dimensions
Read the marked dimensions with the current model drawing; do not infer sizes by measuring the illustration.
Model specification tablesFurther specifications
- Color / finish
- Natural metal finish
- Moisture permeability
- >5,000 g/(24 h·m²)
- Static water pressure resistance
- >100 mbar for 30 minutes
- Area-normalized airflow at 70 mbar
- ≥1.2 L/(min·cm²); customizable
- Drive
- Single slot or hexagonal base
Key features
- Body material304 or 316 stainless steel.
Nickel-plated Brass Threaded Waterproof Breathable Vent
08 / Enclosure openings
Nickel-plated Brass Threaded Waterproof Breathable Vent
A nickel-plated brass vent with a round cap and hexagonal mounting body. Metric, G and NPT rows list airflow, mounting lengths and wrench size separately.
Product reference
- Product group
- Nickel-Plated Brass Waterproof Vents
- Application
- A nickel-plated brass body for a threaded enclosure vent.
Key specifications
- Product Type
- Nickel-plated brass vent
- Body material
- Nickel-plated brass
- Temperature resistance
- −40°C to +150°C
- Ingress protection
- IP68
Product specifications
Construction and details

Product views and dimensions
Read the marked dimensions with the current model drawing; do not infer sizes by measuring the illustration.
Model specification tables
Product views and dimensions
Read the marked dimensions with the current model drawing; do not infer sizes by measuring the illustration.
Model specification tablesFurther specifications
- Color / finish
- Nickel-plated finish
- Moisture permeability
- >5,000 g/(24 h·m²)
- Static water pressure resistance
- >100 mbar for 30 minutes
- Area-normalized airflow at 70 mbar
- ≥1.2 L/(min·cm²); customizable
Key features
- Body materialNickel-plated brass.
Low-profile Hex Nickel-plated Brass Waterproof Breathable Vent
09 / Enclosure openings
Low-profile Hex Nickel-plated Brass Waterproof Breathable Vent
A low-profile nickel-plated brass vent with a hexagonal cap and silicone O-ring. M12×1.5 versions are available with 8 mm or 10 mm thread length.
Product reference
- Product group
- Nickel-Plated Brass Waterproof Vents
- Application
- A low-profile nickel-plated brass enclosure vent.
Key specifications
- Product Type
- Brass flat-hex vent
- Body material
- Nickel-plated brass
- Temperature resistance
- −40°C to +150°C
- Ingress protection
- IP68
Product specifications
Construction and details

Product views and dimensions
Read the marked dimensions with the current model drawing; do not infer sizes by measuring the illustration.
Model specification tablesFurther specifications
- Color / finish
- Nickel-plated finish
- Moisture permeability
- >5,000 g/(24 h·m²)
- Static water pressure resistance
- >100 mbar for 30 minutes
- Area-normalized airflow at 70 mbar
- ≥1.2 L/(min·cm²); customizable
- O-ring material
- Silicone rubber
Key features
- Body materialNickel-plated brass.
- Mounting-face sealSilicone rubber.
Aluminum Threaded Waterproof Breathable Vent
10 / Enclosure openings
Aluminum Threaded Waterproof Breathable Vent
An aluminum vent with a round cap and hexagonal mounting body. Select the thread and length together; M12 finish variants and M16 length variants remain separate options.
Product reference
- Product group
- Aluminum Alloy Waterproof Vents
- Application
- A lightweight metal vent for a threaded enclosure opening.
Key specifications
- Product Type
- Aluminum threaded vent
- Body material
- Aluminum alloy
- Temperature resistance
- −40°C to +150°C
- Ingress protection
- IP68
Product specifications
Construction and details

Product views and dimensions
Read the marked dimensions with the current model drawing; do not infer sizes by measuring the illustration.
Model specification tablesFurther specifications
- Color / finish
- Oxidized, bright or black finish
- Moisture permeability
- >5,000 g/(24 h·m²)
- Static water pressure resistance
- >100 mbar for 30 minutes
- Area-normalized airflow at 70 mbar
- ≥1.2 L/(min·cm²); customizable
Key features
- Body materialAluminum alloy.
Black Aluminum Slotted Waterproof Breathable Vent
11 / Enclosure openings
Black Aluminum Slotted Waterproof Breathable Vent
A black aluminum vent with a round head and a screwdriver slot. M5×0.8 and M6×1 versions have a 10 mm head diameter and a 6.5 mm thread length.
Product reference
- Product group
- Aluminum Alloy Waterproof Vents
- Application
- A small black aluminum vent with screwdriver access.
Key specifications
- Product Type
- Aluminum slotted vent
- Body material
- Aluminum alloy
- Temperature resistance
- −40°C to +150°C
- Ingress protection
- IP68
Product specifications
Construction and details

Product views and dimensions
Read the marked dimensions with the current model drawing; do not infer sizes by measuring the illustration.
Model specification tablesFurther specifications
- Color / finish
- Black oxidized
- Moisture permeability
- >5,000 g/(24 h·m²)
- Static water pressure resistance
- >100 mbar for 30 minutes
- Area-normalized airflow at 70 mbar
- ≥1.2 L/(min·cm²); customizable
- Drive
- Single slot
Key features
- Body materialAluminum alloy.
B Series Waterproof Breathable Explosion-Proof Valve
12 / Enclosure openings
B Series Waterproof Breathable Explosion-Proof Valve
B10, B15, B25 and B55 valves combine enclosure breathing with pressure release at 4–15 kPa. Choose the model by material, mounting thread and airflow.
Product reference
- Product group
- Waterproof Breathable Explosion-Proof Valves
- Application
- Enclosure breathing and pressure release.
Key specifications
- Models
- FBFBXG-B10 / FBFLC-B10 / FBFLC-B15 / FBFLC-B25 / FBFLC-B55
- Material options
- 304 stainless steel or 6061 aluminum
- Ingress protection
- IP67
- Opening pressure
- 4–15 kPa
Product specifications
Construction and details

Product views and dimensions
Read the marked dimensions with the current model drawing; do not infer sizes by measuring the illustration.
Model specification tables
Product views and dimensions
Read the marked dimensions with the current model drawing; do not infer sizes by measuring the illustration.
Model specification tables
Product views and dimensions
Read the marked dimensions with the current model drawing; do not infer sizes by measuring the illustration.
Model specification tables
Product views and dimensions
Read the marked dimensions with the current model drawing; do not infer sizes by measuring the illustration.
Model specification tables
Product views and dimensions
Read the marked dimensions with the current model drawing; do not infer sizes by measuring the illustration.
Model specification tablesFurther specifications
- Continuous operating temperature
- -40°C to +120°C
- Temperature resistance
- -40°C to +150°C
- Flammability class
- UL94 V-0
Key features
- Pressure releaseThe valve opens within a 4–15 kPa pressure range.
- Material optionsB10 has 304 stainless steel and 6061 aluminum versions. B15, B25 and B55 use 6061 aluminum.
H Series Waterproof Breathable Explosion-Proof Valve
13 / Enclosure openings
H Series Waterproof Breathable Explosion-Proof Valve
H15, H25 and H55 are 6061 aluminum valves for enclosure breathing and pressure release at 4–15 kPa. Airflow and mounting dimensions vary by model.
Product reference
- Product group
- Waterproof Breathable Explosion-Proof Valves
- Application
- Enclosure breathing and pressure release.
Key specifications
- Models
- FBFLC-H15 / FBFLC-H25 / FBFLC-H55
- Body material
- 6061 aluminum
- Ingress protection
- IP67
- Opening pressure
- 4–15 kPa
Product specifications
Construction and details

Product views and dimensions
Read the marked dimensions with the current model drawing; do not infer sizes by measuring the illustration.
Model specification tables
Product views and dimensions
Read the marked dimensions with the current model drawing; do not infer sizes by measuring the illustration.
Model specification tables
Product views and dimensions
Read the marked dimensions with the current model drawing; do not infer sizes by measuring the illustration.
Model specification tablesFurther specifications
- Continuous operating temperature
- -40°C to +120°C
- Temperature resistance
- -40°C to +150°C
- Flammability class
- UL94 V-0
Key features
- Pressure releaseThe valve opens within a 4–15 kPa pressure range.
- Body materialThe valve has a 6061 aluminum body.
F550 Battery-Pack Waterproof Breathable Explosion-Proof Vent
14 / Enclosure openings
F550 Battery-Pack Waterproof Breathable Explosion-Proof Vent
A battery-pack vent with a glass-fiber-reinforced polypropylene body, stainless steel cover and ePTFE membrane. It equalizes enclosure pressure during normal operation and releases pressure at 20–50 kPa.
Product reference
- Product group
- Waterproof Breathable Explosion-Proof Valves
- Application
- Enclosure breathing and pressure release.
Key specifications
- Model
- FBFSL-F550
- Body material
- PP with 30% glass fiber
- Ingress protection
- IP67
- Opening pressure
- 20–50 kPa
Product specifications
Construction and details

Product views and dimensions
Read the marked dimensions with the current model drawing; do not infer sizes by measuring the illustration.
Model specification tablesFurther specifications
- Cover material
- 304 stainless steel
- Membrane material
- ePTFE
- Seal material
- Silicone rubber
- Temperature resistance
- -40°C to +125°C
- Airflow at 7 kPa
- ≥6,000 ml/min
- Flammability class
- V-0
- Color
- Black
- Storage temperature
- Room temperature
- Optional ingress protection
- IP68 or IP69K
Key features
- Pressure releaseThe valve opens within a 20–50 kPa pressure range.
- Body materialThe valve has a PP with 30% glass fiber body.
D03 Aluminum One-Way Pressure-Relief Valve
15 / Enclosure openings
D03 Aluminum One-Way Pressure-Relief Valve
A compact M14×1 aluminum pressure-relief valve with an opening-pressure range of 10–30 kPa. The body is 16 mm high and installs at 1–3 N·m.
Product reference
- Product group
- Safety One-Way Pressure-Relief Valves
- Application
- Controlled release of pressure from an enclosure.
Key specifications
- Model
- DXFLC-D03
- Body material
- 6061 aluminum
- Ingress protection
- IP68
- Mounting thread
- M14×1
Product specifications
Construction and details

Product views and dimensions
Read the marked dimensions with the current model drawing; do not infer sizes by measuring the illustration.
Model specification tablesFurther specifications
- Opening pressure
- 10–30 kPa (±3 kPa)
- Continuous operating temperature
- -40°C to +120°C
- Temperature resistance
- -40°C to +150°C
- Installation torque
- 1–3 N·m
- Flammability class
- UL94 V-0
Key features
- Pressure releaseThe valve opens within a 10–30 kPa (±3 kPa) pressure range.
- Body materialThe valve has a 6061 aluminum body.
D01 Stainless Steel One-Way Pressure-Relief Valve
16 / Enclosure openings
D01 Stainless Steel One-Way Pressure-Relief Valve
A small M10×1 stainless steel valve for pressure release in the 150–200 kPa range. The 13 mm body uses a 7 mm thread length.
Product reference
- Product group
- Safety One-Way Pressure-Relief Valves
- Application
- Controlled release of pressure from an enclosure.
Key specifications
- Model
- DXFBXG-D01
- Body material
- 304 stainless steel
- Ingress protection
- IP68
- Mounting thread
- M10×1
Product specifications
Construction and details

Product views and dimensions
Read the marked dimensions with the current model drawing; do not infer sizes by measuring the illustration.
Model specification tablesFurther specifications
- Opening pressure
- 150–200 kPa (±20 kPa)
- Continuous operating temperature
- -40°C to +120°C
- Temperature resistance
- -40°C to +150°C
- Installation torque
- 1–3 N·m
- Flammability class
- UL94 V-0
Key features
- Pressure releaseThe valve opens within a 150–200 kPa (±20 kPa) pressure range.
- Body materialThe valve has a 304 stainless steel body.
D02 Stainless Steel One-Way Pressure-Relief Valve
17 / Enclosure openings
D02 Stainless Steel One-Way Pressure-Relief Valve
An M12×1.5 stainless steel pressure-relief valve with an opening-pressure range of 5–350 kPa and a 34 mm overall height.
Product reference
- Product group
- Safety One-Way Pressure-Relief Valves
- Application
- Controlled release of pressure from an enclosure.
Key specifications
- Model
- DXFBXG-D02
- Body material
- 304 stainless steel
- Ingress protection
- IP68
- Mounting thread
- M12×1.5
Product specifications
Construction and details

Product views and dimensions
Read the marked dimensions with the current model drawing; do not infer sizes by measuring the illustration.
Model specification tablesFurther specifications
- Opening pressure
- 5–350 kPa (±5 kPa)
- Continuous operating temperature
- -40°C to +120°C
- Temperature resistance
- -40°C to +150°C
- Installation torque
- 1–3 N·m
- Flammability class
- UL94 V-0
Key features
- Pressure releaseThe valve opens within a 5–350 kPa (±5 kPa) pressure range.
- Body materialThe valve has a 304 stainless steel body.
D10 Aluminum One-Way Pressure-Relief Valve
18 / Enclosure openings
D10 Aluminum One-Way Pressure-Relief Valve
An M26×1.5 one-way pressure-relief valve with a perforated head, a 5–50 kPa opening-pressure range and a 32 mm overall height.
Product reference
- Product group
- Safety One-Way Pressure-Relief Valves
- Application
- Controlled release of pressure from an enclosure.
Key specifications
- Model
- DXFLC-D10
- Body material
- Aluminum alloy
- Ingress protection
- IP68
- Mounting thread
- M26×1.5
Product specifications
Construction and details

Product views and dimensions
Read the marked dimensions with the current model drawing; do not infer sizes by measuring the illustration.
Model specification tablesFurther specifications
- Opening pressure
- 5–50 kPa (±5 kPa)
- Continuous operating temperature
- -40°C to +120°C
- Temperature resistance
- -40°C to +150°C
- Installation torque
- 1–3 N·m
- Flammability class
- UL94 V-0
Key features
- Pressure releaseThe valve opens within a 5–50 kPa (±5 kPa) pressure range.
- Body materialThe valve has a Aluminum alloy body.
D10Y Aluminum One-Way Pressure-Relief Valve
19 / Enclosure openings
D10Y Aluminum One-Way Pressure-Relief Valve
An M26×1.5 one-way pressure-relief valve with a 30 mm body and 15 mm thread length. Its opening-pressure range is 5–50 kPa.
Product reference
- Product group
- Safety One-Way Pressure-Relief Valves
- Application
- Controlled release of pressure from an enclosure.
Key specifications
- Model
- DXFLC-D10Y
- Body material
- Aluminum alloy
- Ingress protection
- IP68
- Mounting thread
- M26×1.5
Product specifications
Construction and details

Product views and dimensions
Read the marked dimensions with the current model drawing; do not infer sizes by measuring the illustration.
Model specification tablesFurther specifications
- Opening pressure
- 5–50 kPa (±5 kPa)
- Continuous operating temperature
- -40°C to +120°C
- Temperature resistance
- -40°C to +150°C
- Installation torque
- 1–3 N·m
- Flammability class
- UL94 V-0
Key features
- Pressure releaseThe valve opens within a 5–50 kPa (±5 kPa) pressure range.
- Body materialThe valve has a Aluminum alloy body.
D10Y1 Aluminum One-Way Pressure-Relief Valve
20 / Enclosure openings
D10Y1 Aluminum One-Way Pressure-Relief Valve
A long-thread M26×1.5 one-way pressure-relief valve with a 25 mm thread and a 38.5 mm overall height. Its opening-pressure range is 5–50 kPa.
Product reference
- Product group
- Safety One-Way Pressure-Relief Valves
- Application
- Controlled release of pressure from an enclosure.
Key specifications
- Model
- DXFLC-D10Y1
- Body material
- Aluminum alloy
- Ingress protection
- IP68
- Mounting thread
- M26×1.5
Product specifications
Construction and details

Product views and dimensions
Read the marked dimensions with the current model drawing; do not infer sizes by measuring the illustration.
Model specification tablesFurther specifications
- Opening pressure
- 5–50 kPa (±5 kPa)
- Continuous operating temperature
- -40°C to +120°C
- Temperature resistance
- -40°C to +150°C
- Installation torque
- 1–3 N·m
- Flammability class
- UL94 V-0
Key features
- Pressure releaseThe valve opens within a 5–50 kPa (±5 kPa) pressure range.
- Body materialThe valve has a Aluminum alloy body.
S07/S09 Aluminum Pressure-Relief Valve
21 / Enclosure openings
S07/S09 Aluminum Pressure-Relief Valve
S07 and S09 are IP68 aluminum pressure-relief valves with a 5–50 kPa opening-pressure range. Choose M22×1 or M26×1.5 to match the mounting thread.
Product reference
- Product group
- Safety One-Way Pressure-Relief Valves
- Application
- Controlled release of pressure from an enclosure.
Key specifications
- Models
- SYFLC-S07 / SYFLC-S09
- Body material
- 6061 aluminum
- Ingress protection
- IP68
- Opening pressure
- 5–50 kPa (±3 kPa)
Product specifications
Construction and details

Product views and dimensions
Read the marked dimensions with the current model drawing; do not infer sizes by measuring the illustration.
Model specification tablesFurther specifications
- Continuous operating temperature
- -40°C to +120°C
- Temperature resistance
- -40°C to +150°C
- Installation torque
- 1–3 N·m
- Flammability class
- UL94 V-0
Key features
- Mounting threadS07 uses M22×1; S09 uses M26×1.5.
- Opening pressureBoth models have a 5–50 kPa opening-pressure range with a ±3 kPa tolerance.
S10 Aluminum Pressure-Relief Valve
22 / Enclosure openings
S10 Aluminum Pressure-Relief Valve
An aluminum pressure-relief valve with a 5–50 kPa opening-pressure range. Its body height is 31 mm, excluding the projecting stem.
Product reference
- Product group
- Safety One-Way Pressure-Relief Valves
- Application
- Controlled release of pressure from an enclosure.
Key specifications
- Model
- SYFLC-S10
- Body material
- 6061 aluminum
- Ingress protection
- IP68
- Opening pressure
- 5–50 kPa (±3 kPa)
Product specifications
Construction and details

Product views and dimensions
Read the marked dimensions with the current model drawing; do not infer sizes by measuring the illustration.
Model specification tablesFurther specifications
- Continuous operating temperature
- -40°C to +120°C
- Temperature resistance
- -40°C to +150°C
- Installation torque
- 1–3 N·m
- Flammability class
- UL94 V-0
- Nominal thread diameter
- M27
Key features
- Pressure releaseThe valve opens within a 5–50 kPa (±3 kPa) pressure range.
- Body materialThe valve has a 6061 aluminum body.
S10Y Aluminum Pressure-Relief Valve
23 / Enclosure openings
S10Y Aluminum Pressure-Relief Valve
An M27×1.5 aluminum pressure-relief valve with a 5–50 kPa opening-pressure range, a 20 mm thread and a 34.8 mm overall height.
Product reference
- Product group
- Safety One-Way Pressure-Relief Valves
- Application
- Controlled release of pressure from an enclosure.
Key specifications
- Model
- SYFLC-S10Y
- Body material
- Aluminum alloy
- Ingress protection
- IP68
- Mounting thread
- M27×1.5
Product specifications
Construction and details

Product views and dimensions
Read the marked dimensions with the current model drawing; do not infer sizes by measuring the illustration.
Model specification tablesFurther specifications
- Opening pressure
- 5–50 kPa (±3 kPa)
- Continuous operating temperature
- -40°C to +120°C
- Temperature resistance
- -40°C to +150°C
- Installation torque
- 1–3 N·m
- Flammability class
- UL94 V-0
Key features
- Pressure releaseThe valve opens within a 5–50 kPa (±3 kPa) pressure range.
- Body materialThe valve has a Aluminum alloy body.
G10/G16 Aluminum Filter Valve
24 / Enclosure openings
G10/G16 Aluminum Filter Valve
G10 and G16 aluminum filter valves separate approximately 65–85% of particles larger than 10 μm. The two sizes use M20×1.5 and M30×1.5 mounting threads.
Product reference
- Product group
- Safety One-Way Pressure-Relief Valves
- Application
- Particle filtration in an enclosure air path.
Key specifications
- Models
- GLFHT-G10 / GLFHT-G16
- Body material
- 6061 aluminum
- Ingress protection
- IP68
- Continuous operating temperature
- -40°C to +120°C
Product specifications
Construction and details

Product views and dimensions
Read the marked dimensions with the current model drawing; do not infer sizes by measuring the illustration.
Model specification tables
Product views and dimensions
Read the marked dimensions with the current model drawing; do not infer sizes by measuring the illustration.
Model specification tablesFurther specifications
- Temperature resistance
- -40°C to +150°C
- Installation torque
- 1–3 N·m
- Flammability class
- UL94 V-0
- Particle separation efficiency
- Approximately 65–85% for particles larger than 10 μm
Key features
- Particle filtrationThe filter separates approximately 65–85% of particles larger than 10 μm.
- Mounting threadG10 uses M20×1.5; G16 uses M30×1.5.
M02/G01 Push-Button Quick-Exhaust Valve
25 / Enclosure openings
M02/G01 Push-Button Quick-Exhaust Valve
Press the button to release pressure through an aluminum quick-exhaust valve. M02 uses an M6×1 thread; G01 uses G1/8. Both come in black, blue, red or yellow.
Product reference
- Product group
- Safety One-Way Pressure-Relief Valves
- Application
- Controlled release of pressure from an enclosure.
Key specifications
- Models
- AYKPFLC-M02 / AYKPFLC-G01
- Body material
- 6061 aluminum
- Ingress protection
- IP68
- Colors
- Black, blue, red, yellow
Product specifications
Construction and details

Product views and dimensions
Read the marked dimensions with the current model drawing; do not infer sizes by measuring the illustration.
Model specification tables
Product views and dimensions
Read the marked dimensions with the current model drawing; do not infer sizes by measuring the illustration.
Model specification tablesFurther specifications
- Operation
- Push-button pressure release
Key features
- Push-button operationPress the button to open the exhaust path.
- Mounting threadM02 uses M6×1; G01 uses G1/8.
TQM Plastic Vent Caps
26 / Enclosure openings
TQM Plastic Vent Caps
Black vent caps with an ePTFE membrane, polypropylene shell and TPE fitting.
Product reference
- Product group
- Plastic Vent Caps
- Application
- Ventilation through an unthreaded mounting hole.
Key specifications
- Shell material
- Polypropylene (PP)
- Rubber component
- TPE
- Membrane
- ePTFE
- Protection rating
- IP67
Product specifications
Construction and details

Product views and dimensions
Read the marked dimensions with the current model drawing; do not infer sizes by measuring the illustration.
Drawing markers: H · A · B · Φ
Model specification tablesFurther specifications
- Colour
- Black
Key features
- Cap constructionA PP outer shell covers the ePTFE membrane and TPE fitting.
- Mounting-hole sizesChoose the cap using its hole diameter and overall dimensions.
HDPE Waterproof Breathable Plugs
27 / Enclosure openings
HDPE Waterproof Breathable Plugs
D15, D17, W17 and D38 are HDPE plugs with ePTFE membranes for 12.7–12.8 mm mounting holes. Choose the body shape and airflow for the enclosure: ≥1,500, ≥3,000 or ≥4,500 ml/min at 70 mbar.
Product reference
- Product group
- Plastic Waterproof Breathable Plugs
- Application
- Enclosure breathing through a 12.7–12.8 mm mounting hole.
Key specifications
- Models
- D15 / D17 / W17 / D38
- Body material
- HDPE
- Membrane
- ePTFE
- Protection rating
- IP67
Product specifications
Construction and details

Product views and dimensions
Read the marked dimensions with the current model drawing; do not infer sizes by measuring the illustration.
Model specification tables
Product views and dimensions
Read the marked dimensions with the current model drawing; do not infer sizes by measuring the illustration.
Model specification tablesFurther specifications
- Mounting hole
- 12.7–12.8 mm
- Oil repellency grade
- 8
Key features
- Body materialHDPE bodies contain ePTFE breathable membranes.
- AirflowAt 70 mbar, D15 and D17 provide ≥1,500 ml/min, W17 provides ≥3,000 ml/min and D38 provides ≥4,500 ml/min.
SDQLC Metal Humidity Indicators
28 / Enclosure openings
SDQLC Metal Humidity Indicators
Threaded aluminum indicators provide a window for checking humidity inside equipment.
Product reference
- Product group
- Metal Humidity Indicators
- Application
- Visual humidity checks through an enclosure wall.
Key specifications
- Body material
- 6061 aluminum
- Models
- SDQLC-001 / SDQLC-005
- Colour
- Black
- Protection rating
- IP68
Product specifications
Construction and details

Product views and dimensions
Read the marked dimensions with the current model drawing; do not infer sizes by measuring the illustration.
Drawing markers: SDQLC-005 · M24×1.5
Model specification tablesFurther specifications
- Temperature resistance
- −40°C to +150°C
- Installation torque
- 1–3 N·m
- Flammability class
- UL94 V-0
Key features
- Threaded mountingThe two models use M18×1.5 and M24×1.5 threads.
- Viewing windowInspect the indicator through the window without opening the enclosure.
ePTFE Waterproof Breathable Membrane
29 / Enclosure openings
ePTFE Waterproof Breathable Membrane
Hydrophobic ePTFE membrane lets air pass through a microporous structure while resisting liquid water. Available in rolls and die-cut pieces.
Product reference
- Product group
- Waterproof Breathable Membranes
- Application
- Breathing elements for equipment housings and vent assemblies.
Key specifications
- Material
- Expanded polytetrafluoroethylene (ePTFE)
- Structure
- Microporous network
- Forms
- Rolls and die-cut pieces
- Surface property
- Hydrophobic; oil-repellent treatment available
Product specifications
Construction and details
Key features
- Microporous structureInterconnected pores provide the air path through the membrane.
- Rolls and die-cut piecesChoose the format to suit the vent opening and assembly method.
Need mounting dimensions? Ask us for the drawing for this model.
Model specification tables
Model sizes and specifications
PA66 Compact Threaded Waterproof Breathable Vent
Plastic Waterproof Vents
PA66 Compact Threaded Waterproof Breathable Vent
Model specificationsCompact threaded vent dimensions
| Thread / reference | Airflow at 70 mbar (mL/min) | Overall length H (mm) | Thread outside diameter (mm) | Thread length GL (mm) | Width across flats AG (mm) |
|---|---|---|---|---|---|
| M5×0.8-7 | ≥600 | 13 | 5 | 7 | 12 |
| M6×1-7 | ≥600 | 13 | 6 | 7 | 12 |
| M8×1.25-10 | ≥1200 | 18 | 8 | 10 | 17 |
| M8×1-7 | ≥600 | 12.5 | 8 | 7 | 12 |
| M10×1.5-10 | ≥1500 | 18 | 10 | 10 | 17 |
| M12×1.5-10 | ≥1500 | 18 | 12 | 10 | 17 |
| M12×1.5-10 | ≥1200 | 16 | 12 | 10 | 16 |
| M12×1-10 | ≥1200 | 16 | 12 | 10 | 16 |
PA66 Large Threaded Waterproof Breathable Vent
Plastic Waterproof Vents
PA66 Large Threaded Waterproof Breathable Vent
Model specificationsLarge threaded vent dimensions
| Thread / reference | Airflow at 70 mbar (mL/min) | Overall length H (mm) | Thread outside diameter (mm) | Thread length GL (mm) | Width across flats AG (mm) |
|---|---|---|---|---|---|
| M16×1.5-10 | ≥4500 | 18 | 16 | 10 | 22 |
| M18×1.5-10 | ≥4500 | 18 | 18 | 10 | 24 |
| M20×1.5-10 | ≥4500 | 18 | 20 | 10 | 27 |
| M24×1.5-15 | ≥7000 | 25 | 24 | 15 | 36 |
| M32×1.5-15 | ≥8000 | 25 | 32 | 15 | 45 |
| M40×1.5-15 | ≥8500 | 25 | 40 | 15 | 56 |
| M42×1.5-15 | ≥8500 | 25 | 42 | 15 | 56 |
K01–K03 PA66 Snap-in Waterproof Breathable Vent
Plastic Waterproof Vents
K01–K03 PA66 Snap-in Waterproof Breathable Vent
Model specificationsK01–K03 snap dimensions
| Model | Lid diameter A (mm) | Snap height K (mm) | Snap outer diameter AG (mm) | Snap inner diameter GL (mm) | Overall height H (mm) | Airflow at 70 mbar (mL/min) |
|---|---|---|---|---|---|---|
| K01 | 14 | 4 | 8.8 | 7.2 | 9 | ≥800 |
| K02 | 17.5 | 4.5 | 7.8 | 6.4 | 12.4 | ≥1500 |
| K03 | 17.5 | 3.6 | 12 | 10.4 | 11.1 | ≥1500 |
Stainless Steel Threaded Waterproof Breathable Vent
Stainless Steel Waterproof Vents
Stainless Steel Threaded Waterproof Breathable Vent
Model specificationsMetric threaded stainless steel vent dimensions
| Thread / reference | Airflow at 70 mbar (mL/min) | Overall length H (mm) | Thread outside diameter (mm) | Thread length GL (mm) | Width across flats AG (mm) |
|---|---|---|---|---|---|
| M4×0.7 | ≥200 | 12 | 4 | 5 | 8 |
| M5×0.8 | ≥300 | 15 | 5 | 7 | 10 |
| M6×1 | ≥300 | 15 | 6 | 7 | 10 |
| M8×1 | ≥800 | 16.2 | 8 | 7 | 14 |
| M8×1.25 | ≥800 | 16.2 | 8 | 7 | 14 |
| M10×1 | ≥1500 | 16 | 10 | 8 | 17 |
| M10×1.5 | ≥1500 | 16 | 10 | 8 | 17 |
| M12×1.5 | ≥1500 | 14.7 | 12 | 7 | 17 |
| M12×1.5 | ≥1500 | 18 | 12 | 10 | 17 |
| M12×1.75 | ≥1500 | 14.7 | 12 | 7 | 17 |
| M12×1.75 | ≥1500 | 18 | 12 | 10 | 17 |
| M14×1.5 | ≥1800 | 15.7 | 14 | 10 | 19 |
| M16×1.5 | ≥2300 | 19.5 | 16 | 10 | 22 |
| M18×1.5 | ≥2300 | 19.5 | 18 | 10 | 22 |
| M20×1.5 | ≥2300 | 19.5 | 20 | 10 | 22 |
| M22×1.5 | ≥2500 | 22.3 | 22 | 10 | 27 |
| M24×1.5 | ≥2500 | 21 | 24 | 8 | 30 |
| M25×1.5 | ≥2500 | 21 | 25 | 8 | 30 |
| M27×1.5 | ≥2500 | 23.5 | 27 | 10 | 32 |
| M32×1.5 | ≥5500 | 28 | 32 | 15 | 36 |
| M40×1.5 | ≥8500 | 30 | 40 | 15 | 45 |
Model specificationsG threaded stainless steel vent dimensions
| Thread / reference | Airflow at 70 mbar (mL/min) | Overall length H (mm) | Thread outside diameter (mm) | Thread length GL (mm) | Width across flats AG (mm) |
|---|---|---|---|---|---|
| G1/8 | ≥1500 | 16 | 9.8 | 8 | 17 |
| G1/4 | ≥1500 | 14.7 | 13.2 | 7 | 17 |
| G3/8 | ≥2300 | 19.5 | 16.8 | 10 | 22 |
| G1/2 | ≥2300 | 19.5 | 21 | 10 | 24 |
| G3/4 | ≥2300 | 23 | 26.5 | 10 | 32 |
Model specificationsNPT threaded stainless steel vent dimensions
| Thread / reference | Airflow at 70 mbar (mL/min) | Overall length H (mm) | Thread outside diameter (mm) | Thread length GL (mm) | Width across flats AG (mm) |
|---|---|---|---|---|---|
| NPT1/8 | ≥1500 | 16 | 10.2 | 8 | 17 |
| NPT1/4 | ≥1500 | 14.7 | 13.7 | 7 | 17 |
| NPT3/8 | ≥2300 | 19.5 | 17.1 | 10 | 22 |
| NPT1/2 | ≥2300 | 19.5 | 21.3 | 10 | 24 |
| NPT3/4 | ≥2300 | 23 | 26.8 | 10 | 32 |
Low-profile Hex Stainless Steel Waterproof Breathable Vent
Stainless Steel Waterproof Vents
Low-profile Hex Stainless Steel Waterproof Breathable Vent
Model specificationsLow-profile hex stainless steel vent dimensions
| Thread / reference | Airflow at 70 mbar (mL/min) | Overall length H (mm) | Thread outside diameter (mm) | Thread length GL (mm) | Width across flats AG (mm) |
|---|---|---|---|---|---|
| M5×0.8 | ≥200 | 9.2 | 5 | 5 | 8 |
| M6×1 | ≥200 | 9.2 | 6 | 5 | 10 |
| M8×1.25 | ≥550 | 12 | 8 | 7 | 12 |
| M10×1.5 | ≥600 | 13 | 10 | 8 | 14 |
| M12×1.5 | ≥1200 | 13 | 12 | 8 | 16 |
| M12×1.5 | ≥1200 | 15 | 12 | 10 | 16 |
| M14×1.5 | ≥1200 | 15 | 14 | 10 | 19 |
| M16×1.5 | ≥2300 | 15 | 16 | 10 | 20 |
| M18×1.5 | ≥2300 | 15 | 18 | 10 | 22 |
| M20×1.5 | ≥2300 | 15 | 20 | 10 | 24 |
Round Slotted Stainless Steel Waterproof Breathable Vent
Stainless Steel Waterproof Vents
Round Slotted Stainless Steel Waterproof Breathable Vent
Model specificationsRound slotted stainless steel vent dimensions
| Thread / reference | Airflow at 70 mbar (mL/min) | Overall length H (mm) | Thread outside diameter (mm) | Thread length GL (mm) | Head outside diameter AG (mm) |
|---|---|---|---|---|---|
| M3×0.5 | ≥200 | 8 | 3 | 4.5 | 6 |
| M3×0.5 | ≥200 | 8.8 | 3 | 4 | 7 |
| M4×0.7 | ≥200 | 9.8 | 4 | 5 | 8 |
| M5×0.8 | ≥200 | 12.5 | 5 | 7 | 9.8 |
| M6×1 | ≥300 | 12.5 | 6 | 7 | 9.8 |
| M8×1.25 | ≥300 | 13 | 8 | 7 | 11.8 |
| M10×1.5 | ≥600 | 13 | 10 | 7 | 13.8 |
| M12×1.5 | ≥800 | 13 | 12 | 7 | 15.8 |
Slotted Stainless Steel Waterproof Breathable Vent with Hex Base
Stainless Steel Waterproof Vents
Slotted Stainless Steel Waterproof Breathable Vent with Hex Base
Model specificationsSlotted hex-base stainless steel vent dimensions
| Thread / reference | Airflow at 70 mbar (mL/min) | Overall length H (mm) | Thread outside diameter (mm) | Thread length GL (mm) | Head size AG (mm) |
|---|---|---|---|---|---|
| M5×0.8 | ≥300 | 16 | 5 | 7 | 10 |
| M6×1 | ≥300 | 16 | 6 | 7 | 10 |
Nickel-plated Brass Threaded Waterproof Breathable Vent
Nickel-Plated Brass Waterproof Vents
Nickel-plated Brass Threaded Waterproof Breathable Vent
Model specificationsMetric threaded nickel-plated brass vent dimensions
| Thread / reference | Airflow at 70 mbar (mL/min) | Overall length H (mm) | Thread outside diameter (mm) | Thread length GL (mm) | Width across flats AG (mm) |
|---|---|---|---|---|---|
| M5×0.8-5 | ≥200 | 13 | 5 | 5 | 8 |
| M5×0.8-7 | ≥300 | 15 | 5 | 7 | 10 |
| M6×1-7 | ≥300 | 15 | 6 | 7 | 10 |
| M8×1.25-7 | ≥800 | 15.5 | 8 | 7 | 12 |
| M8×1-7 | ≥800 | 15.5 | 8 | 7 | 12 |
| M10×1.5-8 | ≥1200 | 17 | 10 | 8 | 14 |
| M10×0.75-8 | ≥1200 | 17 | 10 | 8 | 14 |
| M12×1-8.5 | ≥1500 | 17.5 | 12 | 8.5 | 16 |
| M12×1.5-8.5 | ≥1500 | 17.5 | 12 | 8.5 | 16 |
| M14×1.5-10 | ≥1500 | 19 | 14 | 10 | 19 |
| M16×1.5-10 | ≥1700 | 19 | 16 | 10 | 20 |
| M18×1.5-10 | ≥1700 | 19 | 18 | 10 | 22 |
| M20×1.5-10 | ≥1700 | 19 | 20 | 10 | 22 |
| M22×1.5-10 | ≥2500 | 22 | 22 | 10 | 27 |
| M24×1.5-8 | ≥2500 | 22 | 24 | 8 | 30 |
| M25×1.5-10 | ≥2500 | 22 | 25 | 10 | 30 |
| M27×1.5-10 | ≥2500 | 22 | 27 | 10 | 32 |
| M32×1.5-15 | ≥5500 | 27 | 32 | 15 | 37 |
| M40×1.5-15 | ≥8500 | 29 | 40 | 15 | 45 |
| M50×1.5-15 | ≥15000 | 30 | 50 | 15 | 55 |
| M63×1.5-15 | ≥18000 | 30 | 63 | 15 | 68 |
Model specificationsG threaded nickel-plated brass vent dimensions
| Thread / reference | Airflow at 70 mbar (mL/min) | Overall length H (mm) | Thread outside diameter (mm) | Thread length GL (mm) | Width across flats AG (mm) |
|---|---|---|---|---|---|
| G1/8 | ≥1200 | 17 | 9.8 | 8 | 14 |
| G1/4 | ≥1500 | 17.5 | 13.2 | 8.5 | 16 |
| G3/8 | ≥1700 | 19 | 16.8 | 10 | 22 |
| G5/8 | ≥1700 | 19 | — | 10 | 22 |
| G1/2 | ≥1700 | 19 | 21 | 10 | 24 |
| G3/4 | ≥2500 | 22 | 26.5 | 10 | 30 |
Model specificationsNPT threaded nickel-plated brass vent dimensions
| Thread / reference | Airflow at 70 mbar (mL/min) | Overall length H (mm) | Thread outside diameter (mm) | Thread length GL (mm) | Width across flats AG (mm) |
|---|---|---|---|---|---|
| NPT1/8 | ≥1200 | 17 | 10.2 | 8 | 14 |
| NPT1/4 | ≥1500 | 17.5 | 13.7 | 8.5 | 16 |
| NPT3/8 | ≥1700 | 19 | 17.1 | 10 | 22 |
| NPT1/2 | ≥1700 | 19 | 21.3 | 10 | 24 |
| NPT3/4 | ≥2500 | 22 | 26.8 | 10 | 30 |
Low-profile Hex Nickel-plated Brass Waterproof Breathable Vent
Nickel-Plated Brass Waterproof Vents
Low-profile Hex Nickel-plated Brass Waterproof Breathable Vent
Model specificationsLow-profile hex nickel-plated brass vent dimensions
| Thread / reference | Airflow at 70 mbar (mL/min) | Overall length H (mm) | Thread outside diameter (mm) | Thread length GL (mm) | Width across flats AG (mm) |
|---|---|---|---|---|---|
| M5×0.8 | ≥200 | 9.2 | 5 | 5 | 8 |
| M6×1 | ≥200 | 9.2 | 6 | 5 | 10 |
| M8×1.25 | ≥550 | 12 | 8 | 7 | 12 |
| M8×1 | ≥800 | 12 | 8 | 7 | 12 |
| M10×1.5 | ≥600 | 13 | 10 | 8 | 14 |
| M12×1.5 | ≥1200 | 13 | 12 | 8 | 16 |
| M12×1.5 | ≥1200 | 15 | 12 | 10 | 16 |
| M14×1.5 | ≥2000 | 15 | 14 | 10 | 19 |
| M16×1.5 | ≥2300 | 15 | 16 | 10 | 20 |
| M20×1.5 | ≥2300 | 15 | 20 | 10 | 24 |
Aluminum Threaded Waterproof Breathable Vent
Aluminum Alloy Waterproof Vents
Aluminum Threaded Waterproof Breathable Vent
Model specificationsMetric threaded aluminum vent dimensions
| Thread / reference | Finish | Airflow at 70 mbar (mL/min) | Length H (mm) | Thread outside diameter (mm) | Thread length GL (mm) | Width across flats AG (mm) |
|---|---|---|---|---|---|---|
| M5×0.8 | Oxidized | ≥200 | 10 | 5 | 4 | 8 |
| M6×1 | Oxidized | ≥200 | 12 | 6 | 6 | 8 |
| M8×1.25 | Oxidized | ≥300 | 15.5 | 8 | 7 | 12 |
| M10×1.5 | Oxidized | ≥600 | 17 | 10 | 8 | 14 |
| M10×1 | Oxidized | ≥600 | 17 | 10 | 8 | 14 |
| M12×1.5 | Oxidized or black oxidized | ≥800 | 19 | 12 | 10 | 16 |
| M12×1.5 | Bright | ≥800 | 19 | 12 | 10 | 16 |
| M14×1.5 | Oxidized | ≥1200 | 21 | 14 | 10 | 19 |
| M16×1.5L | Oxidized or black oxidized | ≥1500 | 19 | 16 | 10 | 20 |
| M16×1.5 | Oxidized | ≥1500 | 21 | 16 | 10 | 20 |
| M18×1.5-10 | Oxidized | ≥1700 | 19 | 18 | 10 | 22 |
| M20×1.5 | Oxidized | ≥1500 | 19 | 20 | 10 | 22 |
| M25×1.5 | Oxidized | ≥2300 | 21 | 25 | 8 | 30 |
| M32×1.5 | Oxidized | ≥4500 | 27 | 32 | 15 | 36 |
| M40×1.5 | Oxidized | ≥8500 | 29 | 40 | 15 | 45 |
Model specificationsG threaded aluminum vent dimensions
| Thread / reference | Finish | Airflow at 70 mbar (mL/min) | Length H (mm) | Thread outside diameter (mm) | Thread length GL (mm) | Width across flats AG (mm) |
|---|---|---|---|---|---|---|
| G1/8 | Oxidized | ≥600 | 17 | 9.8 | 8 | 14 |
| G1/4 | Oxidized | ≥800 | 19 | 13.2 | 10 | 16 |
| G3/8 | Oxidized | ≥1500 | 19 | 16.8 | 10 | 21 |
| G1/2 | Oxidized | ≥1500 | 19 | 21 | 10 | 22 |
| G3/4 | Oxidized | ≥2500 | 22 | 26.5 | 10 | 30 |
Model specificationsNPT threaded aluminum vent dimensions
| Thread / reference | Finish | Airflow at 70 mbar (mL/min) | Length H (mm) | Thread outside diameter (mm) | Thread length GL (mm) | Width across flats AG (mm) |
|---|---|---|---|---|---|---|
| NPT1/8 | Oxidized | ≥600 | 17 | — | 8 | 14 |
| NPT1/4 | Oxidized | ≥800 | 19 | — | 10 | 16 |
| NPT3/8 | Oxidized | ≥1500 | 19 | — | 10 | 21 |
| NPT1/2 | Oxidized | ≥1500 | 19 | — | 10 | 22 |
| NPT3/4 | Oxidized | ≥2500 | 22 | — | 10 | 30 |
Black Aluminum Slotted Waterproof Breathable Vent
Aluminum Alloy Waterproof Vents
Black Aluminum Slotted Waterproof Breathable Vent
Model specificationsSlotted aluminum vent dimensions
| Thread / reference | Airflow at 70 mbar (mL/min) | Overall length H (mm) | Thread outside diameter (mm) | Thread length GL (mm) | Head outside diameter AG (mm) |
|---|---|---|---|---|---|
| M5×0.8 | ≥200 | 12.5 | 5 | 6.5 | 10 |
| M6×1 | ≥200 | 14.5 | 6 | 6.5 | 10 |
B Series Waterproof Breathable Explosion-Proof Valve
Waterproof Breathable Explosion-Proof Valves
B Series Waterproof Breathable Explosion-Proof Valve
Model specificationsB series model dimensions and performance
| Parameter | FBFBXG-B10 | FBFLC-B10 | FBFLC-B15 | FBFLC-B25 | FBFLC-B55 |
|---|---|---|---|---|---|
| Body material | 304 stainless steel | 6061 aluminum | 6061 aluminum | 6061 aluminum | 6061 aluminum |
| Mounting thread | M12×1.5 | M12×1.5 | M20×1.5 | M32×1.5 | M40×1.5 |
| Airflow at 70 mbar | ≥1,200 ml/min | ≥800 ml/min | ≥1,500 ml/min | ≥2,000 ml/min | ≥3,000 ml/min |
| Width across flats (mm) | 22.00 | 16.00 ±0.3 | 28.00 ±0.3 | 45.00 ±0.3 | 50.00 ±0.3 |
| Overall height (mm) | 23.50 | 18.30 ±0.5 | 23.50 ±0.5 | 23.50 ±0.5 | 23.50 ±0.5 |
| Thread length (mm) | 10.00 | 10.00 ±0.3 | 12.00 ±0.3 | 12.00 ±0.3 | 12.00 ±0.3 |
H Series Waterproof Breathable Explosion-Proof Valve
Waterproof Breathable Explosion-Proof Valves
H Series Waterproof Breathable Explosion-Proof Valve
Model specificationsH series model dimensions and performance
| Parameter | FBFLC-H15 | FBFLC-H25 | FBFLC-H55 |
|---|---|---|---|
| Airflow at 70 mbar | ≥1,200 ml/min | ≥1,200 ml/min | ≥3,000 ml/min |
| Mounting thread | — | M32×1.5 | M40×1.5 |
| Width across flats (mm) | 30.00 ±0.3 | 45.00 ±0.3 | 52.00 ±0.3 |
| Overall height (mm) | 23.60 ±0.5 | 23.50 ±0.5 | 23.50 ±0.5 |
| Thread length (mm) | 12.00 ±0.3 | 12.00 ±0.3 | 12.00 ±0.3 |
F550 Battery-Pack Waterproof Breathable Explosion-Proof Vent
Waterproof Breathable Explosion-Proof Valves
F550 Battery-Pack Waterproof Breathable Explosion-Proof Vent
Model specificationsFBFSL-F550 dimensions
| Dimension | Value (mm) |
|---|---|
| Overall width | 79.19 ±0.25 |
| Overall length | 105.19 ±0.25 |
| Body length | 93.19 ±0.25 |
| Overall depth | 23.77 ±0.25 |
| Mounting spacing across width | 50 ±0.2 |
| Mounting spacing along length | 66 ±0.2 |
| Inner spacing | 16 ±0.2 |
D03 Aluminum One-Way Pressure-Relief Valve
Safety One-Way Pressure-Relief Valves
D03 Aluminum One-Way Pressure-Relief Valve
Model specificationsDXFLC-D03 dimensions
| Dimension | Value (mm) |
|---|---|
| Dimensioned body height (excluding projecting tips) | 16.00 ±0.1 |
| Head diameter | 17.70 ±0.1 |
| Lower body diameter | 12.80 ±0.1 |
| Head height | 7.00 ±0.1 |
D01 Stainless Steel One-Way Pressure-Relief Valve
Safety One-Way Pressure-Relief Valves
D01 Stainless Steel One-Way Pressure-Relief Valve
Model specificationsDXFBXG-D01 dimensions
| Dimension | Value (mm) |
|---|---|
| Overall height | 13.00 |
| Thread length | 7.00 |
| Width across flats | 12.00 +0/-0.1 |
| Head diameter | 12.30 |
| Head height | 6.00 |
| Upper head chamfer C1 | 1.00 |
| Lower head chamfer C0.65 | 0.65 |
D02 Stainless Steel One-Way Pressure-Relief Valve
Safety One-Way Pressure-Relief Valves
D02 Stainless Steel One-Way Pressure-Relief Valve
Model specificationsDXFBXG-D02 dimensions
| Dimension | Value (mm) |
|---|---|
| Overall height | 34.00 |
| Thread length | 10.00 |
| Width across flats | 19.00 |
| Head diameter | 21.00 |
| Lower body height | 14.50 |
| Thread end to hex underside | 16.00 |
D10 Aluminum One-Way Pressure-Relief Valve
Safety One-Way Pressure-Relief Valves
D10 Aluminum One-Way Pressure-Relief Valve
Model specificationsDXFLC-D10 dimensions
| Dimension | Value (mm) |
|---|---|
| Overall height | 32.00 |
| Thread length | 15.00 |
| Width across flats | 32.00 |
| Head diameter | 35.00 |
D10Y Aluminum One-Way Pressure-Relief Valve
Safety One-Way Pressure-Relief Valves
D10Y Aluminum One-Way Pressure-Relief Valve
Model specificationsDXFLC-D10Y dimensions
| Dimension | Value (mm) |
|---|---|
| Overall height | 30.00 |
| Thread length | 15.00 |
| Width across flats | 34.00 ±0.2 |
| Head diameter | 37.30 ±0.2 |
D10Y1 Aluminum One-Way Pressure-Relief Valve
Safety One-Way Pressure-Relief Valves
D10Y1 Aluminum One-Way Pressure-Relief Valve
Model specificationsDXFLC-D10Y1 dimensions
| Dimension | Value (mm) |
|---|---|
| Overall height | 38.50 |
| Thread length | 25.00 |
| Head diameter | 34.00 ±0.5 |
| Head height | 13.50 |
S07/S09 Aluminum Pressure-Relief Valve
Safety One-Way Pressure-Relief Valves
S07/S09 Aluminum Pressure-Relief Valve
Model specificationsS07/S09 model dimensions and performance
| Parameter | SYFLC-S07 | SYFLC-S09 |
|---|---|---|
| Mounting thread | M22×1 | M26×1.5 |
| Overall height (mm) | — | 24.00 ±0.5 |
| Body length (mm) | — | 23.00 ±0.5 |
| Thread length (mm) | — | 15.00 ±0.5 |
| Width across flats (mm) | — | 38.00 ±0.5 |
| Head diameter (mm) | — | 42.00 |
S10 Aluminum Pressure-Relief Valve
Safety One-Way Pressure-Relief Valves
S10 Aluminum Pressure-Relief Valve
Model specificationsSYFLC-S10 dimensions
| Dimension | Value (mm) |
|---|---|
| Body height (excluding projecting stem) | 31.00 |
| Thread length | 21.50 |
| Width across flats | 35.00 |
| Lower body diameter | 33.00 |
S10Y Aluminum Pressure-Relief Valve
Safety One-Way Pressure-Relief Valves
S10Y Aluminum Pressure-Relief Valve
Model specificationsSYFLC-S10Y dimensions
| Dimension | Value (mm) |
|---|---|
| Overall height | 34.80 |
| Thread length | 20.00 |
| Width across flats | 38.00 |
G10/G16 Aluminum Filter Valve
Safety One-Way Pressure-Relief Valves
G10/G16 Aluminum Filter Valve
Model specificationsG10/G16 model dimensions and performance
| Parameter | GLFHT-G10 | GLFHT-G16 |
|---|---|---|
| Mounting thread | M20×1.5 | M30×1.5 |
| Overall height (mm) | 32.00 | 32.00 |
| Thread length (mm) | 10.00 | 10.00 |
| Width across flats (mm) | 27.00 | 36.00 |
| Head diameter (mm) | 29.00 | 39.00 |
| Lower body diameter (mm) | 20.00 | 20.00 |
M02/G01 Push-Button Quick-Exhaust Valve
Safety One-Way Pressure-Relief Valves
M02/G01 Push-Button Quick-Exhaust Valve
Model specificationsM02/G01 model dimensions and performance
| Parameter | AYKPFLC-M02 | AYKPFLC-G01 |
|---|---|---|
| Mounting thread | M6×1 | G1/8 |
| Overall length H (mm) | 21.5 | 25 |
| Thread outside diameter (mm) | 6.0 | 9.7 |
| Thread length GL (mm) | 6.0 | 7.5 |
| Width across flats AG (mm) | 10.0 | 14 |
TQM Plastic Vent Caps
Plastic Vent Caps
TQM Plastic Vent Caps
Model specificationsTQM vent cap sizes and airflow
| Model | Airflow at 70 mbar (ml/min) | Overall height H (mm) | Shell diameter A (mm) | Shell height B (mm) | Mounting-hole diameter (mm) | Protection rating |
|---|---|---|---|---|---|---|
| TQM-T01 | ≥800 | 12.5 | 16.2 | 11 | 6.8 | IP67 |
| TQM-T02 | ≥850 | 12.5 | 16.2 | 11 | 7.2 | IP67 |
| TQM-T03A | ≥1,500 | 12.5 | 16.2 | 11 | 7.8 | IP67 |
| TQM-T03 | ≥1,500 | 14 | 17 | 12 | 7.8 | IP67 |
| TQM-T05 | ≥2,000 | 14 | 18.8 | 12 | 10 | IP67 |
| TQM-T06 | ≥2,500 | 16 | 23 | 14 | 12 | IP67 |
| TQM-T07 | ≥300 | 16 | 23.5 | 14 | 16 | IP67 |
HDPE Waterproof Breathable Plugs
Plastic Waterproof Breathable Plugs
HDPE Waterproof Breathable Plugs
Model specificationsHDPE model specifications
| Parameter | D15 | D17 | W17 | D38 |
|---|---|---|---|---|
| Body material | HDPE | HDPE | HDPE | HDPE |
| Membrane | ePTFE | ePTFE | ePTFE | ePTFE |
| Protection rating | IP67 | IP67 | IP67 | IP67 |
| Mounting hole | 12.7–12.8 mm | 12.7–12.8 mm | 12.7–12.8 mm | 12.7–12.8 mm |
| Airflow | ≥1,500 ml/min at 70 mbar | ≥1,500 ml/min at 70 mbar | ≥3,000 ml/min at 70 mbar | ≥4,500 ml/min at 70 mbar |
| Oil repellency grade | 8 | 8 | 8 | 8 |
| Overall height | 8 mm | 14.30 mm | — | — |
| Head diameter | 14.50 mm | 17.00 mm | — | — |
| Mounting diameter | 12.80 mm | 12.80 mm | — | — |
| Internal bore diameter | 9.40 mm | 8.7 mm | — | — |
SDQLC Metal Humidity Indicators
Metal Humidity Indicators
SDQLC Metal Humidity Indicators
Model specificationsSDQLC indicator specifications
| Model | Material | Thread | Temperature resistance | Protection rating | Installation torque |
|---|---|---|---|---|---|
| SDQLC-001 | 6061 aluminum | M18×1.5 | −40°C to +150°C | IP68 | 1–3 N·m |
| SDQLC-005 | 6061 aluminum | M24×1.5 | −40°C to +150°C | IP68 | 1–3 N·m |
Model specificationsSDQLC-005 dimensions
| Dimension | Value (mm) |
|---|---|
| Width across flats | 35.00 ±0.3 |
| Overall length | 16.20 ±0.3 |
| Under-head length | 12.50 ±0.3 |
Product comparison
Airflow and pressure-response options.
Compare venting area or airflow, opening pressure where applicable, flow direction and mounting dimensions.| Product | Construction | Use when | Check first | Review |
|---|---|---|---|---|
| PA66 Compact Threaded Waterproof Breathable Vent | Plastic Waterproof Vents | A small threaded enclosure opening needs a breathable vent. |
| View specifications |
| PA66 Large Threaded Waterproof Breathable Vent | Plastic Waterproof Vents | A larger metric opening needs higher airflow. |
| View specifications |
| K01–K03 PA66 Snap-in Waterproof Breathable Vent | Plastic Waterproof Vents | A nylon vent must snap into an unthreaded panel opening. |
| View specifications |
| Stainless Steel Threaded Waterproof Breathable Vent | Stainless Steel Waterproof Vents | Enclosure ventilation with a stainless steel body. |
| View specifications |
| Low-profile Hex Stainless Steel Waterproof Breathable Vent | Stainless Steel Waterproof Vents | A low-profile stainless vent is needed at the enclosure surface. |
| View specifications |
| Round Slotted Stainless Steel Waterproof Breathable Vent | Stainless Steel Waterproof Vents | A round stainless vent head with screwdriver access. |
| View specifications |
| Slotted Stainless Steel Waterproof Breathable Vent with Hex Base | Stainless Steel Waterproof Vents | A slotted stainless vent with a hexagonal mounting base. |
| View specifications |
| Nickel-plated Brass Threaded Waterproof Breathable Vent | Nickel-Plated Brass Waterproof Vents | A nickel-plated brass body for a threaded enclosure vent. |
| View specifications |
| Low-profile Hex Nickel-plated Brass Waterproof Breathable Vent | Nickel-Plated Brass Waterproof Vents | A low-profile nickel-plated brass enclosure vent. |
| View specifications |
| Aluminum Threaded Waterproof Breathable Vent | Aluminum Alloy Waterproof Vents | A lightweight metal vent for a threaded enclosure opening. |
| View specifications |
| Black Aluminum Slotted Waterproof Breathable Vent | Aluminum Alloy Waterproof Vents | A small black aluminum vent with screwdriver access. |
| View specifications |
| B Series Waterproof Breathable Explosion-Proof Valve | Waterproof Breathable Explosion-Proof Valves | Enclosure breathing and pressure release. |
| View specifications |
| H Series Waterproof Breathable Explosion-Proof Valve | Waterproof Breathable Explosion-Proof Valves | Enclosure breathing and pressure release. |
| View specifications |
| F550 Battery-Pack Waterproof Breathable Explosion-Proof Vent | Waterproof Breathable Explosion-Proof Valves | Enclosure breathing and pressure release. |
| View specifications |
| D03 Aluminum One-Way Pressure-Relief Valve | Safety One-Way Pressure-Relief Valves | Controlled release of pressure from an enclosure. |
| View specifications |
| D01 Stainless Steel One-Way Pressure-Relief Valve | Safety One-Way Pressure-Relief Valves | Controlled release of pressure from an enclosure. |
| View specifications |
| D02 Stainless Steel One-Way Pressure-Relief Valve | Safety One-Way Pressure-Relief Valves | Controlled release of pressure from an enclosure. |
| View specifications |
| D10 Aluminum One-Way Pressure-Relief Valve | Safety One-Way Pressure-Relief Valves | Controlled release of pressure from an enclosure. |
| View specifications |
| D10Y Aluminum One-Way Pressure-Relief Valve | Safety One-Way Pressure-Relief Valves | Controlled release of pressure from an enclosure. |
| View specifications |
| D10Y1 Aluminum One-Way Pressure-Relief Valve | Safety One-Way Pressure-Relief Valves | Controlled release of pressure from an enclosure. |
| View specifications |
| S07/S09 Aluminum Pressure-Relief Valve | Safety One-Way Pressure-Relief Valves | Controlled release of pressure from an enclosure. |
| View specifications |
| S10 Aluminum Pressure-Relief Valve | Safety One-Way Pressure-Relief Valves | Controlled release of pressure from an enclosure. |
| View specifications |
| S10Y Aluminum Pressure-Relief Valve | Safety One-Way Pressure-Relief Valves | Controlled release of pressure from an enclosure. |
| View specifications |
| G10/G16 Aluminum Filter Valve | Safety One-Way Pressure-Relief Valves | Particle filtration in an enclosure air path. |
| View specifications |
| M02/G01 Push-Button Quick-Exhaust Valve | Safety One-Way Pressure-Relief Valves | Controlled release of pressure from an enclosure. |
| View specifications |
| TQM Plastic Vent Caps | Plastic Vent Caps | Ventilation through an unthreaded mounting hole. |
| View specifications |
| HDPE Waterproof Breathable Plugs | Plastic Waterproof Breathable Plugs | Enclosure breathing through a 12.7–12.8 mm mounting hole. |
| View specifications |
| SDQLC Metal Humidity Indicators | Metal Humidity Indicators | Visual humidity checks through an enclosure wall. |
| View specifications |
| ePTFE Waterproof Breathable Membrane | Waterproof Breathable Membranes | Breathing elements for equipment housings and vent assemblies. |
| View specifications |
Need help matching an existing part? Send us its model name or a photo.
Selection checks
Choose the right model
Choose the material and mounting form, then compare airflow and opening pressure for your enclosure.
- Vent and valve functionVenting, pressure relief or both
- Flow requirementAirflow, pressure difference and flow direction
- MountingThread or opening size and enclosure-wall thickness
Product support
Need a model recommendation or a quote?
Send a model name, a photo or a short question. We can help with product selection, samples and pricing. Share any of the details below that you already have.
Request product support- Model or photoStart with a model name, a photo or a short description of what you need.
- Airflow or pressure requirementFor a vent, share the airflow and pressure difference if known. For a relief valve, share the required opening pressure.
- Mounting thread or hole sizeSend the mounting thread or opening diameter and panel thickness if available.
- Water, dust and temperature exposureDescribe the conditions around the enclosure, including water, dust and temperature changes.
Waterproof Vents & Valves FAQ
Product questions
Find answers about fit, wiring and product differences.
Waterproof Vents & Valves
01Is a breathable vent the same as a pressure-relief valve?
No. A breathable vent passes air through its venting element. A relief valve opens in response to pressure; choose its opening pressure and flow direction for the enclosure.
02Which pressure or airflow value should I compare?
For a vent, compare airflow at the stated pressure difference. For a relief valve, compare opening pressure and flow direction. These values describe different functions and are not interchangeable.
PA66 Compact Threaded Waterproof Breathable Vent
PA66 Compact Threaded Waterproof Breathable Vent
01Why are there two M12×1.5-10 vent rows?
The two options differ in body height, airflow and spanner size. Choose the full dimensional row, including the 16 or 18 mm height.
02What seals the compact PA66 vent to the enclosure?
A silicone O-ring seals the mounting face.
PA66 Large Threaded Waterproof Breathable Vent
PA66 Large Threaded Waterproof Breathable Vent
01Which entry sizes does the large PA66 vent cover?
The range covers M16 to M42 entries.
02How much air can the large PA66 vents pass?
The listed sizes provide at least 4,500 to 8,500 ml/min at 70 mbar, depending on the selected row.
K01–K03 PA66 Snap-in Waterproof Breathable Vent
K01–K03 PA66 Snap-in Waterproof Breathable Vent
01Do K01–K03 snap-in vents need a threaded hole?
No. They use a snap-in mounting form. Match the panel opening to the selected model's drawing.
02Are K01, K02 and K03 the same size?
No. Their overall height, mounting dimensions and airflow differ. Use the complete row for the chosen model.
Stainless Steel Threaded Waterproof Breathable Vent
Stainless Steel Threaded Waterproof Breathable Vent
01Which threads are available on the stainless vent?
Metric, G and NPT versions are listed in separate tables.
02Can I compare vent airflow with membrane airflow per square centimetre?
No. The model-table airflow is for the complete vent. The membrane-area value is expressed per square centimetre and uses a different basis.
Low-profile Hex Stainless Steel Waterproof Breathable Vent
Low-profile Hex Stainless Steel Waterproof Breathable Vent
01Why does the stainless flat-hex vent have two M12×1.5 options?
They have different overall and thread lengths. Check both dimensions against the enclosure wall.
02How is the flat-hex vent tightened?
Use the hexagonal head, matching the spanner size in the table.
Round Slotted Stainless Steel Waterproof Breathable Vent
Round Slotted Stainless Steel Waterproof Breathable Vent
01How is the round stainless vent tightened?
The round head has a single screwdriver slot.
02Does the size table give a hexagonal spanner size?
No. It gives the outside diameter of the round head.
Slotted Stainless Steel Waterproof Breathable Vent with Hex Base
Slotted Stainless Steel Waterproof Breathable Vent with Hex Base
01Which threads are available on the hex-base slotted vent?
M5×0.8 and M6×1 are listed.
02What are its height and airflow?
Both versions have a 16 mm overall length and airflow of at least 300 ml/min at 70 mbar.
Nickel-plated Brass Threaded Waterproof Breathable Vent
Nickel-plated Brass Threaded Waterproof Breathable Vent
01Which thread tables cover the brass vent?
Separate Metric, G and NPT tables give the airflow and dimensions for each entry.
02How is the brass vent mounted?
Its threaded body passes through the enclosure opening, with a silicone O-ring at the mounting face.
Low-profile Hex Nickel-plated Brass Waterproof Breathable Vent
Low-profile Hex Nickel-plated Brass Waterproof Breathable Vent
01Which M12×1.5 thread lengths are available?
The flat-hex brass vent is listed with 8 mm and 10 mm thread lengths.
02What is the mounting-face seal?
The mounting face uses a silicone O-ring.
Aluminum Threaded Waterproof Breathable Vent
Aluminum Threaded Waterproof Breathable Vent
01Are all M12 and M16 aluminum vents identical?
No. The tables include different M12 finishes and M16 lengths. Compare the complete row.
02Which thread systems are included?
Metric, G and NPT sizes are listed separately.
Black Aluminum Slotted Waterproof Breathable Vent
Black Aluminum Slotted Waterproof Breathable Vent
01Which thread sizes are available on the black slotted vent?
M5×0.8 and M6×1 are listed.
02What mounting dimensions do the two slotted versions share?
Both have a 10 mm head diameter and 6.5 mm thread length.
B Series Waterproof Breathable Explosion-Proof Valve
B Series Waterproof Breathable Explosion-Proof Valve
01How do the B10 material options differ?
FBFBXG-B10 uses 304 stainless steel and provides ≥1,200 ml/min at 70 mbar. FBFLC-B10 uses 6061 aluminum and provides ≥800 ml/min at 70 mbar.
02What opening pressure does the B series use?
The opening-pressure range is 4–15 kPa across B10, B15, B25 and B55.
H Series Waterproof Breathable Explosion-Proof Valve
H Series Waterproof Breathable Explosion-Proof Valve
01How does airflow vary across the H series?
H15 and H25 provide ≥1,200 ml/min, while H55 provides ≥3,000 ml/min. All three airflow values are measured at 70 mbar.
02What opening pressure does the H series use?
The opening-pressure range is 4–15 kPa across H15, H25 and H55.
F550 Battery-Pack Waterproof Breathable Explosion-Proof Vent
F550 Battery-Pack Waterproof Breathable Explosion-Proof Vent
01At what pressure does FBFSL-F550 open?
The opening-pressure range is 20–50 kPa.
02What material is used for FBFSL-F550?
The body is PP with 30% glass fiber.
D03 Aluminum One-Way Pressure-Relief Valve
D03 Aluminum One-Way Pressure-Relief Valve
01At what pressure does DXFLC-D03 open?
The opening-pressure range is 10–30 kPa (±3 kPa).
02Which mounting thread does DXFLC-D03 use?
The mounting thread is M14×1.
03What tightening torque is specified for DXFLC-D03?
The installation torque is 1–3 N·m.
04What is the continuous temperature range for DXFLC-D03?
The continuous operating range is -40°C to +120°C.
D01 Stainless Steel One-Way Pressure-Relief Valve
D01 Stainless Steel One-Way Pressure-Relief Valve
01At what pressure does DXFBXG-D01 open?
The opening-pressure range is 150–200 kPa (±20 kPa).
02Which mounting thread does DXFBXG-D01 use?
The mounting thread is M10×1.
03What tightening torque is specified for DXFBXG-D01?
The installation torque is 1–3 N·m.
04What is the continuous temperature range for DXFBXG-D01?
The continuous operating range is -40°C to +120°C.
D02 Stainless Steel One-Way Pressure-Relief Valve
D02 Stainless Steel One-Way Pressure-Relief Valve
01At what pressure does DXFBXG-D02 open?
The opening-pressure range is 5–350 kPa (±5 kPa).
02Which mounting thread does DXFBXG-D02 use?
The mounting thread is M12×1.5.
03What tightening torque is specified for DXFBXG-D02?
The installation torque is 1–3 N·m.
04What is the continuous temperature range for DXFBXG-D02?
The continuous operating range is -40°C to +120°C.
D10 Aluminum One-Way Pressure-Relief Valve
D10 Aluminum One-Way Pressure-Relief Valve
01At what pressure does DXFLC-D10 open?
The opening-pressure range is 5–50 kPa (±5 kPa).
02Which mounting thread does DXFLC-D10 use?
The mounting thread is M26×1.5.
03What tightening torque is specified for DXFLC-D10?
The installation torque is 1–3 N·m.
04What is the continuous temperature range for DXFLC-D10?
The continuous operating range is -40°C to +120°C.
D10Y Aluminum One-Way Pressure-Relief Valve
D10Y Aluminum One-Way Pressure-Relief Valve
01At what pressure does DXFLC-D10Y open?
The opening-pressure range is 5–50 kPa (±5 kPa).
02Which mounting thread does DXFLC-D10Y use?
The mounting thread is M26×1.5.
03What tightening torque is specified for DXFLC-D10Y?
The installation torque is 1–3 N·m.
04What is the continuous temperature range for DXFLC-D10Y?
The continuous operating range is -40°C to +120°C.
D10Y1 Aluminum One-Way Pressure-Relief Valve
D10Y1 Aluminum One-Way Pressure-Relief Valve
01At what pressure does DXFLC-D10Y1 open?
The opening-pressure range is 5–50 kPa (±5 kPa).
02Which mounting thread does DXFLC-D10Y1 use?
The mounting thread is M26×1.5.
03What tightening torque is specified for DXFLC-D10Y1?
The installation torque is 1–3 N·m.
04What is the continuous temperature range for DXFLC-D10Y1?
The continuous operating range is -40°C to +120°C.
S07/S09 Aluminum Pressure-Relief Valve
S07/S09 Aluminum Pressure-Relief Valve
01Which thread sizes do S07 and S09 use?
S07 uses M22×1; S09 uses M26×1.5.
02What is the opening pressure for S07 and S09?
Both models have a 5–50 kPa opening-pressure range with a ±3 kPa tolerance.
S10 Aluminum Pressure-Relief Valve
S10 Aluminum Pressure-Relief Valve
01At what pressure does SYFLC-S10 open?
The opening-pressure range is 5–50 kPa (±3 kPa).
02What tightening torque is specified for SYFLC-S10?
The installation torque is 1–3 N·m.
03What is the continuous temperature range for SYFLC-S10?
The continuous operating range is -40°C to +120°C.
S10Y Aluminum Pressure-Relief Valve
S10Y Aluminum Pressure-Relief Valve
01At what pressure does SYFLC-S10Y open?
The opening-pressure range is 5–50 kPa (±3 kPa).
02Which mounting thread does SYFLC-S10Y use?
The mounting thread is M27×1.5.
03What tightening torque is specified for SYFLC-S10Y?
The installation torque is 1–3 N·m.
04What is the continuous temperature range for SYFLC-S10Y?
The continuous operating range is -40°C to +120°C.
G10/G16 Aluminum Filter Valve
G10/G16 Aluminum Filter Valve
01How do G10 and G16 differ?
G10 uses an M20×1.5 thread and a 27 mm width across flats. G16 uses an M30×1.5 thread and a 36 mm width across flats.
02What filtration efficiency do G10 and G16 provide?
The filter separates approximately 65–85% of particles larger than 10 μm.
M02/G01 Push-Button Quick-Exhaust Valve
M02/G01 Push-Button Quick-Exhaust Valve
01How is the M02/G01 valve operated?
Press the button to release air through the exhaust valve.
02Which thread sizes do M02 and G01 use?
M02 uses M6×1; G01 uses G1/8.
TQM Plastic Vent Caps
TQM Plastic Vent Caps
01Are TQM caps threaded?
No. The dimensions specify a mounting-hole diameter rather than a thread.
02Are all caps the same airflow?
No. Compare the airflow value for the chosen TQM model at 70 mbar.
HDPE Waterproof Breathable Plugs
HDPE Waterproof Breathable Plugs
01What mounting hole do these HDPE plugs need?
D15, D17, W17 and D38 fit a 12.7–12.8 mm mounting hole.
02How does airflow vary between the HDPE plug models?
At 70 mbar, D15 and D17 provide ≥1,500 ml/min, W17 provides ≥3,000 ml/min and D38 provides ≥4,500 ml/min.
SDQLC Metal Humidity Indicators
SDQLC Metal Humidity Indicators
01Which threads are available?
SDQLC-001 uses M18×1.5; SDQLC-005 uses M24×1.5.
02What installation torque is specified?
The installation torque is 1–3 N·m.
ePTFE Waterproof Breathable Membrane
ePTFE Waterproof Breathable Membrane
01Is this a complete vent valve?
No. It is the breathing membrane used within a vent or enclosure assembly.
02What information helps specify a membrane?
Send the opening dimensions, required airflow, water exposure and assembly method.