Our Stainless Steel Protective Vent allows enclosures to breathe, preventing condensation while providing IP68 protection. Made from 304/316 steel, it’s ideal for the most harsh industrial environments.
Key Features

| Product Number (Code) |
Metric thread (M) |
Cover outer diameter (K) |
Material | Thread Length
(GL) |
Thread O.D.
(AG) |
Total Height (H) |
Waterproof Grade | Air Permeability | Spanner Size (A&F) |
| BXG-T001 | M5×0.8 | 9.5mm | 304/316 | 7mm | 5mm | 15mm | IP68 | ≥300ml/min/@70mbar | 10 |
| BXG-T002 | M6×1 | 9.5mm | 304/316 | 7mm | 6mm | 15mm | IP68 | ≥300ml/min/@70mbar | 10 |
| BXG-T003A1 | M8×1 | 11.8mm | 304/316 | 7mm | 8mm | 16.2mm | IP68 | ≥800ml/min/@70mbar | 14 |
| BXG-T003 | M8×1.25 | 11.8mm | 304/316 | 7mm | 8mm | 16.2mm | IP68 | ≥800ml/min/@70mbar | 14 |
| BXG-T005A1 | M10×1 | 13.8mm | 304/316 | 8mm | 10mm | 16.5mm | IP68 | ≥1500ml/min/@70mbar | 17 |
| BXG-T005 | M10×1.5 | 13.8mm | 304/316 | 8mm | 10mm | 16.5mm | IP68 | ≥1500ml/min/@70mbar | 17 |
| BXG-T007B | M12×1.5 | 13.8mm | 304/316 | 10mm | 12mm | 18.6mm | IP68 | ≥200ml/min/@70mbar | 17 |
| BXG-T007 | M12×1.5 | 13.8mm | 304/316 | 10mm | 12mm | 18mm | IP68 | ≥1500ml/min/@70mbar | 17 |
| BXG-T006 | M12×1.5 | 13.8mm | 304/316 | 7mm | 12mm | 15mm | IP68 | ≥1500ml/min/@70mbar | 17 |
| BXG-T010 | M16×1.5 | 19.5mm | 304/316 | 10mm | 16mm | 19.5mm | IP68 | ≥2300ml/min/@70mbar | 22 |
| BXG-T012 | M20×1.5 | 19.5mm | 304/316 | 10mm | 20mm | 19.5mm | IP68 | ≥2300ml/min/@70mbar | 22 |
| BXG-T013 | M22×1.5 | 26mm | 304/316 | 10mm | 22mm | 22.8mm | IP68 | ≥2500ml/min/@70mbar | 28 |
| BXG-T014 | M24×1.5 | 29mm | 304/316 | 8mm | 24mm | 21.2mm | IP68 | ≥2500ml/min/@70mbar | 30 |
| BXG-T015 | M25×1.5 | 29mm | 304/316 | 8mm | 25mm | 21.2mm | IP68 | ≥2500ml/min/@70mbar | 30 |
| BXG-T025 | M40×1.5 | 45mm | 304/316 | 15mm | 40mm | 30mm | IP68 | ≥8000ml/min/@70mbar | 45 |

| Product Number (Code) |
Metric thread (M) |
Cover outer diameter (K) |
Material | Thread Length
(GL) |
Thread O.D.
(AG) |
Total Height (H) |
Waterproof Grade | Air Permeability | Spanner Size (A&F) |
| BXG-T005G | G1/8 | 13.8mm | 304/316 | 8mm | 9.7mm | 16.5 | IP68 | ≥1500ml/min/@70mbar | 17 |
| BXG-T006G | G1/4 | 13.8mm | 304/316 | 7mm | 12mm | 15mm | IP68 | ≥1500ml/min/@70mbar | 17 |
| BXG-T010G | G3/8 | 19.5mm | 304/316 | 10mm | 16mm | 19.5mm | IP68 | ≥2300ml/min/@70mbar | 22 |
| BXG-T012G | G1/2 | 19.5mm | 304/316 | 10mm | 20mm | 19.5mm | IP68 | ≥2300ml/min/@70mbar | 22 |
| BXG-T015G | G3/4 | 29mm | 304/316 | 10mm | 26.4mm | 23.5mm | IP68 | ≥2300ml/min/@70mbar | 32 |

| Product Number (Code) |
Metric thread (M) |
Cover outer diameter (K) |
Material | Thread Length
(GL) |
Thread O.D.
(AG) |
Total Height (H) |
Waterproof Grade | Air Permeability | Spanner Size (A&F) |
| BXG-T005NPT | NPT1/8 | 13.8mm | 304/316 | 8mm | 9.7mm | 16.5 | IP68 | ≥1500ml/min/@70mbar | 17 |
| BXG-T006NPT | NPT1/4 | 13.8mm | 304/316 | 7mm | 12mm | 15mm | IP68 | ≥1500ml/min/@70mbar | 17 |
| BXG-T010NPT | NPT3/8 | 19.5mm | 304/316 | 10mm | 16mm | 19.5mm | IP68 | ≥2300ml/min/@70mbar | 22 |
| BXG-T012NPT | NPT1/2 | 19.5mm | 304/316 | 10mm | 20mm | 19.5mm | IP68 | ≥2300ml/min/@70mbar | 22 |
| BXG-T005NPT | NPT1/8 | 13.8mm | 304/316 | 8mm | 9.7mm | 16.5 | IP68 | ≥1500ml/min/@70mbar | 17 |