Technical Parameter


  • Product Type: Aluminum Alloy Waterproof Breathable Valve / Protective Vent
  • Body Material: Aluminum Alloy
  • Finish: Sandblasted Anodized / Bright
  • Protection Rating: IP68
  • Airflow: >1.2 L/min/cm² @70mbar (Customizable)
  • Water Entry Pressure: >5 Bar
  • Operating Temperature: -40°C to +150°C
  • Properties: Oleophobic, Hydrophobic
  • Certifications: CE, RoHS, IEC-60077-1999

Key Features

  • Lightweight & Durable Construction: Made from high-quality aluminum alloy, offering the strength of metal in a lightweight package suitable for weight-sensitive applications.
  • Prevents Condensation & Pressure Buildup: Continuously equalizes pressure by allowing air and moisture vapor to flow freely, effectively preventing harmful condensation and seal fatigue.
  • IP68 Waterproof & Dustproof: Provides the highest level of protection against dust and long-term water immersion (up to 3-5 meters), with a water entry pressure greater than 5 bar.
  • Oleophobic & Hydrophobic Membrane: The advanced membrane repels both water and oil, ensuring high airflow and breathability are maintained even in harsh industrial environments.
  • Robust & Certified: Certified to CE & RoHS standards and has passed vibration and shock testing per IEC-60077-1999 for proven reliability.
  • Premium Finishes: Available with a sandblasted anodized or a bright finish for enhanced corrosion resistance and a high-end aesthetic.
Product Number
(Code)
Metric thread
(M)
Cover outer diameter
(K)
Material Thread Length

(GL)

Thread O.D.

(AG)

Total Height
(H)
Waterproof Grade Air Permeability Spanner Size
(A&F)
LC-T001 M5X0.8 7.5mm aluminum 4mm 5mm 10 IP68 ≥200ml/min/@70mbar 8
LC-T002 M6X1 7.5mm aluminum 6mm 6mm 12 IP68 ≥200ml/min/@70mbar 8
LC-T001Y M5X0.8 9.8mm aluminum 6.5mm 5mm 12.5 IP68 ≥200ml/min/@70mbar Outer diameter 10/slot
LC-T002Y M6X1 9.8mm aluminum 6.5mm 6mm 14.5 IP68 ≥200ml/min/@70mbar Outer diameter 10/slot
LC-T003 M8X1.25 11.8mm aluminum 7mm 8mm 16 IP68 ≥300ml/min/@70mbar 12
LC-T005 M10X1.5 13.4mm aluminum 8mm 10mm 17 IP68 ≥600ml/min/@70mbar 14
LC-T006 M12X1.5 14.8mm aluminum 10mm 12mm 19 IP68 ≥800ml/min/@70mbar 16
LC-T007 M14X1.5 19mm aluminum 10mm 14mm 21 IP68 ≥1200ml/min/@70mbar 19
LC-T008 M16X1.5 19.5mm aluminum 10mm 16mm 19 IP68 ≥1500ml/min/@70mbar 21
LC-T010 M20X1.5 21.8mm aluminum 10mm 20mm 19 IP68 ≥1500ml/min/@70mbar 22
LC-T013 M25X1.5 28.8mm aluminum 8mm 25mm 21 IP68 ≥2300ml/min/@70mbar 30
LC-T017 M32X1.5 35mm aluminum 15mm 32mm 27 IP68 ≥4500ml/min/@70mbar 36
LC-T022 M40X1.5 42mm aluminum 15 40mm 29 IP68 ≥8500ml/min/@70mbar 45