Naša mesingana kabelska prolaznica s ravnim provodom nudi standardno, izravno ulazno mjesto s vodonepropusnom brtvom IP68. TUV certificirana i otporna na koroziju, pouzdani je izbor za izravne priključke kabela.
Ključne značajke

| Metrički tip navoja | |||||||
| Kod | Nit AG | Raspon kabela (mm) | Nazivni promjer navoja (mm) | Promjer otvora za montažu (mm) | Duljina niti GL (mm) | Zajednička duljina H (mm) | Veličina ključa (mm) |
| M12-TR | M 12X1.5 | 6.5-3 | 12 | 12-12.2 | 7 | 19 | 14 |
| M14-TR | MMX 1.5 | 8-4 | 14 | 14-14.2 | 7 | 19 | 17 |
| M16-TR | M16X1.5 | 8-4 | 16 | 16-16.2 | 8 | 20 | 18 |
| M18-TR | M18X1.5 | 10-5 | 18 | 18-18.2 | 8 | 21 | 20 |
| M20-TR | M20X1.5 | 12-6 | 20 | 20-20.2 | 8 | 22 | 22 |
| M22-TR | M22X1.5 | 14-10 | 22 | 22-22.2 | 8 | 23 | 24 |
| M24-TR | M24X1.5 | 14-10 | 24 | 24-24.2 | 9 | 25 | 24/27 |
| M25A-TR | M25X1.5 | 14-10 | 25 | 25-25.2 | 9 | 25 | 24/27 |
| M25B-TR | M25X1.5 | 16-8 | 25 | 25-25.2 | 9 | 27 | 27 |
| M25C-TR | M25X1.5 | 18-13 | 25 | 25-25.2 | 9 | 27 | 30/27 |
| M27A-TR | M27X1.5 | 18-13 | 27 | 27-27.2 | 9 | 27 | 30 |
| M27B-TR | M27X2 | 18-13 | 27 | 27-27.2 | 9 | 27 | 30 |
| M28A-TR | M28X1.5 | 18-13 | 28 | 28-28.2 | 9 | 27 | 30 |
| M28B-TR | M28X2 | 18-13 | 28 | 28-28.2 | 9 | 27 | 30 |
| M30A-TR | M30X1.5 | 18-13 | 30 | 30-30.2 | 9 | 29 | 30/32 |
| M30B-TR | M30X2 | 18-13 | 30 | 30-30.2 | 9 | 29 | 30/32 |
| M32A-TR | M32X1.5 | 22-15 | 32 | 32-32.2 | 10 | 29 | 35 |
| M32B-TR | M32X1.5 | 20-16 | 32 | 32-32.2 | 10 | 29 | 35 |
| M32C-TR | M32X2 | 22-15 | 32 | 32-32.2 | 10 | 29 | 35 |
| M36A-TR | M36X1.5 | 25-18 | 36 | 36-36.2 | 10 | 31 | 40 |
| M36B-TR | M36X2 | 25-18 | 36 | 36-36.2 | 10 | 31 | 40 |
| M37A-TR | M37X1.5 | 25-18 | 37 | 37-37.2 | 10 | 31 | 40 |
| M37B-TR | M37X2 | 25-18 | 37 | 37-37.2 | 10 | 31 | 40 |
| M40A-TR | M40X1.5 | 25-18 | 40 | 40-40.2 | 11 | 31 | 40/45 |
| M40B-TR | M40X2 | 25-18 | 40 | 40-40.2 | 11 | 31 | 40/45 |
| M40C-TR | M40X1.5 | 30-22 | 40 | 40-40.2 | 11 | 35 | 45 |
| M40D-TR | M40X2 | 30-22 | 40 | 40-40.2 | 11 | 35 | 45 |
| M42A-TR | M42X1.5 | 30-22 | 42 | 42-42.2 | 11 | 35 | 45 |
| M42B-TR | M42X2 | 30-22 | 42 | 42-42.2 | 11 | 35 | 45 |
| M60A-TR | M60X1.5 | 44-37 | 60 | 60-60.2 | 13 | 38 | 64 |
| M60B-TR | M60X2 | 44-37 | 60 | 60-60.2 | 13 | 38 | 64 |
| M63A-TR | M63X1.5 | 44-37 | 63 | 63-63.2 | 13 | 38 | 64/68 |
| M63B-TR | M63X2 | 44-37 | 63 | 63-63.2 | 13 | 38 | 64/68 |
| M64A-TR | M64X1.5 | 44-37 | 64 | 64-64.2 | 13 | 38 | 64/68 |
| M64B-TR | M64X2 | 44-37 | 64 | 64-64.2 | 13 | 38 | 64/68 |
| M72-TR | M72X2 | 52-42 | 72 | 72-72.2 | 15 | 42 | 78 |
| M75-TR | M75X2 | 52-42 | 75 | 75-75.2 | 15 | 42 | 78 |
| M80-TR | M80X2 | 62-50 | 80 | 80-80.2 | 15 | 45 | 86/88 |
| M88-TR | M88X2 | 70-60 | 88 | 88-88.2 | 15 | 45 | 98 |
| M100-TR | M100X2 | 80-70 | 100 | 100-100.2 | 15 | 45 | 110 |
| PG tip niti | ||||||
| Kod | Nit AG | Raspon kabela (mm) | Nazivni promjer navoja (mm) | Promjer otvora za montažu (mm) | Duljina niti GL (mm) | Zajednička duljina H (mm) |
| PG7-TR | PG7 | 6.5-3 | 12.5 | 12.5-12.7 | 7 | 14 |
| PG9-TR | PG9 | 8-4 | 15.2 | 15.2-15.4 | 8 | 17 |
| PG11-TR | PG11 | 10-5 | 18.6 | 18.6-18.8 | 8 | 20/21 |
| PG13.5-TR | PG13,5 | 12-6 | 20.4 | 20.4-20.6 | 8 | 22 |
| PG16-TR | PG16 | 14-10 | 22.5 | 22.5-22.7 | 9 | 24 |
| PG21-TR | PG21 | 18-13 | 28.3 | 28.3-28.5 | 9 | 30 |
| PG25-TR | PG25 | 22-15 | 32 | 32-32.2 | 10 | 35 |
| PG29-TR | PG29 | 25-18 | 37 | 37-37.2 | 11 | 40 |
| PG36-TR | PG36 | 33-25 | 47 | 47-47.2 | 12 | 50 |
| PG42-TR | PG42 | 38-32 | 54 | 54-54.2 | 13 | 57 |
| PG48-TR | PG48 | 44-37 | 59.3 | 59.3-59.5 | 14 | 64 |
| PG63-TR | PG63 | 52-42 | 72 | 72-72.2 | 15 | 78 |