Waterproof T-Connector with Screw Terminals, IP68 Splice

Our TXM20 Waterproof T-Connector with Screw Terminals allows for secure, field-serviceable 3-way splices. This 16A IP68 fitting is ideal for branching power in outdoor and wet environments.


Technical Parameter


  • Product Type: Waterproof T-Connector / 3-Way Splice
  • Series / Model: TXM20
  • Shell Material: Nylon PA66 (UL-94V0 Flame Retardant)
  • Conductor Material: Nickel-Plated Copper
  • O-Ring Material: Silicone
  • IP Rating: IP68
  • Operating Temperature: -40°C to +105°C
  • Rated Voltage / Current: 380V / 16A
  • Pin Counts Available: 2, 3
  • Applicable Wire Size: 0.2 – 2.5mm²
  • Applicable Cable O.D.: 5-8mm, 9-12mm
  • Termination: Screw Terminal
  • Certifications: CE, RoHS

Key Features

  • 3-Way T-Shaped Design: Allows one cable input to be split into two outputs, perfect for creating branches in a wiring system or daisy-chaining multiple devices.
  • Easy Screw Terminal Wiring: Features screw-in terminals for fast and secure wire connections (0.2-2.5mm²) without the need for special crimping tools, ideal for field service.
  • IP68 Waterproof Protection: Provides the highest level of protection against dust and long-term water immersion, ensuring reliable connections in wet or outdoor environments.
  • Solid Power Capacity: Rated for up to 380V and 16A, making it suitable for a wide range of power applications, including outdoor lighting, pumps, and base station equipment.
  • Durable & Safe Materials: Constructed with a UL94V-0 flame-retardant Nylon PA66 shell and silicone O-rings for excellent durability and safety.
  • High-Quality Conductors: Utilizes nickel-plated copper for superior conductivity and a reliable, long-lasting connection.

Waterproof T-Connector with Screw Terminals, IP68 Splice

Model TXM20-10 TXM20-11 TXM20-12 TXM20-13 Waterproof T-Connector with Screw Terminals, IP68 Splice
Quantity/bag 10 10 10 10
Core 2 Core 2 Core 3 Core 3 Core
Cable range(mm) 5-8 9-12 5-8 9-12
Per Pcs weight(g) 69 67.8 77.1 75.3
One carton weight(kg) 17.5 17.3 19.5 19.1