Stainless Steel Conduit Connector, IP66 Flex to Box Fitting

Our Stainless Steel Conduit Connector provides a secure, IP66 liquid-tight seal. Made from 304/316 grade steel, it offers superior corrosion resistance for harsh industrial and marine environments.


Technical Parameter


  • Product Type: Stainless Steel Flex to Box Connector
  • Model Series: DPJ
  • Body Material: Stainless Steel (304, 316)
  • Ferrule: Galvanized Iron / Stainless Steel (Please verify ferrule material)
  • Ingress Protection: IP66
  • Operating Temperature: -40°C to +100°C
  • Thread Type: Male Thread (NPT, G, Metric as options) (Assumed industry standard)
  • Body Shape: Hexagonal

Key Features

  • Premium Stainless Steel Construction: Made from high-quality 304 or 316 stainless steel for superior corrosion resistance, ideal for chemical, marine, and food-grade applications.
  • Liquid-Tight Sealing: Achieves an IP66 protection rating, providing a reliable seal against dust and powerful water jets, ensuring connection integrity.
  • Hexagonal Body for Easy Installation: The hex-shaped body allows for easy and secure tightening with a standard wrench, ensuring a firm connection.
  • Secure Conduit Connection: Designed to securely fasten flexible metal conduits, protecting internal wires at the termination point.
  • Versatile Application: Ideal for connecting flexible conduits to switch boxes, motors, and control panels in harsh or hygienic environments.

Stainless Steel Conduit Connector, IP66 Flex to Box Fitting

Hose Specification Inch Thread Opening holes Metric Thread Opening holes
Φ6 G1/4 13.3 M14*1.5 14.2
Φ8 G3/8 16.8 M16*1.5 16.2
Φ10 G3/8 16.8 M16*1.5 16.2
Φ12 G3/8 16.8 M20*1.5 20.2
Φ16 G1/2 21.2 M20*1.5 20.2
Φ20 G3/4 26.6 M25*1.5 25.2
Φ25 G1 33.5 M32*1.5 32.3
Φ32 G1-1/4 42.2 M40*1.5 40.3
Φ38 G1-1/2 48 M50*1.5 50.3
Φ51 G2 60 M60*2 60.3
Φ64 G2-1/2 75.5 M72*2 72.5
Φ75 G3 88.5 M88*2 88.5
Φ100 G4 114 M114*2 115