Stainless Steel Cable Gland, IP68 Corrosion-Resistant Fitting

Our Stainless Steel Cable Gland offers the ultimate IP68 protection in harsh environments. Made from 304/316 grade steel, it provides superior corrosion resistance, ideal for marine and industrial use.


Technical Parameter


  • Product Type: Stainless Steel Cable Gland
  • Material: Stainless Steel (AISI 304, AISI 316)
  • Protection Rating: IP68
  • Operating Temperature: -40°C to 100°C (short term to 120°C)
  • Thread Types: Metric, PG, G(PF/BSP), NPT
  • Available Sizes: M8-M100; PG7-PG63; NPT1/4-NPT3; G1/4-G3
  • Certifications: TUV, CE, RoHS, ISO9001
  • Optional Features: Explosion-Proof (ATEX/IECEx), Electropolished Finish

Key Features

  • Superior Corrosion Resistance: Made from high-quality 304/316 stainless steel, offering exceptional resistance to rust, saltwater, chemicals, and extreme weather.
  • IP68 Certified Protection: Provides the highest level of protection against dust and water ingress, ensuring a completely sealed and reliable connection.
  • High Mechanical Strength: Engineered to withstand high tension, strong vibrations, and mechanical stress without compromising integrity.
  • Wide Operating Temperature: Performs consistently in extreme temperatures ranging from -40°C to 100°C, suitable for any climate.
  • Full Range of Threads: Available in Metric, PG, NPT, and G threads, ensuring compatibility with diverse international equipment.
  • Fully Certified: Meets stringent international standards with CE, TUV, RoHS, and ISO9001 certifications for guaranteed quality and safety.

Stainless Steel Cable Gland, IP68 Corrosion-Resistant Fitting

Thread Type: M
Item Range
Φ mm
Tread Length
GL mm
Thread O.D.
AG mm
Joint Length
H mm
Spanner size
mm
Code
M8×1 2-5 5 8 16 12 SSM8
M10×1 3-6.5 7 10 19 14 SSM10
M12×1.5 3-6.5 7 12 19 14 SSM12
M12×1.5 4-8 8 12 19 17/14 SSM12-8
M14×1.5 3-6 8 14 19 17 SSM14-6
M14×1.5 4-8 8 14 19 17 SSM14
M16×1.5 4-8 8 16 20 18 SSM16
M16×1.5 5-10 8 16 21 20/18 SSM16-10
M18×1.5 5-10 8 18 21 20/21 SSM18
M18×1.5 6-12 8 18 22 22/20 SSM18-12
M20×1.5 6-12 8 20 22 22 SSM20
M20×1.5 10-14 8 20 23 24/22 SSM20-12
M22×1.5 10-14 8 22 23 24 SSM22
M22×1.5 12-16 8 22 23 27/24 SSM22-16
M25×1.5 10-14 9 25 27 24/27 SSM25-14
M25×1.5 12-16 9 25 27 27 SSM25-16
M25×1.5 13-18 9 25 27 30/27 SSM25-18
M27×1.5 13-18 9 27 27 30 SSM27
M32×1.5 13-18 10 32 29 35 SSM32-18
M32×1.5 15-22 10 32 29 35 SSM32
M32×1.5 18-25 10 32 31 40/35 SSM32-25
M36×1.5 15-22 10 36 31 40 SSM36-22
M36×1.5 18-25 10 36 31 40 SSM36
M40×1.5 18-25 11 40 31 40/45 SSM40-25
M40×1.5 22-30 11 40 35 45 SSM40-30
M40×1.5 25-33 11 40 37 50/45 SSM40-33
M47×1.5 25-33 11 47 37 50 SSM47
M50×1.5 32-38 12 50 37 57/55 SSM50
M50×1.5 37-44 13 50 38 64/55 SSM50-44
M60×1.5 37-44 13 60 38 65 SSM60
M63×1.5 37-44 13 63 38 64/68 SSM63
M63×1.5 42-52 13 63 42 78/68 SSM63-52
M72×2 42-52 15 72 42 76/80 SSM72

 

Thread Type :PG
Item Range Tread Length Thread O.D. Joint Length Spanner size Code
Φ mm GL mm AG mm H mm mm
PG7 3-6.5 7 12.5 19 14/15 SSPG7
PG9 4-8 8 15.2 20 17/18 SSPG9
PG11 5-10 8 18.6 21 20/21 SSPG11
PG13.5 6-12 8 20.4 22 22/23 SSPG13.5
PG16 10-14 8 22.5 23 24/25 SSPG16
PG21 13-18 9 28.3 27 30 SSPG21
PG29 18-25 10 37 31 40 SSPG29
PG36 25-33 11 47 37 50 SSPG36
PG42 32-38 13 54 38 60 SSPG42
PG48 37-44 14 59.3 38 65 SSPG48
PG63 42-52 16 72 42 76/80 SSPG63

 

Thread Type :G/NPT
Item Range Tread Length Thread O.D. Joint Length Spanner size Code
Φ mm GL mm AG mm H mm mm
G1/4 3-6.5 7 19 13.1 14 SSG1/4
G3/8 4-8 8 21 16.6 17/20 SSG3/8
G1/2 6-12 8 22 20.9 22/23 SSG1/2
G3/4 13-18 9 25 26.4 30 SSG3/4
G1 18-25 10 29 32.2 40 SSG1/2
G1-1/4 25-33 11 35 41.9 50 NPG1-1/4
G1-1/2 32-38 12 37 47.8 57/55 NPG1-1/2
G2 37-44 14 38 59.6 65 NPG2
G2-1/2 42-52 16 42 75.1 78 NPG2-1/2
G3 65-70 18 45 88 94 NPG3
NPT1/4 3-6.5 11 19 13.6 14 SSNPT1/4
NPT3/8 4-8 11 21 17 17/20 SSNPT3/8
NPT1/2 6-12 13 23.5 21.2 22/24 SSNPT1/2
NPT3/4 13-18 13 26 26.5 30 SSNPT3/4
NPT1 18-25 16 33 33.2 40 SSNPT1
NPT1-1/4 22-32 16 37.5 41.9 50 SSNPT1 1/4
NPT1-1/2 30-38 18 38.5 48 55/58 SSNPT1 1/2
NPT2 37-44 18 40 60 65 SSNPT2
NPT2-1/2 42-52 18 40 72.6 77 SSNPT2-1/2
NPT3 55-61 18 41 88.6 94 SSNPT3
Form Contact
Bepto Logo

Get More Benefits Since Submit The Info Form

Form Contact