Our mini IP68 Waterproof Junction Box offers a rugged, submersible seal for outdoor wire splices. Featuring easy screw terminals and available in 2, 3, & 4-way configurations for ultimate flexibility.
Key Features
| OrderCode | MN-05 | MN-06 | MN-07 |
| Qty/bag | 1 | 1 | 1 |
| 2T | 3ways | 3ways | 3ways |
| Locking Range | 3-6.5 | 5-8 | 7-10 |
| Unit Weight (g) | 76 | 75.2 | 74.4 |
| Ctn Weight (kg) | 10.6 | 10.5 | 10.4 |
| Protection Rate | IP68 | ||
| Temperature Resistance | -40℃ to +105℃ | ||
| Storing Temperature | Normal Temperature | ||
| Main Material | PA6 Nylon | ||
| O-ring Material | Silicone (environmental material) | ||
| Cable Range | 3-6.5mm. 5-8mm, 7-10mm (3 kinds of rubber for options) | ||
| Connecting Method | By screwing nuts | ||
| Conductor Material | 59-1 Brass | ||
| Cable Square mm | 0.5-2.5mm2 | ||
| Voltage Resistance | 1500V | ||
| Ampere/Voltage | 24A/450V | ||
| Flame retardant grade | UL-94V0 | ||
| Package Qty | Qty/bag:1pc,Qty/Ctn:144bags, Ctn size: 49cm*35cm*23cm | ||