Need a high-power IP68 Waterproof Connector? TS13CP (plug) and TS13CS (socket) are engineered for durability, with gold-plated contacts and V-0 flame retardant housing for demanding applications.
Key Features

| TS13series Solder contact spec | |||||||
| Contact QTY | 2 | 3 | 4 | 5 | 6 | 7 | 9 |
| Male contact face view | ![]() |
![]() |
![]() |
![]() |
![]() |
![]() |
![]() |
| Rated current(A) | 13 | 13 | 5 | 5 | 5 | 5 | 3 |
| Contact diameter(mm) | Φ1.6×2 | Φ1.6×3 | Φ1×4 | Φ1×5 | Φ1×6 | Φ1×7 | Φ0.7×9 |
| Rated voltage(AC.V) | 250 | 250 | 200 | 180 | 125 | 125 | 125 |
| Test voltage(AC.V) 1min | 1500 | 1500 | 1500 | 1000 | 1000 | 1000 | 1000 |
| Contact resistance (mΩ) | 2.5 | 2.5 | 5 | 5 | 5 | 5 | 10 |
| Wire size (mm2/AWG) | ≤2/14 | ≤2/14 | ≤0.75/18 | ≤0.75/18 | ≤0.75/18 | ≤0.75/18 | ≤0.5/20 |