Flexible Nylon Cable Gland for Bend Protection, IP68

Our Flexible Nylon Cable Gland features a spiral design for superior bend protection. This IP68 fitting prevents cable fatigue and damage in dynamic applications like robotics and moving machinery.


Technical Parameter


  • Product Type: Flexible / Anti-Bending Nylon Cable Gland
  • Body Material: Nylon PA66
  • Seal Material: NBR (Nitrile Butadiene Rubber) or EPDM (Weathering Resistance Rubber)
  • Protection Rating: IP68
  • Static Temperature: -40°C to 100°C (short term to 120°C)
  • Dynamic Temperature: -20°C to 80°C (short term to 100°C)
  • Thread Types: Metric, PG
  • Colors: Black (RAL 9005), Light Gray (RAL 7035), custom colors available

Key Features

  • Flexible Bend Protection: Features an integrated spiral guard that offers superior anti-bending protection, preventing cable fatigue and damage from flexing and vibration.
  • IP68 Certified Protection: Provides a robust seal against dust and water ingress, ensuring reliable performance in demanding indoor and outdoor environments.
  • High Strain Relief: The special design of the clamping claws and seal provides exceptional gripping force, securely holding the cable against pulling forces.
  • Durable Nylon PA66 Material: Constructed from high-quality Nylon PA66 for excellent mechanical strength and durability.
  • Broad Chemical Resistance: Resistant to salt water, weak acids, alcohol, oil, grease, and common solvents.
  • Ideal for Dynamic Applications: Recommended for use on moving machinery, robotics, automation systems, and any application where cables are subject to frequent movement.

Flexible Nylon Cable Gland for Bend Protection, IP68

PG/M type
Code Model Cable Range(mm) Thread O.D. L2(mm) Thread engt L1(mm) Spanner size(mm)
PG7-NFL PG7 3~6.5 12.5 8 16
PG9-NFL PG9 4~8 15.2 8 19
PG11-NFL PG11 5~10 18.6 8 22
PG13.5-NFL PG13.5 6~12 20.4 9 24
PG-16NFL PG16 10~14 22.5 10 27
PG21-NFL PG21 13~18 28.3 10 33
M12-NFL M12 3~6.5 12 8 16
M16-NFL M16 4~8 16 8 19
M18-NFL M18 5~10 18 8 22
M20-NFL M20 6~12 20 9 24
M22-NFL M22 10~14 22 10 27
M25-NFL M25 13~18 25 10 33
M27-NFL M27 13~18 27 10 33