Female Thread Cable Gland, IP68 for Male Threaded Entries

Our Female Thread Cable Gland is designed to mount on male-threaded outlets. This IP68 fitting provides a secure, waterproof seal for cables on equipment with external threads, ensuring a reliable connection.


Technical Parameter


  • Product Type: Female Thread / Internal Thread Cable Gland
  • Body Material: Nickel-Plated Brass, Stainless Steel (304/316L)
  • Claw: Nylon (PA)
  • Seal & O-Ring: NBR (Nitrile Rubber)
  • Protection Rating: IP68 – 10 Bar
  • Static Temperature: -40°C to 100°C (short term to 120°C)
  • Dynamic Temperature: -20°C to 80°C (short term to 100°C)
  • Thread Types: Metric, PG, G, NPT (Internal/Female Thread)
  • Certifications: TUV, ISO9001, CE

Key Features

  • Internal (Female) Mounting Thread: Uniquely designed with an internal thread to securely mount onto equipment outlets, pipes, or ports that have an external (male) thread.
  • IP68-10 Bar Waterproof Protection: Delivers the highest level of certified protection against dust and high-pressure water, ensuring a completely sealed and reliable connection.
  • Premium Material Options: Available in robust Nickel-Plated Brass or high-grade Stainless Steel (304/316L) for superior corrosion and chemical resistance.
  • High Strain Relief: A special design of the clamping claws and seal provides exceptional gripping force and superior resistance to pulling and twisting.
  • TUV & ISO Certified Quality: Manufactured under strict quality controls and certified by TUV and ISO9001, guaranteeing reliability and performance.
  • Fully Customizable: Thread types, sizes, and materials can be fully customized to meet specific project requirements.
Code Thread

specification

Available cable

range

(mm)

Thread O.D
(mm)
Mounting Hole

Diamte
(mm)

Thread

Length (mm)

Spanner size
(mm)
M12-NLW M12×1.5 6.5-3 12 12-12.2 7 14
M14-NLW M14×1.5 8-4 14 14-14.2 7 17
M16-NLW M16×1.5 8-4 16 16-16.2 8 18
M18-NLW M18×1.5 10-5 18 18-18.2 8 20
M20-NLW M20×1.5 12-6 20 20-20.2 8 22
M22-NLW M22×1.5 14-10 22 22-22.2 8 24
M24-NLW M24×1.5 14-10 24 24-24.2 9 24/27
M25A-NLW M25×1.5 14-10 25 25-25.2 9 24/27
M25B-NLW M25×1.5 16-8 25 25-25.2 9 27
M25C-NLW M25×1.5 18-13 25 25-25.2 9 30/27
M27A-NLW M27×1.5 18-13 27 27-27.2 9 30
M27B-NLW M27×2 18-13 27 27-27.2 9 30
M28A-NLW M28×1.5 18-13 28 28-28.2 9 30
M28B-NLW M28×2 18-13 28 28-28.2 9 30
M30A-NLW M30×1.5 18-13 30 30-30.2 9 30/32
M30B-NLW M30×2 18-13 30 30-30.2 9 30/32
M32A-NLW M32×1.5 22-15 32 32-32.2 10 35
M32B-NLW M32×1.5 20-16 32 32-32.2 10 35
M32C-NLW M32×2 22-15 32 32-32.2 10 35
M36A-NLW M36×1.5 25-18 36 36-36.2 10 40
M36B-NLW M36×2 25-18 36 36-36.2 10 40
M37A-NLW M37×1.5 25-18 37 37-37.2 10 40
M37B-NLW M37×2 25-18 37 37-37.2 10 40
M40A-NLW M40×1.5 25-18 40 40-40.2 11 40/45
M40B-NLW M40×2 25-18 40 40-40.2 11 40/45
M40C-NLW M40×1.5 30-22 40 40-40.2 11 45
M40D-NLW M40×2 30-22 40 40-40.2 11 45
M42A-NLW M42×1.5 30-22 42 42-42.2 11 45
M42B-NLW M42×2 30-22 42 42-42.2 11 45
M50A-NLW M50×1.5 38-32 50 50-50.2 12 57/55
M50B-NLW M50×2 38-32 50 50-50.2 12 57/55
M60A-NLW M60×1.5 44-37 60 60-60.2 13 64
M60B-NLW M60×2 44-37 60 60-60.2 13 64
M63A-NLW M63×1.5 44-37 63 63-63.2 13 64/68
M63B-NLW M63×2 44-37 63 63-63.2 13 64/68
M72-NLW M72×2 52-42 72 72-72.2 15 78
M75-NLW M75×2 52-42 75 75-75.2 15 78
M80-NLW M80×2 62-50 80 80-80.2 18 86/88
M88-NLW M88×2 70-60 88 88-88.2 18 98
M100-NLW M100×2 80-70 100 100-100.2 20 110