500V High-Voltage In-line Connector, TS17RS/RP IP68

Our 500V High-Voltage In-line Connector (TS17RS/RP) creates a rugged, IP68 splice for industrial power and signal cables. It features a secure threaded coupling and gold-plated contacts for reliable performance.


Technical Parameter


  • Series: TS17 Series
  • Models: TS17RP (Reverse Cable Plug), TS17RS (Reverse Cable Socket)
  • Coupling Type: Threaded
  • Shell Material: PC, Nylon PA66 (UL94V-0)
  • Insert Material: PPS (Max Temp 260°C)
  • Contact Material: Brass with Gold Plating
  • IP Rating: IP68
  • Operating Temperature: -40°C to +85°C
  • Mating Cycle: 500 cycles
  • Pin Counts Available: 2, 3, 4, 5, 7, 9, 10
  • Rated Current: 5A / 10A (Varies by pin count)
  • Termination: Solder or Crimp

Key Features

  • High Voltage Rating: Withstands operating voltages up to 500V (AC), making it suitable for demanding power and industrial control applications.
  • Designed for In-line Connections: The TS17RP (Reverse Plug) and TS17RS (Reverse Socket) are specifically designed to join two cables together, creating a secure and continuous connection in the middle of a run.
  • Versatile Termination Options: Offers both Solder and Crimp contact versions, providing flexibility for different assembly requirements and user preferences.
  • IP68 Waterproof Protection: Provides the highest level of protection against dust and long-term water immersion, ensuring reliable connections in wet or outdoor environments.
  • Secure Threaded Coupling: Features a robust threaded locking mechanism that resists vibration and ensures a stable, mated connection.
  • High-Performance Materials: Constructed with a UL94V-0 flame-retardant shell, high-temperature resistant PPS inserts (260°C), and gold-plated brass contacts.

500V High-Voltage In-line Connector, TS17RSRP IP68

TS17 Series solder contact spec
Contact QTY 2 3 4 5 7 9 10
Male contact face view 2Ping 3Ping 4Ping 5Ping 7Ping 9Ping 10Ping
Rated current(A) 10 10 5 5 5 5 5
Contact diameter(mm) Φ1.5×2 Φ1.5×3 Φ1×4 Φ1×5 Φ1×7 Φ1×9 Φ1×10
Rated voltage(AC.V) 500 500 500 500 400 400 400
Test voltage(AC.V) 1min 1500 1500 1500 1000 1200 1200 1200
Contact resistance (mΩ) 2.5 2.5 5 5 5 5 10
Wire size (mm2/AWG) ≤2/14 ≤2/14 ≤0.75/18 ≤0.75/18 ≤0.75/18 ≤0.75/18 ≤0.7/
TS17 Series crimp contact spec
Contact QTY 2 3 4
Male contact face view 2Ping 3Ping-2 4Ping-2
Rated current(A) 10 10 5
Contact diameter(mm) Φ1.5×2 Φ1.5×3 Φ1×4
Rated voltage(AC.V) 500 500 500
Test voltage(AC.V) 1min 1500 1500 1500
Contact resistance (mΩ) 2.5 2.5 5
Insulation resistance (mΩ) 2000 2000 2000

 