Cross-threading

Illustrated explanation

Recognize different causes of a damaged threaded joint

3Cross-threading
Recognize different causes of a damaged threaded jointCallout 1: Galling. Callout 2: Seizure. Callout 3: Cross-threading. Callout 4: Stripped ridges. Callout 5: Self-loosening. Adhesive wear, seizure, a misaligned start, sheared ridges and loosening are distinct problems. Increased torque can worsen several of these conditions. Current term: Cross-threading, callout 3. 1Adhesion + torn materialGalling 2Seizure 3Cross-threading 4Stripped ridges 5Self-loosening
  1. Thread galling

    Raised and torn material indicates adhesive wear. Review material pairing, friction, cleanliness and permitted lubrication.

  2. Thread seizure

    The joint no longer moves freely. Galling, corrosion or deformation may be responsible; seizure names the condition, not one cause.

  3. Cross-threadingThis term

    The mating part starts at the wrong angle or path. Extra tightening force must not be used to overcome a damaged start.

  4. Thread stripping

    Sheared ridges remove load-carrying engagement. Review material strength, effective engagement and installation loading.

  5. Self-loosening

    Relative movement or settlement can reduce clamp load. Initial tightening torque alone does not prove service stability.

Adhesive wear, seizure, a misaligned start, sheared ridges and loosening are distinct problems. Increased torque can worsen several of these conditions.

Exaggerated failure sketches without load values. Investigate the cause and replace or repair components through the approved assembly procedure.