Illustrated explanation
2Face sealCompression, sealing faces and extrusion
- Seal compression
Squeeze changes the seal cross-section between the free and installed states. More compression does not always improve sealing.
- Face sealThis term
A face seal acts between opposing surfaces. Check the gasket, seating faces and available compression space.
- Seal extrusion
An unsupported gap can allow elastomer to move out of its intended space. Check clearance, pressure, temperature and material.
A supported elastomer changes shape when compressed between mating faces. A separate example shows material pushed into an unsupported clearance under load or pressure.
Conceptual gasket sections with exaggerated deformation. Required squeeze, housing dimensions, material and pressure limits depend on the specified seal.