Chemical resistance

Illustrated explanation

Exposure can change polymer dimensions and integrity

6Chemical resistance
Exposure can change polymer dimensions and integrityCallout 1: Moisture uptake. Callout 2: Controlled conditioning. Callout 3: Hydrolysis. Callout 4: Swelling. Callout 5: Stress cracking. Callout 6: Chemical compatibility. Moisture uptake, controlled conditioning, chemical chain changes, swelling and stress-assisted cracking describe different exposure outcomes. A material name alone cannot resolve compatibility. Current term: Chemical resistance, callout 6. 1Moisture uptake 2Temperature + humidity + timeControlled conditioning 3Hydrolysis 4Exposure-dependent growthSwelling 5Stress cracking 6Fluid / T / concentration / timeChemical compatibility
  1. Water absorption / hygroscopicity

    Water can enter the material rather than merely sit on its surface. Conditioning and moisture content can change dimensions and response.

  2. Moisture conditioning

    The material is brought to a defined moisture condition. Compare results from equivalent conditioning and handling.

  3. Hydrolysis

    The exposure can chemically alter susceptible chains. Moisture uptake and hydrolysis are different mechanisms.

  4. Swelling

    Absorbed fluid can increase dimensions or volume. Check the actual fluid and compound rather than assuming stable seal squeeze.

  5. Environmental stress cracking (ESC)

    A susceptible polymer cracks under combined exposure and stress. Evaluate the assembled load and the specific environment.

  6. Chemical resistanceThis term

    A defined chemical exposure is evaluated for the actual material. Resistance to one fluid or condition does not establish general chemical suitability.

Moisture uptake, controlled conditioning, chemical chain changes, swelling and stress-assisted cracking describe different exposure outcomes. A material name alone cannot resolve compatibility.

Exaggerated qualitative material sketches. The fluid, concentration, temperature, time and actual compound must be specified for selection.