Seal hardness

Illustrated explanation

Separate strength, extension, tearing and indentation

5Seal hardness
Separate strength, extension, tearing and indentationCallout 1: Maximum tensile stress. Callout 2: Yield response. Callout 3: Extension. Callout 4: Tear propagation. Callout 5: Indentation hardness. Tension measurements distinguish yield, maximum stress and extension, while tearing and indentation use different loading geometries. Their results cannot be substituted for each other. Current term: Seal hardness, callout 5. 1StrainStressMaximum tensile stress 2StrainStressYield response 3Extension 4Tear propagation 5Indentation hardness
  1. Tensile strength / UTS

    The marked peak represents maximum engineering tensile stress for the stated test. It is separate from yield strength and elongation.

  2. Yield strength

    The marked transition represents the specified yielding criterion. Use the actual material’s method rather than assuming one sharp yield point.

  3. Elongation

    The specimen length changes under tensile loading. State the gauge length and the point or condition at which elongation is measured.

  4. Tear strength

    The notched geometry promotes tear propagation. Tear strength uses its stated specimen and method, rather than an ordinary tensile result.

  5. Seal hardnessThis term

    An indenter probes the compound’s resistance to indentation. Hardness alone does not establish seal compatibility, compression or extrusion limits.

Tension measurements distinguish yield, maximum stress and extension, while tearing and indentation use different loading geometries. Their results cannot be substituted for each other.

Qualitative curves and specimen sketches without measured values. Method, specimen, direction, temperature and loading rate govern comparisons.