Magnetic susceptibility

Illustrated explanation

Magnetic response and induced currents describe different effects

2Magnetic susceptibility
Magnetic response and induced currents describe different effectsCallout 1: Field response. Callout 2: Magnetization response. Callout 3: Induced circulating current. Permeability and susceptibility describe material response to a magnetic field, while a changing field can induce circulating current in conductive material. Current term: Magnetic susceptibility, callout 2. 1B related to HField response 2Magnetization related to HMagnetization response 3Changing magnetic fieldInduced circulating current
  1. Magnetic permeability

    Permeability relates flux density and magnetic field under the stated conditions. Grade name alone does not establish the complete magnetic behaviour.

  2. Magnetic susceptibilityThis term

    The arrows represent the material’s magnetization response. Susceptibility and permeability are related but different quantities.

  3. Eddy current

    A changing field can drive a closed current path in a conductor. Material, thickness, geometry and frequency affect the response.

Permeability and susceptibility describe material response to a magnetic field, while a changing field can induce circulating current in conductive material.

Conceptual field and current paths. No alloy’s magnetic state, shielding factor or current magnitude is assigned.