Electrical conductivity / resistivity

Illustrated explanation

A galvanic path needs metals, electrical contact and an electrolyte

4Electrical conductivity / resistivity
A galvanic path needs metals, electrical contact and an electrolyteCallout 1: Galvanic cell. Callout 2: Series / actual couple. Callout 3: Isolation barrier. Callout 4: Bulk electrical transport. A dissimilar-metal connection and a wet conductive path can form a corrosion cell. Breaking the intended electrical path is a separate design decision from choosing the metal or coating. Current term: Electrical conductivity / resistivity, callout 4. 1Metals + contact + electrolyteGalvanic cell 2Specified electrolyteSeries / actual couple 3Intentional separationIsolation barrier 4R = resistivity × L / ABulk electrical transport
  1. Galvanic corrosion

    The two metals share an electrical path and electrolyte. Their pairing, areas and actual exposure influence the corrosion mechanism.

  2. Galvanic series / galvanic couple

    A series describes behaviour in a stated environment; a couple is the actual connected metal pair. Do not transfer one ranking to every exposure.

  3. Electrical isolation

    The separating layer interrupts the illustrated conductive route. Review required bonding and safety connections for the complete assembly.

  4. Electrical conductivity / resistivityThis term

    Bulk conductivity and resistivity describe the material under stated conditions. Conductor length and area also affect the resistance.

A dissimilar-metal connection and a wet conductive path can form a corrosion cell. Breaking the intended electrical path is a separate design decision from choosing the metal or coating.

Conceptual electrical and corrosion paths. No universal galvanic ranking, corrosion rate or protective-earth arrangement is specified.