Thermal aging

Illustrated explanation

Identify the exposure before comparing aging performance

3Thermal aging
Identify the exposure before comparing aging performanceCallout 1: UV exposure. Callout 2: Light-driven degradation. Callout 3: Heat aging. Callout 4: Long-term thermal index. Callout 5: Ozone exposure. Light, heat and ozone can change material properties through different exposure mechanisms. Resistance claims need their own method, duration and actual formulation. Current term: Thermal aging, callout 3. 1Evaluate defined light exposureUV exposure 2O2Light-driven degradation 3Temperature + timeHeat aging 4Exposure timeStated propertySpecified temperaturesLong-term thermal index 5O3Ozone exposure
  1. UV resistance

    The arrows represent the stated light exposure. Confirm test conditions and retained properties for the actual material.

  2. Photodegradation / photo-oxidation

    Light can change susceptible material, with oxidation where oxygen participates. Check the actual mechanism and exposure evidence.

  3. Thermal agingThis term

    Sustained heat exposure can alter material properties. Use the specified aging method and retained-property criteria.

  4. Relative thermal index (RTI)

    The index follows long-term evaluation of a specified material property. Electrical and mechanical property categories are not one interchangeable temperature rating.

  5. Ozone resistance

    The exposure can cause cracking in susceptible compounds under the stated conditions. Ozone resistance is different from general outdoor durability.

Light, heat and ozone can change material properties through different exposure mechanisms. Resistance claims need their own method, duration and actual formulation.

Conceptual exposure and degradation sketches without lifetime predictions. Accelerated exposure does not automatically represent service years.