NSS / AASS / CASS

Illustrated explanation

Controlled laboratory exposures answer different questions

2NSS / AASS / CASS
Controlled laboratory exposures answer different questionsCallout 1: Salt-mist exposure. Callout 2: NSS / AASS / CASS. Callout 3: Temperature + humidity. Callout 4: Light / broader aging. Salt mist, acidified corrosion exposures, humid heat and light-based weathering stress different aspects of a specimen. The test method and acceptance criteria must accompany any reported result. Current term: NSS / AASS / CASS, callout 2. 1Salt-mist exposure 2NSSNeutralAASSAcidifiedCASS+ copperDifferent controlled exposuresNSS / AASS / CASS 3Steady or cyclic procedureTemperature + humidity 4Specify the exposure programmeLight / broader aging
  1. Salt-spray test

    The specimen receives a defined salt-mist exposure. State the method, orientation, duration and corrosion acceptance criteria.

  2. NSS / AASS / CASSThis term

    Neutral, acidified and copper-accelerated acidified salt spray are different exposures. Do not substitute one result for another method.

  3. Damp heat

    Elevated temperature and humidity are combined under a defined procedure. Confirm whether the method is steady, cyclic or another specified sequence.

  4. Accelerated weathering / aging

    Weathering includes defined light and environmental exposure; accelerated aging covers broader intensified conditions. Validate any relation to field use separately.

Salt mist, acidified corrosion exposures, humid heat and light-based weathering stress different aspects of a specimen. The test method and acceptance criteria must accompany any reported result.

Conceptual chambers with no exposure concentration, duration or field-life factor. An accelerated test does not give a universal service-life conversion or approval for every environment.