Insulation resistance

Illustrated explanation

Bulk insulation and surface tracking are different paths

3Insulation resistance
Bulk insulation and surface tracking are different pathsCallout 1: Permittivity. Callout 2: Bulk breakdown. Callout 3: Insulation resistance. Callout 4: CTI determination. Callout 5: PTI proof condition. An electric field crosses an insulating body, while leakage and wet-contaminant tracking can follow its surface. Permittivity, dielectric strength and tracking indices describe different properties. Current term: Insulation resistance, callout 3. 1Field in a dielectricPermittivity 2Bulk breakdown 3LeakageInsulation resistance 4Compare test voltagesCTI determination 5One specified conditionPTI proof condition
  1. Permittivity

    The dielectric changes the relationship between electric field and stored charge. Permittivity is not a dielectric breakdown rating.

  2. Dielectric strength

    Breakdown crosses the material under a defined electric stress. State thickness, electrodes, conditioning and test procedure.

  3. Insulation resistanceThis term

    A defined voltage produces a measured leakage current. Temperature, moisture and time affect the measured resistance.

  4. Comparative tracking index (CTI)

    Wet-contaminant testing establishes a comparative index. Surface tracking differs from breakdown through the insulating body.

  5. Proof tracking index (PTI)

    The material is assessed at a specified proof condition. That result does not determine its complete comparative tracking index.

An electric field crosses an insulating body, while leakage and wet-contaminant tracking can follow its surface. Permittivity, dielectric strength and tracking indices describe different properties.

Conceptual electrical paths, not test circuits or voltage limits. Material condition, geometry and the applicable test method determine each result.