Electroless nickel plating

Illustrated explanation

Coating methods and continuity must be specified separately

2Electroless nickel plating
Coating methods and continuity must be specified separatelyCallout 1: Electroplating. Callout 2: Electroless nickel. Callout 3: Anodic oxide. Callout 4: Layer thickness. Callout 5: Pores / holidays. Electroplating uses an electrical process, electroless deposition uses a chemical process and anodizing forms an oxide on the specified alloy. Thickness and defects remain independent inspection questions. Current term: Electroless nickel plating, callout 2. 1External electrical supplyElectroplating 2Chemical depositionElectroless nickel 3Oxide on specified alloyAnodic oxide 4Layer normal to surfaceLayer thickness 5Pores / holidays
  1. Electroplating

    A controlled electrical process deposits the specified metal. Substrate preparation and deposition conditions affect the coating.

  2. Electroless nickel platingThis term

    The bath deposits nickel by the specified chemical process. Require composition, preparation and performance evidence for that coating.

  3. Anodizing

    The process forms an oxide on a suitable substrate. Its thickness, sealing and duty need their actual specifications.

  4. Plating thickness

    The thickness is measured normal to the coated surface under the stated method. Check local variation and the actual drawing limits.

  5. Coating porosity / holidays

    A pore and a discontinuity can expose different paths through the coating. Inspection must address the relevant defect and coverage requirements.

Electroplating uses an electrical process, electroless deposition uses a chemical process and anodizing forms an oxide on the specified alloy. Thickness and defects remain independent inspection questions.

Conceptual coating sections without alloy assignments or thickness values. These process names do not establish identical corrosion or contact performance.